    • 1. 发明公开
    • 마이크로파 세라믹 발열체 조성물 및 그 제조 방법
    • 陶瓷加热元件组成由微波辐射及其制备
    • KR1020030033196A
    • 2003-05-01
    • KR1020010064513
    • 2001-10-19
    • 채경호
    • 채경호
    • C04B35/00
    • C04B35/16A61N2005/066C04B35/64C04B2103/0097C04B2111/00836C04B2111/00965C04B2201/32
    • PURPOSE: Provide is a ceramic heating element composition generating a large quantity of heat at a fast-heating rate by radiating microwaves. Accordingly, the heating elements are applied to dryers, sterilizers, heating vessels for microwave ranges, ceramic heaters, etc. CONSTITUTION: The preparation method of ceramic heating element composition comprises the steps of: mixing 25-60pts.wt. of pottery stone with 5.6-46pts.wt. of metal oxides containing 1.2-10pts.wt of cobalt oxide(Co3O4), 0.8-10pts.wt. of silicon carbide(SiC), 1.2-8pts.wt. of manganese oxide(MnO2), 1.2-8pts.wt. of copper oxide(CuO) and 1.2-10pts.wt. of iron oxide(Fe2O3); adding 18-50pts.wt. of water and 7-22pts.wt. of surfactant; drying the mixture at 110-160deg.C for 1-3hrs; forming; sintering at 900-1200deg.C. The resultant ceramic heating elements are heated at a rate of 130-280 deg.C/min to a temperature of 400-820deg.C.
    • 目的:提供一种通过辐射微波在快速加热速率下产生大量热量的陶瓷加热元件。 因此,将加热元件施加到干燥器,灭菌器,微波炉加热容器,陶瓷加热器等。构成:陶瓷加热元件组合物的制备方法包括以下步骤:将25-60pts.wt。 的陶器与5.6-46pts.wt。 含有1.2-10pts.wt的氧化钴(Co3O4)的金属氧化物,0.8-10pts.wt。 的碳化硅(SiC),1.2-8pts.wt。 的氧化锰(MnO2),1.2-8pts.wt。 的氧化铜(CuO)和1.2-10pts.wt。 的氧化铁(Fe2O3); 增加18-50pts.wt。 的水和7-22pts.wt。 的表面活性剂; 将混合物在110-160℃下干燥1-3小时; 成型; 烧结900-1200℃。 将所得的陶瓷加热元件以130-280℃/分钟的速率加热至400-820℃的温度。