    • 11. 发明授权
    • Spark plug for internal-combustion engine
    • 内燃机火花塞
    • US08653725B2
    • 2014-02-18
    • US13497745
    • 2010-08-19
    • Haruki YoshidaToshitaka Honda
    • Haruki YoshidaToshitaka Honda
    • H01T13/20
    • H01T13/41C03C8/02
    • A spark plug that prevents a sharp increase in resistance of a resistor and materializes an excellent load life performance. The spark plug has a resistor formed by heat-sealing of a resistor composition that contains, at least, a conductive material and glass powder. The glass powder contains between 35.0 mol % and 69.8 mol % SiO2, between 15.0 mol % and 49.8 mol % B2O3, between 5.0 mol % and 20.0 mol % Li2O, and at least one additive selected from MgO, CaO, SrO, BaO, Na2O, K2O, ZnO, and ZrO2 in a total of between 2.6 mol % and 25.0 mol %. Further, the total content of Li2O and the additive(s) in the glass powder is between 15.2 mol % and 45.0 mol %, and the ratio of the Li2O content to the total content of the additive(s) is between 1.3 and 5.0.
    • 一种防止电阻器电阻急剧增加的火花塞,实现了极好的负载寿命。 火花塞具有通过热封至少包含导电材料和玻璃粉末的电阻器组合物形成的电阻器。 玻璃粉末含有35.0摩尔%至69.8摩尔%的SiO 2,15.0摩尔%至49.8摩尔%的B 2 O 3,5.0摩尔%至20.0摩尔%的Li 2 O,以及至少一种选自MgO,CaO,SrO,BaO,Na 2 O的添加剂 ,K 2 O,ZnO和ZrO 2,总计为2.6摩尔%至25.0摩尔%。 此外,玻璃粉末中的Li 2 O和添加剂的总含量为15.2摩尔%〜45.0摩尔%,Li 2 O含量与添加剂的总量的比例为1.3〜5.0。
    • 14. 发明申请
    • SPARK PLUG FOR INTERNAL-COMBUSTION ENGINE
    • 用于内燃机的火花塞
    • US20120176021A1
    • 2012-07-12
    • US13497745
    • 2010-08-19
    • Haruki YoshidaToshitaka Honda
    • Haruki YoshidaToshitaka Honda
    • H01T13/20
    • H01T13/41C03C8/02
    • A spark plug that prevents a sharp increase in resistance of a resistor and materializes an excellent load life performance. The spark plug has a resistor formed by heat-sealing of a resistor composition that contains, at least, a conductive material and glass powder. The glass powder contains between 35.0 mol % and 69.8 mol % SiO2, between 15.0 mol % and 49.8 mol % B2O3, between 5.0 mol % and 20.0 mol % Li2O, and at least one additive selected from MgO, CaO, SrO, BaO, Na2O, K2O, ZnO, and ZrO2 in a total of between 2.6 mol % and 25.0 mol %. Further, the total content of Li2O and the additive(s) in the glass powder is between 15.2 mol % and 45.0 mol %, and the ratio of the Li2O content to the total content of the additive(s) is between 1.3 and 5.0.
    • 一种防止电阻器电阻急剧增加的火花塞,实现了极好的负载寿命。 火花塞具有通过热封至少包含导电材料和玻璃粉末的电阻器组合物形成的电阻器。 玻璃粉末含有35.0摩尔%至69.8摩尔%的SiO 2,15.0摩尔%至49.8摩尔%的B 2 O 3,5.0摩尔%至20.0摩尔%的Li 2 O,以及至少一种选自MgO,CaO,SrO,BaO,Na 2 O的添加剂 ,K 2 O,ZnO和ZrO 2,总计为2.6摩尔%至25.0摩尔%。 此外,玻璃粉末中的Li 2 O和添加剂的总含量为15.2摩尔%〜45.0摩尔%,Li 2 O含量与添加剂的总量的比例为1.3〜5.0。
    • 15. 发明申请
    • SPARK PLUG
    • SPARK插头
    • US20120126683A1
    • 2012-05-24
    • US13388103
    • 2010-09-22
    • Haruki YoshidaToshitaka Honda
    • Haruki YoshidaToshitaka Honda
    • H01T13/20
    • H01T13/41C03C8/02
    • A spark plug exhibits excellent load life performance even when the resistor thereof has been thermally compacted at slightly varied heating temperatures. The spark plug includes an insulator having an axial hole extending therethrough along the axial direction; a center electrode inserted into a front end portion of the axial hole; a terminal electrode inserted into a rear end portion of the axial hole; a resistor disposed in the axial hole to be located between the center electrode and the terminal electrode, and containing at least an electrically conductive material and glass. The resistor contains 15.0 or more mass % of SiO2, 20.4-44.8 mass % of B2O3, 2.5-6.3 mass % of Li2O, and 3.5-14.6 mass % of BaO. The ratio of B2O3 to the total amount of Li2O and BaO is 1.43 or higher. The ratio of Li2O to BaO is 0.22 or higher.
    • 即使电阻器在稍微变化的加热温度下被热压缩,火花塞也显示出优异的负载寿命性能。 火花塞包括具有沿轴向延伸穿过的轴向孔的绝缘体; 插入所述轴孔的前端部的中心电极; 插入所述轴孔的后端部的端子电极; 设置在所述轴向孔中的电阻器,位于所述中心电极和所述端子电极之间,并且至少包含导电材料和玻璃。 该电阻器含有15.0质量%以上的SiO 2,20.4〜44.8质量%的B 2 O 3,2.5〜6.3质量%的Li 2 O和3.5〜14质量%的BaO。 B2O3与Li2O和BaO的总量之比为1.43以上。 Li2O与BaO的比例为0.22以上。