    • 8. 发明专利
    • Surface treatment material
    • 表面处理材料
    • JP2014141364A
    • 2014-08-07
    • JP2013009924
    • 2013-01-23
    • Bekku Kkベック株式会社
    • ISHIZUNO MASAFUMI
    • C04B41/50C04B24/26C04B28/02C04B41/48C09D1/08C09D5/02C09D201/02
    • PROBLEM TO BE SOLVED: To obtain a surface treatment material excellent in adhesion and durability.SOLUTION: A surface treatment material includes a powder composition containing cement and a liquid composition containing a synthetic resin emulsion. The powder composition contains 50 wt.% or more of the cement. The synthetic resin emulsion in the liquid composition comprises a cationic group and/or nitrile group-containing synthetic resin emulsion (x) having an average particle diameter of 0.5 μm or less and a synthetic resin emulsion (y) having an average particle diameter larger than the synthetic resin emulsion (x). The cement and the synthetic resin emulsion is mixed so that the weight ratio of the solid content is 100:1-50.
    • 要解决的问题:获得粘合性和耐久性优异的表面处理材料。溶液:表面处理材料包括含有水泥的粉末组合物和含有合成树脂乳液的液体组合物。 粉末组合物含有50重量%以上的水泥。 液体组合物中的合成树脂乳液包含平均粒径为0.5μm以下的含阳离子性基团和/或含腈基的合成树脂乳液(x),平均粒径大于的平均粒径的合成树脂乳液(y) 合成树脂乳液(x)。 将水泥和合成树脂乳液混合,使固体成分的重量比为100:1-50。