    • 16. 发明公开
    • Organic light emitting display and manufacturing method of the same
    • 有机发光显示及其制造方法
    • KR20100027902A
    • 2010-03-11
    • KR20080087001
    • 2008-09-03
    • LG DISPLAY CO LTD
    • YOO DONG HEE
    • H05B33/04H01L51/50
    • H01L27/3211H01L21/02211H01L22/12H01L41/39H01L2251/558
    • PURPOSE: An organic electroluminescent display device and a manufacturing method thereof are provided to protect a sub pixel formed in a substrate from the moisture by forming an adhesive member between a substrate and a sealing substrate facing the substrate. CONSTITUTION: A sub pixel(120) is formed on a substrate(110). The sub pixel is formed to a passive matrix type or an active matrix type. A surface(130) of an upper electrode is changed to N Rich state by executing a nitrogen plasma to the upper electrode of the sub pixel. At least three layered inorganic protective film(140) is formed on the sub pixel. The inorganic protective film comprises a first inorganic protective film(141), a second inorganic protective film(142) which is thicker than the first inorganic protective film, and a third inorganic protective film(143) which is thinner than the second inorganic protective film.
    • 目的:提供一种有机电致发光显示装置及其制造方法,通过在基板与面向基板的密封基板之间形成粘接部件来保护形成在基板上的子像素与水分。 构成:在衬底(110)上形成子像素(120)。 子像素形成为无源矩阵型或有源矩阵型。 通过对子像素的上电极执行氮等离子体,使上电极的表面(130)变为N浓度。 在子像素上形成至少三层无机保护膜(140)。 无机保护膜包括比第一无机保护膜厚的第一无机保护膜(141),第二无机保护膜(142)和比第二无机保护膜薄的第三无机保护膜(143) 。
    • 17. 发明公开
    • 유기물 및 나노 미세기공을 함유하는 PZT계 압전 후막및 이의 제조 방법
    • 含PZT的压电薄膜含有机材料和纳米孔及其制备方法
    • KR1020080111641A
    • 2008-12-24
    • KR1020070059845
    • 2007-06-19
    • 한국기계연구원
    • 한병동박동수최종진
    • H01L41/16H01L41/18B82Y40/00
    • H01L41/1876C04B35/491H01L41/316H01L41/39
    • A PZT based piezoelectric thick film containing an organic compound and nano pore and a manufacturing method thereof are provided to shorten film deposition time and be manufactured with rapid thermal processing heating-up and cooling speed and have high stability as thickness of a film which can be evaporated is thick. A PZT based piezoelectric thick film comprises: an organic material containing Pb which is one or more selected from the group consisting of lead acetate[Pb(CH3CO2)23H2O] and lead nitrate[Pb(NO3)2]; an organic material containing Zr which is one or more selected from the group consisting of zirconium propoxide, zirconium ethoxide, zirconium butoxide and zirconium chloride; and an organic material containing Ti which is one or more selected from the group consisting of titanium propoxide, titanium ethoxide, titanium butoxide and titanium chloride.
    • 提供了含有有机化合物和纳米孔的PZT基压电厚膜及其制造方法,以缩短膜沉积时间,并且以快速热处理加热和冷却速度制造,并且具有作为膜的厚度的高稳定性 蒸发浓 基于PZT的压电厚膜包括:含有Pb的有机材料,其是选自乙酸铅[Pb(CH 3 CO 2)2·3H 2 O]和硝酸铅[Pb(NO 3)2]中的一种或多种; 含有Zr的有机材料是选自丙酸锆,乙醇锆,丁氧基锆和氯化锆中的一种或多种的有机材料; 以及含有Ti的有机材料,其为选自丙醇钛,乙醇钛,丁醇钛和氯化钛中的一种或多种。
    • 19. 发明公开
    • 고출력 압전세라믹스와 이를 이용한 트랜스포머
    • 高输出压电陶瓷和使用它的变压器
    • KR1020040091803A
    • 2004-11-02
    • KR1020030025373
    • 2003-04-22
    • 류주현
    • 류주현정영호
    • C04B35/491
    • H01L41/187C04B2235/3251H01L41/39
    • PURPOSE: Provided are a high-output piezoelectric ceramics based on PNW-PMN-PZT, which has high strength and improved piezoelectric characteristics including quality coefficient, dielectric constant and grain size. CONSTITUTION: The piezoelectric ceramics comprise the composition of (Pb0.94Sr0.06)£(Ni1/2W1/2)0.02(Mn1/3Nb2/3)0.07(Zr0.51Ti0.49)0.91|O3 + 0.5 wt% of PbO + 0.3 wt% of Fe2O3 + 0.25 wt% of CeO2, to which Nb2O5 is added as an additive. The additive, Nb2O5 is added in an amount of 0.1-0.5 wt%, preferably in the amount of 0.3 wt%. The piezoelectric ceramics provide a piezoelectric transformer, particularly for use in PDAs, having excellent piezoelectric characteristics.
