    • 2. 发明授权
    • 변색 전통 전와류의 제조 방법
    • 制作改性颜色的传统瓷砖的方法
    • KR101450175B1
    • 2014-10-14
    • KR1020140069160
    • 2014-06-09
    • 동부요업 주식회사
    • 박문환
    • C04B33/32C04B33/04
    • C04B33/04C04B33/14
    • The present invention relates to a method for manufacturing a traditional clay product with modified colors and, more specifically, to a method for manufacturing a traditional clay product that is not black but is of modified colors mixing slate grey, silver grey, dark brown and black in various patterns. The traditional clay product with modified colors according to the present invention sinters using clay of a unique composition, incompletely combusts the same to make formation of various colors possible, and has an advantage of mass producing high quality traditional clay products with modified colors in a short time by a capsule-type kiln.
    • 本发明涉及一种用于制造具有改性颜色的传统粘土产品的方法,更具体地说,涉及一种不是黑色但具有混合板岩灰色,银灰色,深棕色和黑色的改性颜色的传统粘土产品的制造方法 在各种模式。 根据本发明的具有改性颜色的传统粘土产品使用独特组合物的粘土烧结,不完全燃烧它们以形成各种颜色,并且具有在短时间内大量生产具有改性颜色的高品质传统粘土产品的优点 时间由胶囊型窑。
    • 5. 发明公开
    • 폐건전지 분쇄분말을 이용한 세라믹 점토 벽돌 제조 방법
    • 使用废弃电池粉末制造陶瓷颜色粘土砖的方法
    • KR1020080081801A
    • 2008-09-10
    • KR1020070129022
    • 2007-12-12
    • 임형학
    • 임형학
    • B28B3/20C04B14/10C04B14/06
    • C04B33/32B09B3/0041C04B33/04C04B33/1325C04B33/14C04B35/64C04B2235/3262C04B2235/3284C04B2235/3418C04B2235/349C04B2235/422C04B2235/6021C04B2235/606C04B2235/6562C04B2235/6565C04B2235/9661H01M6/52H01M10/54Y02P40/69Y02W30/84
    • A ceramic clay brick manufacturing method using crushed powder of waste batteries is provided to reduce the cost of purchasing manganese dioxide used as a coloring admixture in producing ceramic clay bricks of black, dark red, or dark brown color. A ceramic clay brick manufacturing method using crushed powder of waste batteries comprises the steps of: crushing the clay mixture in the size of 0.5~2mm by using a roller crusher, wherein the clay mixture is produced by mixing clay of 70wt.%, sand or soil cement of 20~28wt.%, and crushed powder of 2~10wt.% obtained from the waste batteries as a coloring admixture for bricks; kneading the crushed clay mixture to make the water content at 18~22%, extruding the clay mixture in the shape of a brick by using a vacuum extrusion pug mill, and cutting the extruded clay mixture in the predetermined size; drying the extruded and molded bricks for 30~40 hours in a drying chamber, in order to adjust the water content to 0~5%; and preheating, sintering, and cooling the dried bricks at normal temperature or 1000°C, 1000~1200°C, and 1200°C or normal temperature, respectively in a continuous kiln.
    • 提供了使用废电池粉碎的陶瓷粘土砖制造方法,以降低在生产黑色,深红色或深棕色陶瓷粘土砖时用作着色混合物的二氧化锰购买成本。 使用废电池粉碎的陶瓷粘土砖制造方法包括以下步骤:通过使用辊式破碎机将粘土混合物破碎为0.5〜2mm,其中粘土混合物通过混合70重量%的粘土,砂或 20〜28重量%的土壤水泥,废旧电池作为砖的着色混合物得到的2〜10重量%的粉碎粉末; 捏合粘土混合物使其含水量为18〜22%,采用真空挤压搅拌机将粘土混合物挤压成砖状,并以预定尺寸切割挤出的粘土混合物; 在干燥室中干燥挤出成型的砖30〜40小时,以将含水量调节至0〜5%; 并在连续窑中分别在常温或1000℃,1000〜1200℃,1200℃或常温下预热,烧结和冷却干砖。