    • 생산성이 향상된 식물유래 조성물을 함유한 복합 친환경 장섬유 부직포 및 그 제조방법
    • 包含从植物得到的组合物的复合非织造织物及其制造方法
    • KR1020140083359A
    • 2014-07-04
    • KR1020120153018
    • 2012-12-26
    • 도레이첨단소재 주식회사
    • 김연수박서진윤영일토미오카김동욱윤제득
    • D04H3/007D01D5/34D04H3/147D04H3/016
    • D04H3/007D01D5/34D01F8/06D04H3/016D04H3/105D04H3/153D04H13/00D10B2321/021D10B2321/022D10B2401/12
    • The present invention relates to an eco-friendly composite long-fibrous non-woven fabric containing a plant-derived composition to improve productivity and a method for preparing the same. According to the method for preparing the eco-friendly composite long-fibrous non-woven fabric containing a plant-derived composition to improve productivity of the present invention, a filament constituting the non-woven fabric is formed in a sheath-core type, and polypropylene is positioned for a core component and plant-derived polyethylene is positioned for a sheath component, thereby preparing a composite long-fibrous spunbond non-woven fabric. The method comprises the steps of: respectively melting a core component and a sheath component using separate extruders, spinning the respective polymers through a composite spinning nozzle, giving cooling air to the spun filament to be solidified, and then making the solidified filament into a stretched filament having a small fiber diameter through a stretching procedure; integrating the stretched filament on a porous screen belt, which is continuously driven, to form a non-woven web; and binding the integrated non-woven fabric webs by various methods such as thermal bonding to give shape stability to the non-woven fabric webs, wherein the spinning is performed by adding a phosphorus-based antioxidant as an antioxidant contained in the sheath component. According to the method for preparing the eco-friendly composite long-fibrous non-woven fabric containing a plant-derived composition to improve productivity of the present invention, the phosphorus-based antioxidant is added as an antioxidant contained in the sheath component, thereby remarkably reducing yarn cutting and defects at the time of spinning, and thus improving process stability and increasing productivity of the eco-friendly non-woven fabric.
    • 本发明涉及含有提高生产率的植物来源组合物的环保型复合长纤维无纺布及其制备方法。 根据制备含有植物来源组合物以提高本发明生产率的环保型复合长纤维无纺布的方法,构成无纺布的长丝以皮芯型形成, 将聚丙烯定位成核心部件,并将植物衍生的聚乙烯定位于鞘组分,从而制备复合长纤维纺粘非织造织物。 该方法包括以下步骤:使用单独的挤出机分别熔化芯组分和鞘组分,通过复合纺丝喷嘴纺出各聚合物,向纺丝丝提供冷却空气以固化,然后将固化的长丝制成拉伸 通过拉伸程序具有小纤维直径的丝; 将拉伸的细丝整合在连续驱动的多孔筛网带上,以形成无纺网; 并通过各种各样的方法如热粘合来结合整体的无纺织物幅材,以赋予无纺布幅材的形状稳定性,其中通过添加作为鞘成分中所含的抗氧化剂的磷系抗氧化剂进行纺丝。 根据制备含有植物来源的组合物以提高本发明的生产率的环保型复合长纤维无纺布的方法,作为包含在鞘成分中的抗氧化剂添加磷系抗氧化剂,因此显着地 减少纺丝时的纱线切割和缺陷,从而提高生态环保无纺布的工艺稳定性和生产率。
    • 77. 发明公开
    • 유기매체 흡착용 폴리에스터 장섬유 부직포 및 그 제조방법
    • 用于吸收有机介质的聚酯纺织品的非织造织物及其制备方法
    • KR1020090120583A
    • 2009-11-25
    • KR1020080046466
    • 2008-05-20
    • 도레이첨단소재 주식회사
    • 박서진최필곤김동욱
    • D04H3/14D04H3/016D04H3/011
    • D04H3/011D04H3/016D04H3/147D04H13/00D10B2331/04D10B2505/04
    • PURPOSE: Non woven fabric for polyester textile for adsorption of an organic medium and a method for preparing the same are provided to remove the organic medium rapidly remaining in various printed circuit boards. CONSTITUTION: A method for preparing non woven fabric for polyester textile for adsorption of an organic medium includes a step for forming a non woven fabric laminate and a step for compressing the woven fabric laminate at a temperature of 130~200 °C and with the pressure of 40~80 kg/cm^2 between thermal compression rolls. The nonwoven fabric laminate includes an internal non-woven layer and an outer non-woven layer. The internal non-woven layer is comprised of ethylene terephthalate polymer materials gained by spinning, cooling and drawing ethylene terephthalate, an ethylene terephthalate polymer, and a copolymer of isophthalic acid.
