    • 21. 发明公开
    • 내화성능이 향상된 CFT 용 콘크리트 조성물
    • CFT混凝土组合物的耐火能力
    • KR1020130096474A
    • 2013-08-30
    • KR1020120017952
    • 2012-02-22
    • 주식회사 포스코건설
    • 김현배이종인김우재유조형홍석범
    • C04B14/38C04B16/06C04B24/24C04B14/02
    • C04B14/38C04B14/02C04B16/06C04B24/287C04B2111/28
    • PURPOSE: A concrete composition for concrete filled tube (CFT) with improved fire resisting capacity is provided to improve mobility at a solid state and workability, rigidity and fire resisting capacity after being solid by comprising a nylon fiber, a long steel fiber, and a short steel fiber. CONSTITUTION: A concrete composition for concrete filled tube (CFT) with improved fire resisting capacity comprises: 150-200 kg of water; 800-950 kg of binding material; 400-500 kg of fine aggregate; 700-900 kg of coares aggregate; 6-20kg of polycarboxylic acid based water reducing agent; 5-40 kg steel fiber; and 1-2 kg of nylon fiber per unit volume 1m^3. A water to binder ratio (W/B) of the concrete composition for CFT is 17-18%, and the fine aggregate percentage (S/a) is 35-40%. The steel fiber comprises a long steel fiber which has a length less than 55 mm and over 50 mm, a short steel fiber which has a length less than 15 mm and over 5 mm. The long steel fiber is used along with the short steel fiber as a ratio of 1:1.
    • 目的:提供具有改善的耐火能力的混凝土填充管(CFT)的混凝土组合物,以通过包括尼龙纤维,长钢纤维和长纤维的纤维来提高固体的移动性和固化后的可加工性,刚性和耐火能力 短钢纤维。 构成:具有改善耐火能力的混凝土填充管(CFT)的混凝土组合物包括:150-200kg水; 800-950公斤装订材料; 400-500公斤细骨料; 700-900公斤的骨料; 6-20kg多元羧酸减水剂; 5-40公斤钢纤维; 和1-2kg尼龙纤维每单位体积1m ^ 3。 CFT混凝土组合物的水与粘合剂比(W / B)为17-18%,细骨料比(S / a)为35-40%。 钢纤维包括长度小于55mm和超过50mm的长钢纤维,长度小于15mm且超过5mm的短钢纤维。 长钢纤维与短钢纤维一起以1:1的比例使用。