    • 15. 发明授权
    • Non-magnetic mono-component developer
    • 非磁性单组分显影剂
    • US5981132A
    • 1999-11-09
    • US219426
    • 1998-12-23
    • Katsunori KuroseMasahiro AnnoChikara TsutsuiMinoru Nakamura
    • Katsunori KuroseMasahiro AnnoChikara TsutsuiMinoru Nakamura
    • A61K31/726A61K31/728G03G9/08G03G9/087G03G9/097
    • G03G9/0819A61K31/726A61K31/728G03G9/08782G03G9/08795G03G9/097G03G9/09708
    • 1. A non-magnetic mono-component developer comprising:toner particles containing at least a binder resin and a coloring agent and having a volume mean particle size D of 4 to 10 .mu.m;first inorganic fine particles having a mean primary particle size of 1 to 40 nm, the quantity of addition of the first inorganic fine particles being 0.1 to 2% by weight relative to the quantity of the toner particles;second inorganic fine particles having a mean primary particle size of 40 to 100 nm and not less than 10 nm larger than the first inorganic fine particles, the quantity of addition of the second inorganic fine particles being 0.1 to 2.5% by weight relative to the quantity of the toner particles, the total quantity of addition of the first and second inorganic fine particles being 0.8 to 3% by weight relative to the quantity of the toner particles; andthird inorganic fine particles having a mean primary particle size of 100 nm to 1000 D/16 nm and not less than 10 nm larger than the second inorganic fine particles, the quantity of addition of the third inorganic fine particles being 0.3 to 3% by weight relative to the quantity of the toner particles.
    • 1.一种非磁性单组分显影剂,其包含:至少含有粘合剂树脂和着色剂并且体积平均粒径D为4至10μm的调色剂颗粒; 平均一次粒径为1〜40nm的第一无机细粒子,第一无机细粒子的添加量相对于调色剂粒子的量为0.1〜2重量% 第二无机细颗粒的平均一次粒径为第一无机细颗粒大40至100nm且不小于10nm,第二无机细颗粒的添加量相对于数量为0.1至2.5重量% 的调色剂颗粒,第一和第二无机细颗粒的总添加量相对于调色剂颗粒的量为0.8至3重量%; 第三无机细颗粒的平均一次粒径为比第二无机细颗粒大100nm至1000D / 16nm且不小于10nm,第三无机细颗粒的添加量为0.3至3%,通过 相对于调色剂颗粒的量的重量。