    • 10. 发明授权
    • 폴리머를 포함하는 콘크리트 상판 보수용 몰탈 조성물 및 이를 이용한 보수방법
    • 含有聚合物的修补乳液组合物及其修复方法
    • KR100872518B1
    • 2008-12-08
    • KR1020080082900
    • 2008-08-25
    • 주식회사 한수도로산업
    • 박정호
    • C04B14/02C04B28/00C04B24/00C04B24/02
    • C04B41/53C04B41/009C04B41/5076C04B2103/0045C04B2103/20C04B2103/50C04B2111/00491C04B2111/72C04B41/4869C04B41/4876C04B41/526C04B41/5315C04B28/02
    • A repairing method using a repairing mortar composition containing a polymer is provided to reduce a setting time and to be inexpensive. A repairing method using a repairing mortar composition containing a polymer comprises steps of: removing a weak part of an upper plate of a concrete; cleaning the upper plate of the concrete from which the weak part is removed; maintaining a wetting state of the cleaned weak part; uniformly coating a polymer primer composition for repairing the upper plate of the concrete manufactured by adding water of 3~25 parts by weight based a polymer primer of the upper plate of 100 parts by weight consisting of a powdery polymer of 1-30 weight% selected from a PAE redispersible powder resin, POLY SAE redispersible powder resin, an ultra rapid hardening cement of 70-99 weight%, a POLY ethyl vinyl acetate based redispersible powder resin, and a PVA-VeoVa based redispersible powder resin at the weak part of the wetting state; and installing a mortar composition for repairing the upper plate of the concrete including water of 3~25 weight% and a powdery polymer of 1~10 weight% selected from the PAE based redispersible powder resin, the PVA-VeoVa based redispersible powder resin, the POLY SAE based redispersible powder resin, the ultra rapid hardening cement of 10~46 weight% in the upper plate of the concrete treated by the primer, aggregate of 50~86 weight%, and the POLY ethyl vinyl acetate based redispersible powder resin.
    • 提供使用含有聚合物的修复砂浆组合物的修复方法以减少凝固时间并且便宜。 使用包含聚合物的修复砂浆组合物的修复方法包括以下步骤:去除混凝土的上板的弱部分; 清理掉薄弱部分的混凝土上板; 保持清洁的弱部分的润湿状态; 均匀涂覆聚合物底漆组合物,用于修复通过加入3〜25重量份的水制成的混凝土的上板,基于上板的聚合物底漆为100重量份,由选自1-30重量%的粉末状聚合物 来自PAE可再分散粉末树脂,POLY SAE可再分散粉末树脂,70-99重量%的超快速硬化水泥,基于聚乙酸乙烯酯的可再分散粉末树脂POLY乙烯基乙酸酯,以及基于PVA-VeoVa的可再分散粉末树脂 润湿状态; 并安装用于修复包含3〜25重量%的水的混凝土的上板的砂浆组合物和选自基于PAE的可再分散粉末树脂,PVA-VeoVa基的可再分散粉末树脂的1〜10重量%的粉末状聚合物, POLY SAE基可再分散粉末树脂,超快速硬化水泥10〜46重量%,在底漆混凝土上层处理,骨料50〜86%,聚乙酸乙烯酯基可再分散粉末树脂。