    • 2. 发明授权
    • Storage-stable, single-component concentrate, production and use thereof
for the production of cathodically depositable electrocoating lacquer
baths
    • 储存稳定的单组分浓缩物,其生产和用途用于生产阴极沉积的电涂漆浴
    • US5965000A
    • 1999-10-12
    • US860625
    • 1997-05-27
    • Klausjorg Klein
    • Klausjorg Klein
    • C09D5/44C09D17/00
    • C09D5/4488
    • Concentrate containing cathodically depositable binders, optionally crosslinking agents, optionally organic solvents, pigments and optionally extenders, together with water, having a solids content of 35 to 50 wt. % at a weight ratio of pigment and optionally extender to binder and crosslinking agent of 0.01:1 to 0.4:1, having a viscosity of 100 to 500 mPa.cndot.s, measured by rotational viscosimetry at 20.degree. C. and a shear gradient of 150 s.sup.-1 and a solvent content of 0 to below 20 wt. %, relative to solids content, process for the production thereof and use thereof in processes for producing or replenishing cathodically depositable electrocoating lacquer baths.
    • PCT No.PCT / EP95 / 04613 371日期:1997年5月27日 102(e)日期1997年5月27日PCT提交1995年11月23日PCT公布。 公开号WO96 / 17023 日期1996年6月6日含有固体含量为35至50重量%的阴极可沉积的粘合剂,任选的交联剂,任选的有机溶剂,颜料和任选的增量剂与水一起的浓缩物。 %的颜料和任选的增量剂与粘合剂和交联剂的重量比为0.01:1至0.4:1,粘度为100-500mPa.s,通过旋转粘度测定在20℃和剪切梯度为150 s-1,溶剂含量为0〜20wt。 相对于固体含量的%,其生产方法及其在生产或补充阴极可沉积的电涂漆浴的方法中的用途。
    • 5. 发明授权
    • Process for multi-layer coating
    • 多层涂层工艺
    • US5869198A
    • 1999-02-09
    • US930518
    • 1997-09-30
    • Marcus ErneJurgen DobertKlausjorg KleinMatthias Kimpel
    • Marcus ErneJurgen DobertKlausjorg KleinMatthias Kimpel
    • B05D1/36B05D7/00B05D7/14C25D13/06
    • B05D7/577Y10T428/12569Y10T428/31522
    • A process for the multi-layer coating of electrically conductive substrates by the electrophoretic deposition of a first coating layer comprising an electrophoretically depositable aqueous coating medium, to which a second coating layer, comprising a first color- and/or effect-imparting base lacquer coating medium, is applied wet-into-wet, and the first and second coating layers thus obtained are stoved jointly, whereupon a third coating layer comprising a second color- and/or effect-imparting base lacquer coating medium is applied and a fourth coating layer comprising a clear lacquer coating medium is applied wet-into-wet thereto and the third and fourth coating layers are stoved jointly, wherein the total dry coat thickness of the second and third coating layers produced from the base lacquer coating media is between 15 and 40 .mu.m and the proportion of the second coating layer is between 20 and 50% of the total dry coat thickness of the second and third coating layers.