    • 目的:提供用于吸收有机介质的聚酯纺织物的无纺布及其制备方法,以除去快速残留在各种印刷电路板中的有机介质。 构成:用于制备用于吸收有机介质的聚酯织物的无纺织物的方法包括形成无纺织物层压体的步骤和在130〜200℃的温度下压缩机织织物层压体的步骤和压力 热压辊之间为40〜80 kg / cm ^ 2。 无纺布层压体包括内部无纺布层和外部无纺布层。 内部无纺布层由通过纺丝,冷却和拉伸对苯二甲酸乙二醇酯,对苯二甲酸乙二醇酯聚合物和间苯二甲酸共聚物获得的对苯二甲酸乙二醇酯聚合物材料组成。
    • 78. 发明公开
    • 섬유속 및 웹
    • 光纤网络和网络
    • KR1020090027768A
    • 2009-03-17
    • KR1020097002683
    • 2007-08-10
    • 이에스 화이바비젼즈 가부시키가이샤이에스 화이바비젼즈 홍콩 리미티드이에스 화이바비젼즈 리미티드 파트너쉽이에스 화이바비젼즈 아페에스
    • 미야우치미노루시모쓰유키하루마에카와아키노리
    • D04H3/016D01D5/34D04H3/018
    • D04H13/002D01F8/06D01F8/14D04H1/42D04H3/018D04H3/02D04H3/147Y10T428/24132Y10T428/2924
    • There is provided a fiber bundle that strikes an excellent balance between the properties and performance of the resulting web and the finished products obtained from this web, and cost, ease of work, and productivity. There is also provided a method for manufacturing a web using this fiber bundle. There is also provided a web that is uniform and has excellent soft touch and bulkiness. This is achieved by a fiber bundle with a total denier of 10,000 to 500,000 dtex, obtained by bundling thermoplastic, conjugate, continuous fibers that have a single filament denier of 0.5 to 100 dtex/f and in which the center of gravity of conjugate components varies among the conjugate components in a fiber cross section, wherein the thermoplastic, conjugate, continuous fibers that make up the fiber bundle have a spontaneous crimp of 8 to 30 crimps per 2.54 cm, the fiber bundle density as defined by D1/(W1 L L1) (where D1 is the total denier, W1 is the fiber bundle width, and L1 is the fiber bundle thickness) is 100 to 2000 dtex/mm2, and the density ratio by spreading (the web density/fiber bundle density after spreading by drawing to a ratio of 1.6 in a pinch roller spreading machine at a rate of 25 m/min and a fiber bundle temperature of 25) is 0.10 or less.
    • 提供了一种纤维束,其在所得到的纤维网的性能和性能以及从该纤维网获得的成品之间达到极好的平衡,并且成本,易于工作和生产率。 还提供了一种使用该纤维束制造网的方法。 还提供了均匀且具有优良的柔软触感和蓬松性的网。 这通过具有10,000至500,000dtex的总旦数的纤维束实现,其通过将具有0.5至100dtex / f的单丝旦数的热塑性共轭连续纤维捆扎而获得,并且其中共轭组分的重心变化 在纤维横截面中的共轭组分中,其中构成纤维束的热塑性共轭连续纤维每2.54cm具有8至30个卷曲的自发卷曲,由D1 /(W1L L1 )(D1为总旦数,W1为纤维束的宽度,L1为纤维束的厚度)为100〜2000dtex / mm 2,扩展后的密度比(通过拉伸扩展后的纤维网密度/纤维束密度 在挤压辊式撒布机中以25m / min的速度和25束的纤维束温度的比例为1.6)为0.10以下。