    • 1. 发明公开
    • 마찰교반접합을 이용한 사각 프레임의 제조방법
    • 制造矩形框架的方法
    • KR1020140111075A
    • 2014-09-18
    • KR1020130023664
    • 2013-03-06
    • (주)태광테크한국알박(주)
    • 김주호노중석소병호윤순겸
    • B23K20/12
    • Disclosed is a method for manufacturing a square frame using friction stir welding whereby sides of the frame in predetermined lengths are prepared, are welded in the shape of ′��prime;, and are usded. According to the present invention, the method includes comprises: a preparation step of preparing four sides of the frame which are made of a material that can be processed by friction stir welding; an arrangement step of arranging the sides of the frame in the shape of ′��prime;; a first welding step of performing friction stir welding on an upper side of a boundary where the sides of the frame meet; and a second welding process of performing friction stir welding on a lower side of a boundary where the sides of the frame meet. It is preferred that the first welding step and the second welding step are performed to be overlapped by each other inside the frame. On both sides of the boundary, an auxiliary plate made of the same material with that of the frame is arranged to closely contact the boundary. Therefore, a tool for friction stir welding may start operation from an outer part of the auxiliary plate and finish the operation at an inner part of the auxiliary plate.
    • 公开了一种使用摩擦搅拌焊接制造正方形框架的方法,其中准备了预定长度的框架的两侧,以“ ”的形式被焊接,并被使用。 根据本发明,该方法包括:制备框架的四边的制备步骤,其由可通过摩擦搅拌焊接加工的材料制成; 布置步骤,将框架的侧面布置成“ prime”; 在框架的两侧相交的边界的上侧执行摩擦搅拌焊接的第一焊接步骤; 以及在框架的两侧相交的边界的下侧进行摩擦搅拌焊接的第二焊接工艺。 优选地,第一焊接步骤和第二焊接步骤在框架内彼此重叠。 在边界的两侧,配置与框架相同的材料制成的辅助板与边界紧密接触。 因此,用于摩擦搅拌焊接的工具可以从辅助板的外部开始操作,并且在辅助板的内部部分完成操作。
    • 2. 发明授权
    • 구조체 및 그 제조방법
    • 其结构和制造方法
    • KR101555628B1
    • 2015-09-25
    • KR1020140090503
    • 2014-07-17
    • 한국알박(주)(주)태광테크
    • 소병호김선영김주호노중석김동규주영환정윤철
    • B23K20/12
    • B23K20/12
    • 본 발명은 구조체 및 그 제조방법에 관한 것으로서, 적어도 두 개의 금속 판재를 용접하여 형성되는 대면적의 구조체로서, 적어도 일측 가장자리에서 연장되어 돌출 형성되는 볼록부가 구비되는 제1금속 판재와, 상기 제1금속 판재의 일측에 구비되며 일측에 상기 볼록부가 삽입되어 맞물려지는 오목부가 구비되는 제2금속 판재를 포함하고, 상기 제1금속 판재와 상기 제2금속 판재 사이에 형성되는 접합선이 상기 제2금속 판재와 마주보는 상기 제1금속 판재의 일측면 직선 길이보다 긴 것을 특징으로 하고, 금속판재를 마찰교반용접으로 접합시킨 후 접합선의 물리적인 특성이 접합 전 금속판재 자체의 물리적인 특성 간의 차이를 저감시킬 수 있다
    • 本发明涉及焊接有至少两块金属板的面积大的结构体及其制造方法。 该结构包括:具有从至少一个边缘突出的凸出部分的第一金属板; 以及第二金属板,设置在所述第一金属板的一侧,并且在一侧具有凸部,以允许所述凸部插入和接合。 第一和第二金属板之间的焊接线比第一金属板的面对第二金属板的一侧的直线长。 在金属板的摩擦搅拌焊接之后,通过焊接线的物理特性可以减少焊接之前的金属板的自身物理特性之间的不同。
    • 3. 发明公开
    • 챔버 및 이의 제조방법
    • 室及其制造方法
    • KR1020160002508A
    • 2016-01-08
    • KR1020140080945
    • 2014-06-30
    • (주)태광테크한국알박(주)
    • 김주호노중석김동규주영환이원천정윤철소병호김선영
    • H01L21/02
    • H01L21/02
    • 본발명은챔버를구성하는구성요소들을마찰교반접합을이용해접합함으로써, 제조공정의단순화로제조시간의단축및 생산비용의절감을도모할수 있을뿐만아니라접합부위에대한결함발생을현저히낮출수 있게하는챔버및 이의제조방법에관한것으로, 수직한사각바(bar) 형상으로제공되는 4개의모서리부재와, 수직한판 형상으로제공되는다수의측벽부재를준비하는단계(S1); 각각의모서리부재및 각각의측벽부재에연결수단을형성하는단계(S2); 연결수단을이용해순차적으로모서리부재와측벽부재를연결하면서모서리부재와측벽부재의이음부를마찰교반접합하여내부가중공되고상부및 하부가열린사각벽체를형성하는단계(S3); 및제조하고자하는챔버의높이에맞게사각벽체의상부및 하부를절삭하는단계(S4);를포함한다.
