    • The present invention relates to a method for producing a concrete block which is made to realize the texture of a natural stone and show various colors along with improved resistance. The method reduces the generation of carbon dioxide (CO2) by recycling industrial byproducts. The method according to an embodiment of the present invention comprises the steps of: preparing a first mixture by mixing a slag powder of 5-40 parts by weight with an admixture of 0.1-2.0 parts by weight based on cement of 100 parts by weight; preparing a base layer aggregate by mixing the first mixture of 16-20 parts by weight with an aggregate of 100 parts by weight; producing a first molded material by inserting the base layer aggregate in a mold frame and primarily vibrating and pressurizing the base layer aggregate; preparing a second mixture by mixing a pigment of 0.1-3.0 parts by weight, based on the cement of 100 parts by weight, with the first mixture; preparing a surface layer aggregate by mixing the second mixture of 16-20 parts by weight with an aggregate of 100 parts by weight; producing a second molded material by laminating the surface layer aggregate on the top surface of the first molded product and secondarily vibrating and pressurizing the surface layer aggregate; and curing the second molded material and processing the surface thereof. [Reference numerals] (AA) Prepare a first mixture (Mix cement, a slag powder, and an admixture); (BB) Prepare a base layer aggregate (Mix an aggregate and the first mixture) (Aggregate diameter 0-3 mm 30-45 wt%, 3-6 mm 25-40 wt%, 6-8 mm 15-25 wt%, 8-13 mm 1-10 wt%); (CC) Add the base layer aggregate in a mold frame to be primarily vibrated and pressurized; (DD) Prepare a second mixture (Mix the first mixture and a pigment); (EE) Prepare a surface layer aggregate (Mix an aggregate and the second mixture) (Aggregate diameter 0-2 mm 60-90 wt%, 2-4 mm 10-40 wt%); (FF) Add the surface layer aggregate in a mold frame to be temporarily hardened by a roller; (GG) Secondarily vibrate and pressurize the surface layer aggregate; (HH) Cure; (II) Process surface
    • 本发明涉及一种制造混凝土块的方法,该混凝土块是为了实现天然石材的质地而呈现的各种颜色以及改进的阻力。 该方法通过回收工业副产物来减少二氧化碳(CO2)的产生。 根据本发明实施方案的方法包括以下步骤:通过将5-40重量份的粉末粉末与基于100重量份的水泥的0.1-2.0重量份的混合物混合来制备第一混合物; 通过将16-20重量份的第一混合物与100重量份的骨料混合来制备基底层聚集体; 通过将基层聚集体插入模架中并主要对基层聚集体进行振动和加压来生产第一模塑材料; 通过将基于100重量份的水泥的0.1-3.0重量份的颜料与第一混合物混合来制备第二混合物; 通过将16-20重量份的第二混合物与100重量份的聚集体混合来制备表面层聚集体; 通过在第一模制产品的顶表面上层压表面层聚集体并对表面层聚集体进行二次振动和加压来生产第二模塑材料; 并固化第二模塑材料并加工其表面。 (AA)制备第一混合物(混合水泥,炉渣粉末和混合物); (BB)制备基层骨料(混合骨料和第一混合物)(聚集体直径0-3mm 30-45wt%,3-6mm 25-40wt%,6-8mm 15-25wt% 8-13mm 1-10wt%); (CC)将基层聚集体添加到模架中以主要振动和加压; (DD)准备第二混合物(混合第一混合物和颜料); (EE)制备表面层聚集体(混合聚集体和第二混合物)(聚集体直径0-2mm 60-90重量%,2-4mm 10-40重量%); (FF)将表层聚集体添加到模具框架中以通过辊暂时硬化; (GG)二次振动加压表层聚集体; (HH)治愈; (二)工艺表面