热词
    • 72. 发明授权
    • 점착제 조성물
    • 粘合剂组合物
    • KR101314202B1
    • 2013-10-02
    • KR1020130002029
    • 2013-01-08
    • 동우 화인켐 주식회사
    • 최한영유지희
    • C09J175/04C09J133/04C09J9/00
    • C09J175/04C08G18/6229C08G18/6254C08G18/672C09J133/066
    • PURPOSE: An adhesive composition is provided to remarkably improve antistatic property and durability without increasing viscosity, thereby reducing curing period without using a crosslinking catalyst. CONSTITUTION: An adhesive composition contains 100.0 parts by weight of an acrylic copolymer, 0.1-3 parts by weight of an isocyanate-based crosslinking agent, and 0.1-5 parts by weight of an ionic antistatic agent. The curing period at 23°C, 65% RH is 24 hours or less. The viscosity change before and after maintaining it at 24 hours is 50 % or less. The acrylic copolymer contains 68-95.9 parts by weight of C1-12 alkyl group-containing (meth)acrylate monomer, 5-20 parts by weight of a (meth)acrylic acid, and 0.5-2 parts by weight of 4-hydroxybutylacrylate based on 100.0 parts by weight of the total weight of the copolymer.
    • 目的:提供粘合剂组合物以显着提高抗静电性和耐久性而不增加粘度,从而在不使用交联催化剂的情况下减少固化时间。 构成:粘合剂组合物含有100.0重量份的丙烯酸共聚物,0.1-3重量份的异氰酸酯基交联剂和0.1-5重量份的离子抗静电剂。 23℃,65%RH的固化时间为24小时以下。 在24小时保持前后的粘度变化为50%以下。 丙烯酸共聚物含有68-95.9重量份的含C1-12烷基的(甲基)丙烯酸酯单体,5-20重量份(甲基)丙烯酸,和0.5-2重量份的基于丙烯酸4-羟基丁酯的 100.0重量份的共聚物的总重量。
    • 75. 发明公开
    • 점착제 조성물, 이를 이용한 점착제층 및 편광판
    • 胶粘组合物,粘合层和偏光板
    • KR1020130020541A
    • 2013-02-27
    • KR1020120061565
    • 2012-06-08
    • 동우 화인켐 주식회사
    • 정경문유지희한은구
    • C09J133/04C09J7/00G02B5/30
    • C09J133/26G02B5/30
    • PURPOSE: An adhesive composition is provided to obtain an adhesion and durability for adhesive by using a low molecular weight copolymer and to reduce curing period. CONSTITUTION: An adhesive composition comprises an acrylic copolymer, an isocyanate-based crosslinking agent, a polyfunctional (meth)acrylate monomer, and a photopolymerization initiator. The acrylic copolymer is obtained by copolymerizing 94-99 weight% of a (meth)acrylate monomer with a C1-12 alkyl group; and 1-6 weight% of a polymerizable monomer which contains an amide-containing monomer, a carboxy-containing monomer, and a hydroxy-containing monomer. The weight ratio of the amide-containing monomer to the carboxy-containing monomer is 0.5-10. The weight average molecular weight of the adhesive composition is 200,000-900,000.
    • 目的:提供粘合剂组合物以通过使用低分子量共聚物获得粘合剂的粘合性和耐久性,并减少固化时间。 构成:粘合剂组合物包含丙烯酸共聚物,异氰酸酯类交联剂,多官能(甲基)丙烯酸酯单体和光聚合引发剂。 丙烯酸共聚物通过使94-99重量%的(甲基)丙烯酸酯单体与C 1-12烷基共聚而获得; 和1-6重量%的含有酰胺的单体,含羧基的单体和含羟基的单体的可聚合单体。 含酰胺单体与含羧基单体的重量比为0.5-10。 粘合剂组合物的重均分子量为20万〜90万。
    • 77. 发明公开
    • 태양전지 이면 보호 시트용 접착제 조성물, 접착제층 및 이면 보호 시트
    • 太阳能电池背面保护片,粘合层和背面保护片的粘合剂组合物
    • KR1020120137779A
    • 2012-12-24
    • KR1020110056828
    • 2011-06-13
    • 동우 화인켐 주식회사
    • 한은구정경문유지희
    • C09J133/06C09J11/06C09J7/02
    • C09J133/062C09J7/22C09J7/30C09J7/385C09J11/06C09J133/066C09J2201/606C09J2203/322
