    • 석재 슬러지 블록 및 제조방법
    • 石灰泥块及其生产方法
    • KR1020130111054A
    • 2013-10-10
    • KR1020120033546
    • 2012-03-30
    • 박수만
    • 박수만
    • C04B18/12C04B14/02B28B1/14B28B11/24
    • Y02W30/93C04B18/12B28B1/14B28B11/24C04B14/02C04B18/0418
    • PURPOSE: A stone sludge block and a manufacturing method thereof are provided to manufacture stone sludge block with excellent strength at low cost through a simple mixing process by using stone sludge and burning process sludge. CONSTITUTION: A manufacturing method of stone sludge block comprises the following steps: (S1) producing first mixed sludge by mixing stone sludge with cement; (S2) manufacturing second mixing sludge by mixing the first mixing sludge with burner sludge; (S3) manufacturing a block mixture by mixing the second mixing sludge, water and admixture; and (S4) curing the block mixture. The second mixing sludge includes stone sludge, cement and burner sludge at a weight ratio of 1-3:1-1.5:3-4. The second mixing sludge additionally includes stone powder. The cement is super-high-early-strength cement and the admixture includes fluidifier. The curing is performed at 5-40°C for 8-12 days. [Reference numerals] (AA) First mixed sludge + burner sludge; (BB) First mixed sludge + burner sludge + stone powder; (CC) Second mixed sludge; (S1) Aggregate sludge + cement → first mixed sludge; (S3) Second mixed sludge + water + compound + waterproof solution → block composite; (S4) Grinding, processing after curing block composite
    • 目的:提供石泥泥块及其制造方法,通过使用石泥和燃烧工艺污泥的简单混合工艺,以低成本制造出具有优异强度的石泥块。 构成:石泥块的制造方法包括以下步骤:(S1)通过将石泥与水泥混合生产第一混合污泥; (S2)通过将第一混合污泥与燃烧器淤泥混合来制造第二混合污泥; (S3)通过混合第二混合淤泥,水和混合物制造块混合物; 和(S4)固化块状混合物。 第二个混合污泥包括重量比为1-3:1-1.5:3-4的石泥渣,水泥和燃烧泥浆。 第二混合污泥还包括石粉。 水泥是超高强度水泥,混合物包括流化剂。 固化在5-40℃下进行8-12天。 (附图标记)(AA)第一混合污泥+燃烧器污泥; (BB)首先混合污泥+燃烧器污泥+石粉; (CC)第二混合污泥; (S1)聚集污泥+水泥→第一混合污泥; (S3)第二混合污泥+水+复合+防水溶液→块复合材料; (S4)研磨,加工后固化块复合