    • 1. 发明授权
    • 비정질 실리콘 박막의 결정화 방법
    • 非晶硅薄膜的结晶方法
    • KR100806846B1
    • 2008-02-22
    • KR1020070005608
    • 2007-01-18
    • 성균관대학교산학협력단
    • 이준신황성현정성욱박형준이정인
    • H01L21/324
    • H01L21/324H01L21/02532H01L21/02628H01L21/02667
    • A method for crystallizing an amorphous silicon thin film is provided to coat the silicon thin film with metal particles by immersing a substrate with the amorphous silicon thin film into a metal solution. A metal solution containing a catalytic metal is prepared, and then a substrate(101) deposited with an amorphous silicon thin film(103) is coated with the metal solution. Heat treatment is performed on the coated substrate to crystallize the amorphous silicon thin film. The metal solution further contains a solvent material for melting the catalytic material, and an adhesive material for bonding the catalytic material to the substrate. The metal solution comprises (NiCl2)4H2, (Na8C6H5O7)2H2O, NH4Cl, (NaH2PO2)2H2O, ammonia water and deionized water.
    • 提供了一种使非晶硅薄膜结晶的方法,通过将具有非晶硅薄膜的衬底浸入金属溶液中,用金属颗粒涂覆硅薄膜。 制备含有催化金属的金属溶液,然后用金属溶液涂覆沉积有非晶硅薄膜(103)的基板(101)。 在涂覆的基材上进行热处理以使非晶硅薄膜结晶。 金属溶液还含有用于熔化催化材料的溶剂材料和用于将催化材料粘合到基材上的粘合剂材料。 金属溶液包含(NiCl2)4H2,(Na8C6H5O7)2H2O,NH4Cl,(NaH2PO2)2H2O,氨水和去离子水。
    • 2. 发明授权
    • 산소질화알루미늄 계면층을 갖는 유기 발광 소자 및 그제조방법
    • 具有氧化铝界面层的有机发光装置及其制造方法
    • KR100834820B1
    • 2008-06-03
    • KR1020070005620
    • 2007-01-18
    • 성균관대학교산학협력단
    • 이준신박형준김현민장경수정동근남은경
    • H05B33/20H05B33/22
    • H01L51/5024H01L51/5008H01L51/5012H01L51/5056H01L51/56
    • An organic light emitting device having an aluminum oxynitride interface layer and a method for manufacturing the same are provided to improve light emitting efficiency and to reduce driving voltage in comparison with an organic light emitting device without the interface layer. An organic light emitting device includes an anode(2), a hole transport layer(4), an interface layer(3), a light emitting layer(5), a buffer layer(6), and a cathode(7). The anode is formed on an upper part of a substrate(1). The hole transport layer is formed on an upper part of the anode. The interface layer is formed between the anode and the hole transport layer to facilitate hole injection from the anode to the hole transport layer and made of aluminum oxynitride. The light emitting layer is formed on an upper part of the hole transport layer. The buffer layer is formed on an upper part of the light emitting layer. The cathode is formed on an upper part of the buffer layer.
    • 提供具有氮氧化铝界面层的有机发光器件及其制造方法,以提供与没有界面层的有机发光器件相比的发光效率和降低驱动电压。 有机发光器件包括阳极(2),空穴传输层(4),界面层(3),发光层(5),缓冲层(6)和阴极(7)。 阳极形成在基板(1)的上部。 空穴传输层形成在阳极的上部。 界面层形成在阳极和空穴传输层之间,以便于从阳极到空穴传输层的空穴注入并由氮氧化铝制成。 发光层形成在空穴传输层的上部。 缓冲层形成在发光层的上部。 阴极形成在缓冲层的上部。