    • PURPOSE: An adhesive composition for protecting backside of solar battery is provided to minimize the adhesion loss even under high temperature and/or high humid environment, and to obtain durability and adhesion. CONSTITUTION: An adhesive composition for protecting backside of a solar battery comprises: an acryl-based copolymer of which weight-average molecular weight is 10,000-1,000,000 and the glass transition temperature is (-22) - 20 °C, and a crosslinking agent. The adhesive layer is formed by hardening an adhesive composition for protecting the backside of a solar battery. The glass transition temperature of the adhesive layer is (-5)-30 °C. A protection sheet is that at least two or more pieces of films are attached by the adhesive composition as a medium. [Reference numerals] (AA,CC) Film; (BB) Adhesive layer
    • 目的:提供一种用于保护太阳能电池背面的粘合剂组合物,即使在高温和/或高湿度环境下也能最小化粘附损失,并获得耐久性和粘附性。 构成:用于保护太阳能电池背面的粘合剂组合物包括:重均分子量为10,000-1,000,000和玻璃化转变温度为(-22)-20℃的丙烯酸类共聚物和交联剂。 通过硬化用于保护太阳能电池的背面的粘合剂组合物来形成粘合剂层。 粘合剂层的玻璃化转变温度为(-5)-30℃。 保护片是通过粘合剂组合物作为介质连接至少两片以上的薄膜。 (标号)(AA,CC)膜; (BB)粘合层
    • 78. 发明公开
    • 점착제 조성물, 이를 포함하는 편광판 및 액정표시장치
    • 胶粘组合物,包含它们的极化板和液晶显示装置
    • KR1020120071372A
    • 2012-07-02
    • KR1020120051597
    • 2012-05-15
    • 동우 화인켐 주식회사
    • 유지희이상진정경문
    • C09J11/06C09J133/04G02B5/30G02F1/13
    • C09J11/06B32B2457/202C08K5/0025C09J133/04G02B5/30G02F1/13
    • PURPOSE: An adhesive composition is provided to remarkably reduce curing period, maintaining physical properties required for an existing adhesive, to improve productivity, and to obtain enough pot-life. CONSTITUTION: An adhesive composition comprises an acrylic copolymer containing a functional group which is cross-linkable with isocyanate, an isocyanate-based cross-linking agent, a silane coupling agent, a cross-linking promoter in chemical formula 1. In chemical formula 1, X is aliphatic amine group. The aliphatic amine group is a pyrrolidine group, or a piperidine group. The cross-linking agent is a mixture of 4-pyrrolidinopyridine, 4-piperidinopyridine, and a mixture thereof. In a polarizing plate, an adhesive layer consisting of the adhesive composition is laminated. A liquid crystal display device comprises the polarizing plate on at least one side of a liquid crystal cell.
    • 目的:提供粘合剂组合物以显着降低固化时间,保持现有粘合剂所需的物理性能,提高生产率,并获得足够的使用寿命。 组成:粘合剂组合物包含含有可与异氰酸酯交联的官能团的丙烯酸共聚物,异氰酸酯基交联剂,硅烷偶联剂,化学式1中的交联促进剂。在化学式1中, X是脂族胺基。 脂族胺基是吡咯烷基或哌啶基。 交联剂是4-吡咯烷基吡啶,4-哌啶基吡啶及其混合物的混合物。 在偏光板中,层叠由粘合剂组合物组成的粘合剂层。 液晶显示装置包括在液晶单元的至少一侧上的偏振片。
    • 80. 发明公开
    • 편광자의 제조방법
    • 制备极化剂的方法
    • KR1020120002815A
    • 2012-01-09
    • KR1020100063517
    • 2010-07-01
    • 동우 화인켐 주식회사
    • 유지희조성우
    • G02B5/30G02F1/1335H05B33/02
    • C09K19/54
    • PURPOSE: A polarizer manufacturing method is provided to improve optical characteristics, thereby reducing the thickness of a polarizer and increasing the area of the polarizer without wrinkles and ruptures of a film in a high stretching ratio condition. CONSTITUTION: A polarizer manufacturing method is comprised of a first cross-linking step and a second cross-linking step. A polyvinyl alcohol film is dipped in a first cross-linking aqueous solution in the first cross-linking step. The first cross-linking aqueous solution includes a boron compound. The polyvinyl alcohol film is dipped in a second cross-linking aqueous solution in the second cross-linking step. The second cross-linking aqueous solution includes a cyclic polybasic carboxylic acid compound which has two or more carboxyl groups.
    • 目的:提供一种提高光学特性的偏振片制造方法,从而降低偏振器的厚度,并且在高拉伸比条件下增加偏振片的面积而不产生褶皱和膜的破裂。 构成:偏振器制造方法由第一交联步骤和第二交联步骤组成。 在第一交联步骤中将聚乙烯醇膜浸入第一交联水溶液中。 第一交联水溶液包括硼化合物。 在第二交联步骤中将聚乙烯醇薄膜浸渍在第二交联水溶液中。 第二交联水溶液包含具有两个以上羧基的环状多元羧酸化合物。