    • 3. 发明公开
    • 공기정화용 세라믹필터 제조방법 및 그 세라믹필터 모듈
    • 陶瓷过滤器净化室内空气污染和陶瓷过滤器模块的制造技术
    • KR1020090121839A
    • 2009-11-26
    • KR1020080047942
    • 2008-05-23
    • 강원대학교산학협력단
    • 박영구박준석고재철
    • B01D39/00
    • PURPOSE: A method for manufacturing a ceramic filter for air purification and a ceramic filter module thereof are provided to offer good applicability of the filter applied on various spaces. CONSTITUTION: A method for manufacturing a ceramic filter for air purification includes a step for producing a compound by kneading alumina of 3 ~ 10 weight%, magnesium oxide of 1.5 ~ 5 weight%, titanium oxide of 2 ~ 6 weight%, composite metal oxides of 2 ~ 7 weight%, PVA of 25 ~ 50 weight%, EVA of 15 ~ 40 weight%, a dispersing agent of 1.5 ~ 5 weight%, and an inorganic binder of 1.5 ~ 5 weight%. The compound is adhered to a polymer filter made of PP. The compound is dried at a temperature of 50 ~ 80°C for 20 ~ 50 minutes. A ceramic filter module includes a HEPA filter(10), the ceramic filter(11), and an active carbon filter(13).
    • 目的:提供一种空气净化用陶瓷过滤器的制造方法及陶瓷过滤器组件,能够适用于各种空间的过滤器。 构成:用于空气净化的陶瓷过滤器的制造方法包括:将3〜10重量%的氧化铝,1.5〜5重量%的氧化镁,2〜6重量%的氧化钛,复合金属氧化物 为2〜7重量%,PVA为25〜50重量%,EVA为15〜40重量%,分散剂为1.5〜5重量%,无机粘合剂为1.5〜5重量%。 该化合物粘附在由PP制成的聚合物过滤器上。 该化合物在50〜80℃的温度下干燥20〜50分钟。 陶瓷过滤器模块包括HEPA过滤器(10),陶瓷过滤器(11)和活性炭过滤器(13)。