    • PCT No.PCT / EP96 / 01316 Sec。 371日期:1997年9月30日 102(e)日期1997年9月30日PCT 1996年3月26日PCT公布。 WO96 / 30131 PCT出版物 日期1996年10月3日一种用于通过电泳沉积包含电泳可沉积的水性涂料介质的第一涂层来多层涂覆导电基材的方法,第二涂层包含第一颜色和/或效果 将基材漆涂布介质湿润湿润,将如此获得的第一和第二涂层共同烘烤,由此施加包含第二颜色和/或效果赋予基漆涂层介质的第三涂层 并且将包含透明漆涂层介质的第四涂层湿润湿润,并将第三和第四涂层共同烘烤,其中由基漆涂料介质制备的第二和第三涂层的总干涂层厚度 在15至40μm之间,第二涂层的比例为第二和第三涂布层的总干涂层厚度的20-50% rs。
    • 6. 发明授权
    • Process for the production of multilayer coatings
    • 多层涂料生产工艺
    • US5389406A
    • 1995-02-14
    • US136588
    • 1993-10-14
    • Klaus-Peter DoeblerWolfgang GoldnerMatthias KimpelKlausjorg Klein
    • Klaus-Peter DoeblerWolfgang GoldnerMatthias KimpelKlausjorg Klein
    • B05D1/00B05D1/36B05D3/02B05D7/00C09D175/04C25D13/00C25D13/06
    • B05D7/542B05D1/36C09D175/04B05D1/007B05D2451/00
    • A process is described for producing multilayer coatings in which a first coating layer of a first aqueous coating medium is applied to an electrically conducting substrate by electrophoretic deposition, is provided wet-in-wet with a second coating layer of a second aqueous coating medium, followed by joint stoving, wherein a coating medium based on one or more vehicles stabilised by ionic groups and which crosslink on stoving with the formation of urethane groups is used for the second coating layer, and the coating media are selected so that the maximum pigment/vehicle weight ratio of the first coating medium is 1:1, that the ratio of the pigment/vehicle weight ratio of the first coating medium to that of the second coating medium is up to 1.8, and the minimum stoving temperature interval of the second coating layer is above that of the first coating layer or overlaps the latter so that the lower limit of the interval for the second coating layer is above the lower limit of the interval for the first coating layer.
    • 描述了一种用于生产多层涂层的方法,其中通过电泳沉积将第一含水涂层介质的第一涂层施加到导电基材上,在第二涂层介质的第二涂层上湿润湿润, 接着进行联合烘烤,其中使用基于一种或多种由离子基团稳定并在形成氨基甲酸酯基团的烘烤上交联的载体的涂料介质,并且选择涂料介质以使最大颜料/ 第一涂布介质的载体重量比为1:1,第一涂布介质的颜料/载体重量比与第二涂布介质的重量比高达1.8,第二涂层的最小烘干温度间隔 层高于第一涂层的厚度或与后者重叠,使得第二涂层的间隔的下限高于第二涂层的下限 val为第一涂层。
    • 10. 发明授权
    • Process for the production of catalyst pastes containing dibutyltin
oxide and the use thereof
    • 生产含氧化二丁基锡催化剂的方法及其用途
    • US5176804A
    • 1993-01-05
    • US622539
    • 1990-12-05
    • Gabriele ButtnerNorbert DavidKlausjorg Klein
    • Gabriele ButtnerNorbert DavidKlausjorg Klein
    • C09D5/44C09D7/12C09D7/14C25D13/06
    • C09D5/4492
    • 1 Process for producing a catalyst paste for cathodically separable electrophoretic dipping lacquers.2.1 Use was made of dibutyltin oxide by way of a catalyst paste for electrophoretic dipping lacquers, dispersed in pasting binders. An object is to provide a new process for producing such catalyst pastes while saving time and energy.2.2 A process is provided for producing a catalyst paste for cathodically separable electrophoretic dipping lacquers, wherein the dibutyltin oxide is first pre-dispersed with an organic solvent and an organic acid such as is commonly used for neutralizing cathodically separable electrophoretic dipping lacquers, whereupon it is dispersed with the pasting binder and water and ground.2.3 Cathodic electrophoretic dip lacquering making use of catalyst pastes containing dibutyltin oxide.
    • 1制备用于阴极分离的电泳浸渍漆的催化剂浆料的方法。 2.1使用二丁基氧化锡通过电泳浸渍漆的催化剂浆料分散在糊状粘合剂中。 目的是提供一种生产这种催化剂浆料的新方法,同时节省时间和精力。 2.2提供了用于生产用于阴极可分离电泳浸渍漆的催化剂浆料的方法,其中二丁基氧化锡首先用有机溶剂和有机酸预分散,例如通常用于中和阴极分离的电泳浸渍漆,因此它是 用粘合剂和水分散并研磨。 2.3阴极电泳浸漆,使用含有二丁基氧化锡的催化剂浆料。