    • 目的:提供基于PNW-PMN-PZT的高输出压电陶瓷,其具有高强度和改善的压电特性,包括质量系数,介电常数和晶粒尺寸。 构成:压电陶瓷包含(Pb0.94Sr0.06)£(Ni1 / 2W1 / 2)0.02(Mn1 / 3Nb2 / 3)0.07(Zr0.51Ti0.49)0.91 | O3 + 0.5wt%的PbO + 0.3重量%的Fe 2 O 3 + 0.25重量%的CeO 2,添加Nb 2 O 5作为添加剂。 添加剂Nb 2 O 5的添加量为0.1-0.5重量%,优选为0.3重量%。 压电陶瓷提供压电变压器,特别是用于PDA中,具有优良的压电特性。
    • 20. 发明公开
    • 공침전법에 의한 압전세라믹스 제조방법
    • 通过共同生产方法制造压电陶瓷
    • KR1020030026271A
    • 2003-03-31
    • KR1020030010600
    • 2003-02-20
    • 학교법인 동의학원최재업
    • 최재업이병우
    • C04B35/622
    • H01L41/1876H01L41/39
    • PURPOSE: A production method of piezoelectric ceramic powder by coprecipitation is provided, which simplifies filtering and washing, and improves sintering density and forms crystalline microstructure by using nitrates and ammonium oxalates instead of chlorides as raw materials and (Zr·Ti)-peroxynitrate. CONSTITUTION: The lead zirconate titanate(PZT) powder is prepared by mixing Pb(NO3)2 solution with (Zr·Ti)-peroxynitrate(ZrxTi1-xO2(NO3)2) solution in a composition ratio of PbZrxTi1-xO3 (0
    • 目的:提供通过共沉淀制备压电陶瓷粉末的方法,通过使用硝酸盐和草酸铵代替氯化物作为原料和(Zr·Ti) - 过氧化硝酸盐,简化了过滤和洗涤,提高了烧结密度,形成结晶微观结构。 构成:以PbZrxTi1-xO3(0 <= 1)的组成比混合Pb(NO3)2溶液与(Zr·Ti) - 过氧硝酸盐(ZrxTi1-xO2(NO3)2)溶液),制备钛酸锆酸铅(PZT) x <= 1),加入H 2 O 2,将混合溶液滴加到氨水中,洗涤共沉淀,并在30分钟内在600℃下煅烧。 (Zr·Ti) - 过氧硝酸盐溶液是通过以Zr x Ti 1-x O 2(0 <= x <= 1)的组成比混合ZrOCl 2或ZrO(NO 3)2作为锆源和TiCl 4作为钛源的步骤, ,并加入H 2 O 2,得到红色溶液; 将混合溶液滴加到碱性溶液如NH 4 OH,NaOH或KOH中以形成沉淀,白色过氧化物络合物; 过滤和洗涤,直到从析出物中除去Cl-离子; 将获得的沉淀物溶解在稀HNO 3中。 另外,由(1-y)PbZr x Ti1-xO3 + y(zM1O3 +(1-z)M2O5)的组成式表示的掺杂有M3 +(La)或M5 +(Nb)的锆钛酸铅(PZT),其中0 < x = 1,0 <= y <= 0.05,0 <= z <= 1,M1:三价金属(M3 +:Y,La)和M2:五价金属(M5 +:V,Nb) (Zr·Ti) - 过氧化钛(Zr x Ti 1-x O 2(NO 3)2)溶液的Pb(NO 3)2溶液,(La,Nb)添加的PZT溶液中加入La(NO3)3和铌(Nb) 将混合溶液加入氨水中,洗涤形成共沉淀,并在600℃下煅烧30min以上。