    • 本发明涉及一种能够促进制造时间缩短和生产成本降低的室,由于制造过程简单,能够显着降低焊接部的缺陷的发生,因为构成室的元件通过摩擦搅拌 焊接及其制造方法。 室的制造方法包括以下步骤:(S1)准备设置成垂直矩形棒形状的四个角部件,以及设置成垂直板形状的多个侧壁件; (S2)在每个拐角构件和每个侧壁构件处形成连接装置; (S3),通过对角部件和侧壁部件的接合部进行摩擦搅拌焊接而形成内部为中空的矩形壁,并且上部和下部打开,同时顺序地将角部件和 侧壁构件; 和(S4)根据要制造的室的高度切割矩形壁的上部和下部。
    • 4. 发明授权
    • 마찰교반접합을 이용한 사각 프레임 수냉판의 제조방법
    • 水冷却板制造方法
    • KR101388964B1
    • 2014-05-26
    • KR1020130023665
    • 2013-03-06
    • (주)태광테크한국알박(주)
    • 김주호노중석소병호윤순겸
    • B23K20/12
    • Disclosed is a method for manufacturing a rectangular frame water cooling plate, which remarkably reduces the manufacturing cost and causes few deformation and defects. According to the present invention, the method includes the steps of preparing frames made of a friction stir weldable material; arranging the frames in the form of ″��Prime; or ″��Prime; and conducting a first friction stir welding for the upper surfaces of the boundary portions of the frames coming into contact with each other; conducting a second friction stir welding for the lower surfaces of the boundary portions of the frames coming into contact with each other; forming grooves along the top center portions of the frames to form passages; forming mounting portions on both sides of the top surface of each passage and welding a cover plate to the mounting portions through friction stir welding; and forming inlet/outlet ports communicating with the passages to circulate cooling water.
    • 公开了一种制造矩形框架水冷却板的方法,其显着降低了制造成本,并且几乎没有变形和缺陷。 根据本发明,该方法包括制备由摩擦搅拌可焊接材料制成的框架的步骤; 以“ Prime”的形式排列框架; 或“ Prime; 并且对于彼此接触的框架的边界部分的上表面进行第一摩擦搅拌焊接; 对彼此接触的框架的边界部分的下表面进行第二摩擦搅拌焊接; 沿着框架的顶部中心部分形成沟槽以形成通道; 在每个通道的顶表面的两侧形成安装部分,并通过摩擦搅拌焊将盖板焊接到安装部分; 并且形成与通道连通以使冷却水循环的入口/出口。
    • 5. 发明公开
    • 후판 접합용 마찰교반접합 공구
    • 用于焊接厚板的摩擦焊接工具
    • KR1020160020007A
    • 2016-02-23
    • KR1020140104303
    • 2014-08-12
    • (주)태광테크
    • 김주호노중석김동규주영환정윤철
    • B23K20/12
    • B23K20/12
    • 본발명은숄더부의면적증대를최소화하면서두께가 100㎜이상인후판을접합할수 있게하는후판접합용마찰교반접합공구에관한것으로, 본발명은원통형상을가지며선단면상에숄더부를형성하는로터, 및숄더부의중심부에서부터로터의회전축선을따라돌출되는프로브를가지는마찰교반접합공구에있어서, 프로브는숄더부의중심부에서부터숄더부의외측으로연장되는원뿔형상을가지고, 프로브의길이는하기관계식 1을만족시키며, 숄더부의직경은하기관계식 2를만족시킨다. [관계식 1] 0.75T ≤ L1
    • 本发明涉及一种用于焊接厚板的摩擦搅拌焊接工具,其可以使肩部单元的面积增加最小化并焊接厚度为100mm或更厚的厚板。 用于焊接厚板的摩擦搅拌焊接工具包括:具有圆柱形形状的转子,并在其前端表面上形成肩部单元; 以及从所述台肩单元的中部沿着所述转子的旋转轴线突出的探针。 探头具有从肩部单元的中间部分朝向肩部单元的外部延伸的锥形。 探头的长度满足以下相互作用公式0.75T <= L1
