    • 1. 发明授权
    • 사염화 타이타늄 정제 장치 및 이를 이용한 정제 방법
    • KR101860842B1
    • 2018-05-24
    • KR1020180015019
    • 2018-02-07
    • 인천화학 주식회사
    • 김진호황윤후이동현
    • B01D3/32
    • B01D3/32
    • 사염화타이타늄의정제방법및 정제장치가제공된다. 사염화타이타늄사염화타이타늄반응기에서넘어온철과알루미늄등의염화물과용해성고융점염화물및 고형물이함유된비정제사염화타이타늄(Crude TiCl)을강제순환펌프및 탱크, 증발드럼과열교환기(Forced Circulation Pump Tank & Flash Drum, Heat Exchanger) 장치에서사염화타이타늄(TiCl)을증발시켜분리해냄과동시에미네랄오일(Mineral Oil) 이나식용유등을첨가하여바나듐계(Vanadium) 불순물을슬러리(Slurry)화시켜고체-기체로분리제거시킨다. 바나듐(Vanadium)계불순물과미네랄오일이충분히반응할수 있는시간과공간을제공하며비정제사염화타이타늄(Crude TiCl) 및슬러리(Slurry)와미네랄오일이반응에필요한반응열과증발열을제공한다. 제 1 증류탑(1st Distillation Tower)에서는후속공정인제 2 증류탑저부에서유입되는고형물, 고융점슬러리(Slurry)를탑 상부에분사시켜앞 공정으로부터증기에포함되어하부로인입되는고융점불순물등을씻어내리는데용이한구조의버블캡트레이형(Bubble Cap Tray)증류탑을설치한다. 제 2 증류탑(2nd Distillation Tower) 에서는앞 공정에서고융점불순물및 슬러리(Slurry)를거의대부분제거함으로써증류탑내부에막힘현상이없으므로장기간보수없이연속운전가능하다.
    • 2. 发明授权
    • 불소 함유 니켈 슬라임으로부터 고순도 니켈의 제조방법
    • 来自含有镍的硅藻的纯镍的制造方法
    • KR101570795B1
    • 2015-11-23
    • KR1020140187015
    • 2014-12-23
    • 인천화학 주식회사
    • 이상호강용호김광규신기웅
    • C25C1/08C25C7/02
    • C25C1/08C25C7/02
    • 본발명은불소함유니켈슬라임으로부터고순도니켈의제조방법에관한것으로, 구체적으로니켈슬라임을산세및 수세시킨후 수산화물을첨가하고여과시켜니켈슬라임에포함된철 및불소를제거하는단계; 전해정련장치의전해조에전해액을공급하고외부순환관을통해전해액을리시브탱크로배출시킨후 펌프를이용하여전해조의음극이구비되는음극포켓에상기전해액을공급하여전해액을순환시키는단계; 및상기철 및불소가제거된니켈슬라임을전해조의양극이구비되는양극포켓에구비시키고상기양극및 음극에전류를인가하는단계;를포함하는불소함유니켈슬라임으로부터고순도니켈의제조방법에관한것이다.
    • 本发明涉及一种由含有氟的镍泥制造高纯度镍的方法,其特征在于,包括以下步骤:使镍粘泥酸化,用水洗涤镍泥,向镍泥中加入氢氧化物,并过滤镍泥以除去 来自镍泥的铁和氟; 向电解精炼装置的电解槽供给电解液的步骤,通过外循环管将电解液排出到接收罐,并通过泵将电解液供给到具有电解槽的负极的阴极袋,由此 循环电解液; 定位镍粘泥的步骤,其中铁和氟从具有电解槽的正极和负极的两极口袋中去除,并将电流施加到正极和负极。 根据本发明,不需要诸如阳离子交换树脂膜的昂贵的装置,从而显着地降低了工艺成本。
    • 3. 发明授权
    • 무전해 니켈도금폐액으로부터 니켈을 회수하는 방법
    • 从废电镀镍镀层中回收高浓度镍的方法
    • KR101467356B1
    • 2014-12-11
    • KR1020140047786
    • 2014-04-22
    • 인천화학 주식회사
    • 신기웅김진호노민석
    • C22B23/00C22B7/00
    • 본 발명은 무전해 니켈도금폐액으로부터 니켈을 고농도로 회수하는 방법에 관한 것으로서, 좀 더 구체적으로 설명하면, 무전해 니켈도금폐액으로부터 불순물을 제거한 후, 이온교환수지법으로 유기물 등을 제거하여 니켈이 흡착된 이온교환수지를 제조한 다음, 이로부터 산세액으로 처리하여 니켈화합물 용액을 얻고, 이온교환수지를 재생한 후, 재생된 이온교환수지 및 니켈화합물 용액을 이용하여 동일 공정을 반복 수행하여 니켈을 고농도로 회수하는 방법에 관한 것이다.
      이러한, 본 발명은 기존의 수산화니켈의 제조공정에 비해 공정운임 비용을 절감할 수 있으며, 또한 기존의 용액 농축 방법으로 증발법과 같은 고비용의 농축공정이 생략시킬 수 있는 바, 생산비용을 절감하면서도 고농도로 니켈을 제조할 수 있다.
