    • 4. 发明授权
    • 항피브릴화 고광택 아크릴 섬유의 제조 방법
    • 用于生产抗纤维化高光泽丙烯酸纤维的方法
    • KR1019950002813B1
    • 1995-03-27
    • KR1019930000229
    • 1993-01-09
    • 한국과학기술연구원
    • 이화섭조성무박종수조서현
    • D01F6/18
    • The fiber defects such as voids in yarn which were formed during the manufacturing process were removed through the structure elaboration process. For example, AN 25 wt.% and DMSO 75 wt.% were polymerized at 60≦̸C for 7hrs in the presence of initiator AIBN 0.15 mol.% on the basis of AN. The unreacted AN in the polymer solution was removed and the polymer solution was spun into 50% DMSO aqueous solution through the 0.12 mm spinning nozzle and extended as 2.5 times in the 70≦̸C water and then the extended yarn was dried primary at 90-120≦̸C and silicone was applicated on it and dried secondary at 120-170≦̸C and the yarn was extended again as 7.5 times.
    • 纤维缺陷如在制造过程中形成的纱线中的空隙通过结构细化过程被去除。 例如,AN 25重量%和DMSO 75重量%在基于AN的引发剂AIBN 0.15摩尔%的存在下,在60℃下聚合7小时。 除去聚合物溶液中的未反应的AN,并将聚合物溶液通过0.12mm纺丝喷嘴旋转到50%DMSO水溶液中,并在70& C,C水中延伸2.5倍,然后将延伸纱线在90-120℃干燥 ; C和硅胶涂覆在其上,并在120-170℃下干燥二次,C再次延伸7.5次。
    • 5. 发明公开
    • 무연신 초극세 아크릴 섬유의 제조 방법
    • KR1019940018498A
    • 1994-08-18
    • KR1019930000230
    • 1993-01-09
    • 한국과학기술연구원
    • 이화섭엄성진조성무박종수조서현
    • D01F6/18
    • 본 발명은 대기 중으로 압출 방사되었을 때 용매가 자발적으로 상분리되어 나오는 자발 응고에 의한 무연신 초극세 아크릴 섬유의 제조 방법에 관한 것이다. 본 발명은 a)통상의 방법에 따라 아크릴로니트릴 단량체 단독, 또는 아크릴로니트릴 단량체 70중량% 이상과, 1종 이상의 공단량체 30중량% 미만을 유기 용매중에서 중합시켜 제조된 분자량이 150,000~1,500,000이고, 고유 점도가 1~15dl/g인 아크릴 중합체 3 내지 20중량% 농도의 방사 조성물을 얻는 단계, b)상기 단계 a)에서 얻은 방사 조성물을 대기 중으로 압찰 방사하여 가늘게 함으로써 용매가 자발적으로 상분리되어 나오는 발 응고 단계, 및 c)상기 단계 b)에서 얻은 압출 필라멘트를 방사 노즐로부터 일정 거리에서 일정 속도 이상으로 권취하는 단계로 이루어진다. 본 발명의 방법은 다기 중에서 일정 속도 이상으로 권취하여 배향 결정화시켰기 때문에 후연신 없이도 강도를 지닌 초극세 아크릴 섬유를 기존의 아크릴 방사법에 비하여 훨씬 간편하고 경제적으로 제조할 수 있다.