    • 19. 发明公开
    • 산소부화용 카본 멤브레인 제조방법
    • 制造碳膜以加入氧气的方法
    • KR1020090067431A
    • 2009-06-25
    • KR1020070135103
    • 2007-12-21
    • 주식회사 포스코재단법인 포항산업과학연구원
    • 이종규
    • B01D71/44
    • A method of manufacturing a carbon membrane for oxygen enrichment is provided to improve permeability and selectivity by increasing the contraction ratio of the membrane. A method of manufacturing a carbon membrane for oxygen enrichment comprises the steps of: primarily pyrolyzing a polyethylene naphthalate film in an inert gas atmosphere of a furnace in which a temperature of 300 to 500 deg.C is maintained for 0.5 to 1 hour; and secondly pyrolyzing the polyethylene naphthalate film in an inert gas atmosphere containing oxygen of a furnace in which a temperature of 700 to 800 deg.C is maintained for 1 to 2 hours. The polyethylene naphthalate film is prepared by using naphthalate that is an aromatic compound as raw material. The insert gas contains 0.5 to 1% of oxygen in the second pyrolysis process.
    • 提供制造用于富氧的碳膜的方法,以通过增加膜的收缩比来提高渗透性和选择性。 制造用于富氧的碳膜的方法包括以下步骤:主要在保持温度为300-500℃的炉的惰性气体气氛中将聚萘二甲酸乙二醇酯膜热解0.5至1小时; 其次将聚萘二甲酸乙二醇酯膜在含有700〜800℃温度的炉的氧气的惰性气氛中热解1〜2小时。 聚萘二甲酸乙二醇酯膜通过使用作为原料的芳香族化合物的萘二甲酸酯制备。 插入气体在第二热解过程中含有0.5至1%的氧气。
    • 20. 发明授权
    • 전기탈이온 장치용 이온교환섬유
    • 전기탈이온장치용이온교환섬유
    • KR100454093B1
    • 2004-10-26
    • KR1020020009927
    • 2002-02-25
    • 광주과학기술원
    • 문승현최용진연경호
    • B01D71/44B01D61/44D01F6/46
    • PURPOSE: An ion exchange textile which is easily handled compared to conventional ion exchange resin used as ion conductive spacer and has very high ion removal efficiency by having non-crosslinking bond, thereby increasing overall specific surface area, rate constant and permeability coefficient. CONSTITUTION: The ion exchange textile for electrodeionization process is characterized in that it is obtained by graft polymerizing a monomer having ion exchange group onto polyolefin based textile irradiated by radiation, wherein the ion exchange textile has overall rate constant (k) of 140 to 150 h¬-1 and permeability coefficient of 17,000 to 19,000 L/hr·m·atm, wherein density of the polyolefin based textile is 0.2 to 0.6 g/cm¬3, wherein the total amount of radioactive rays is 10 to 100 kGy, and wherein the monomer having ion exchange group is selected from sodium sulfonic acid derivative, potassium sulfonic acid derivative, vinylbenzyl trimethyl ammonium chloride, vinylbenzyl triethyl ammonium chloride, vinylbenzyl chloride, vinylbenzyl pyridinium chloride, and vinylbenzyl pyridinium bromide.
    • 目的:与用作离子导电间隔物的常规离子交换树脂相比,易于处理的离子交换织物,并且由于具有非交联键而具有非常高的离子去除效率,由此增加总比表面积,速率常数和渗透系数。 构成:用于电去离子过程的离子交换织物的特征在于它是通过将具有离子交换基团的单体接枝聚合到辐射辐照的聚烯烃基织物上而获得的,其中离子交换织物具有140至150小时的总速率常数(k) ; -1和17,000至19,000L / hr& m& midm; atm的渗透系数,其中聚烯烃基织物的密度为0.2至0.6g / cm 3;其中放射性射线的总量为10至100 kGy,并且其中具有离子交换基团的单体选自磺酸钠衍生物,磺酸钾衍生物,乙烯基苄基三甲基氯化铵,乙烯基苄基三乙基氯化铵,乙烯基苄基氯,乙烯基苄基吡啶鎓氯化物和乙烯基苄基吡啶鎓溴化物。