    • 本发明涉及从废弃化学镀镍中回收镍的方法。 根据本发明,从废电镀镍电镀中除去杂质,通过使用离子交换树脂法除去有机材料等来制备吸附了镍的离子交换树脂,通过 酸性溶液处理,再生离子交换树脂,通过使用再生离子交换树脂和镍化合物溶液重复执行相同的工艺来回收高浓度镍。 根据本发明,与现有的氢氧化镍制备方法相比,可以节省工艺费用和成本,并且可以省略使用现有的溶液浓缩方法的蒸发方法等昂贵的浓缩方法。 因此,能够节省生产成本,能够生产高浓度的镍。
    • 5. 发明授权
    • 고순도 설파민산 코발트의 제조방법
    • 高纯度硫酸钴的制备方法
    • KR101305318B1
    • 2013-09-06
    • KR1020130039446
    • 2013-04-10
    • 인천화학 주식회사
    • 김권웅유길재김광규
    • C22B23/00C22B3/04C22B3/42
    • PURPOSE: A method for manufacturing high purity cobalt sulfamate is provided to effectively remove metallic impurities, and to effectively control sulfate ions from a manufacturing process. CONSTITUTION: A method for manufacturing high purity cobalt sulfamate includes: a step of injecting solid sulfamate into cobalt slurry, and then manufacturing a cobalt sulfamate-containing solution with stirring and reacting the solid sulfamate and the cobalt slurry under a temperature of 30 to 60°C at a stirring speed of 200 to 800 rpm for 5 to 15 hours; a step of filtering the cobalt sulfamate-containing solution in order to manufacture a filtered cobalt sulfamate-containing solution; a step of removing metallic impurities from the filtered cobalt sulfamate-containing solution; and a step of depressurizing and concentrating the cobalt sulfamate-containing solution from which the metallic impurities are removed. [Reference numerals] (AA) Sulfate ion (ppm); (BB) Comparative example 1; (CC) Example 1-1; (DD) Amount of increase of SO_4^2 (g/L) depending on metal concentrations (Co content); (EE) Adjust the pH ratio of reaction solution; (FF) Adjust the pH of reaction solution
    • 目的:提供高纯度氨基磺酸钴的制造方法,有效去除金属杂质,有效控制制造工序中的硫酸根离子。 构成:制造高纯度氨基磺酸钴的方法包括:将固体氨基磺酸盐注入钴浆料中,然后搅拌制备含氨基磺酸钴溶液并使固体氨基磺酸盐和钴浆料在30至60℃的温度下反应的步骤 C,搅拌速度为200〜800rpm,搅拌5〜15小时; 过滤含氨基磺酸钴溶液以制备过滤的含氨基磺酸氨酯溶液的步骤; 从过滤的含氨基磺酸氨溶液中除去金属杂质的步骤; 以及将去除了金属杂质的含氨基磺酸钴溶液减压浓缩的工序。 (AA)硫酸根离子(ppm); (BB)比较例1; (CC)实施例1-1; (DD)取决于金属浓度(Co含量),SO_4 ^ 2(g / L)的增加量; (EE)调整反应溶液的pH值; (FF)调节反应溶液的pH值
    • 6. 发明授权
    • 황산니켈 결정의 제조 방법
    • 制备镍硫酸盐晶体的方法
    • KR100981366B1
    • 2010-09-10
    • KR1020090112081
    • 2009-11-19
    • 인천화학 주식회사
    • 강용호
    • C01G53/10C01B17/96
    • PURPOSE: A manufacturing method of a nickel sulfate crystal is provided to simplify the manufacturing process by removing a removal process of hydroxide nickel and nickel carbonate, and a drying process of the nickel sulfate crystal. CONSTITUTION: A manufacturing method of a nickel sulfate crystal comprises the following steps: mixing nickel, sulfuric acid, and water to form a nickel sulfate composition with the pH of 4~6; heating and condensing the nickel sulfate composition to form a nickel sulfate solution with the specific gravity of 1.54~1.56; mixing the specific gravity nickel sulfate solution with the sulfuric acid to form a nickel sulfate strong acid solution with the pH of 2~3; cooling the nickel sulfate strong acid solution, and mixing nickel sulfate powder before crystallizing to form a crystalline nickel sulfate composition; and centrifuge-separating the crystalline nickel sulfate composition to obtain the nickel sulfate crystal.
    • 目的:提供一种硫酸镍晶体的制造方法,通过除去氢氧化镍和碳酸镍的去除工序以及硫酸镍晶体的干燥工序来简化制造工序。 构成:硫酸镍晶体的制造方法包括以下步骤:将镍,硫酸和水混合以形成pH为4〜6的硫酸镍组合物; 加热并冷凝硫酸镍组合物,形成比重为1.54〜1.56的硫酸镍溶液; 将比重硫酸镍溶液与硫酸混合,形成pH为2〜3的硫酸镍强酸溶液; 冷却硫酸镍强酸溶液,并在结晶之前混合硫酸镍粉末以形成结晶硫酸镍组合物; 离心分离结晶硫酸镍组合物,得到硫酸镍晶体。