    • 유재기김덕환정득종
    • D02G1/18
    • In the method, unelongated polyester yarns of high orientation (A) and unelongated polyester yarns of low orientation (B) have double refraction index difference of 40 to 80×10-3, Ad/Bd of 1.3 to 2.0, AD/BD of 0.6 to 1.0 and dry heat contractibility difference of 10 to 15 %, 2 kinds of unelongated yarns with Ad being less than 6 denier are interlaced and pass through a transforming hot plates having depressed parts at predetermined intervals so as to be elongated and twisted at Tg+40≦̸C
    • 在该方法中,高取向(A)和低取向(B)的未连续聚酯纱线的未延伸聚酯纱具有40至80×10 -3,Ad / Bd为1.3至2.0的双重折射率差,AD / BD为0.6 至1.0〜10%,干热收缩率差为10〜15%,Ad为小于6旦的2种未连续纱线交织并通过具有凹陷部分的变形热板,以预定间隔延长并扭曲Tg + 40&nlE; C <=热板温度<= Tg + 70&nlE; C。 (Ad =高取向的未长丝单丝的尺寸,Bd =低取向的未长丝单丝的尺寸,AD =高取向的未连续复丝的总尺寸,BD =低取向的未连续复丝的总尺寸,Tg =聚酯长丝的温度 第一过渡点)