    • 6. 发明公开
    • 포터블형 마찰교반접합 장치
    • 便携式摩擦焊接装置
    • KR1020160019999A
    • 2016-02-23
    • KR1020140104251
    • 2014-08-12
    • (주)태광테크
    • 김주호노중석김동규주영환정윤철
    • B23K20/12
    • 본발명은기구적인구성을간소화하면서접합헤드의진행거리를선택적으로연장시킬수 있게하는포터블형마찰교반접합장치에관한것으로, 피접합물의맞대어진접합부위를마찰교반접합방식으로접합하는접합헤드부; 상부면상에피접합물들의접합부위가맞대어지도록고정시키는제 1 베드, 및제 1 베드에형성되어마찰교반접합시 접합부위를따라접합헤드부의진행을안내하는한 쌍의제 1 가이드프레임을가지는제 1 베이스; 및접합부위의길이가제 1 베이스의길이보다긴 경우일단이제 1 베드의타단에연결되어제 1 베드와함께피접합물을고정시키는제 2 베드, 및제 2 베드에형성됨과아울러일단이제 1 가이드프레임의타단과연결되어마찰교반접합시 제 1 가이드프레임과함께접합헤드부의진행을안내하는한 쌍의제 2 가이드프레임을가지는제 2 베이스;를포함한다.
    • 本发明涉及一种简化机械结构的便携式摩擦搅拌焊接装置,并且可以选择性地延长焊接头的移动距离。 便携式摩擦搅拌焊接装置包括:焊接头单元,用于通过摩擦搅拌焊接方法焊接彼此接触的目标焊接对象物的焊接部分; 第一基座,包括第一床,用于将目标焊接对象固定在其上表面上,以使目标焊接对象的焊接部彼此接触;以及一对第一引导框架,其形成在第一床上以引导 当摩擦搅拌焊接时焊头单元沿着焊接部分移动; 以及第二基座,其包括连接到所述第一床的另一端的第二床,以便如果所述焊接部分的长度长于所述第一基座的长度,则将所述目标焊接对象与所述第一床固定,以及一对第二引导件 形成在第二床上的框架,其一端连接到第一引导框架的另一端,以在摩擦搅拌焊接时引导焊接头单元与第一引导框架的移动。
    • 9. 发明公开
    • 센터설정장치 및 이를 구비한 파이프 접합설비
    • 中心控制装置和管道焊接机
    • KR1020130082252A
    • 2013-07-19
    • KR1020120003353
    • 2012-01-11
    • (주)태광테크
    • 김주호노중석최동학
    • B23K37/053B23K20/12
    • PURPOSE: A centering device and a pipe welding device with the same are provided to facilitating a welding process and to improve weldability by processing the inner and outer curvature of a base material to be identical. CONSTITUTION: A pipe welding device includes a frame (100), a supporting member (110), a centering device (200), an upper press unit (300), and a welding unit (400). The frame forms an outer shape of the pipe welding device and supports a rolled base material. The supporting member supports a joint portion of the rolled base material to be positioned on the upper of the frame. The centering device sets the joint portion of the base material. The upper press unit presses both sides of a contacted portion of the base material, thereby fixing the base material to the supporting member. The welding unit manufactures a pipe by welding the contacted portion of the base material.
    • 目的:提供一种定心装置和具有该定中心装置的管道焊接装置,以便于焊接过程,并通过将基材的内部和外部曲率加工成相同来提高可焊性。 构造:管道焊接装置包括框架(100),支撑构件(110),定心装置(200),上压力单元(300)和焊接单元(400)。 框架形成管状焊接装置的外形,并且支撑轧制的基材。 支撑构件支撑被轧制的基材的接合部分,以被定位在框架的上部。 定心装置设置基材的接合部分。 上压单元按压基材的接触部分的两侧,从而将基材固定到支撑构件上。 焊接单元通过焊接基材的接触部分来制造管。