    • 4. 发明专利
    • Optical glass, and optical element
    • 光学玻璃和光学元件
    • JP2010260739A
    • 2010-11-18
    • JP2009111301
    • 2009-04-30
    • Ohara Inc株式会社オハラ
    • TSUCHIBUCHI NANAOGINO MICHIKO
    • C03C3/16C03C3/062C03C3/064C03C3/066C03C3/068C03C3/17C03C3/19C03C3/21G02B1/00
    • PROBLEM TO BE SOLVED: To provide optical glass which has a low Abbe number (ν
      d ) even though the refractive index (n
      d ) thereof is within a desired range, and which is highly transparent to visible light, and in which devitrification and clouding hardly occurs upon production and working of the glass, and from which a preform material and an optical element are easily produced by polishing, and to provide an optical element.
      SOLUTION: The optical glass contains, in mass% relative to the total mass of the glass in terms of oxides, 5.0 to 40.0% of a P
      2 O
      5 component and 10.0 to 60.0% of an Nb
      2 0
      5 component. In the optical glass, the wavelength (λ
      70 ) at which spectral transmittance shows 70% is ≤500 nm, and the optical glass has a liquid phase temperature of 500 to 1,200°C. Further, the optical element is composed of the optical glass as a matrix.
      COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:为了提供具有低阿贝数(ν d )的光学玻璃,即使其折射率(n d )在期望的 并且对可见光高度透明,并且在玻璃的制造和加工时几乎不发生失透和混浊,并且通过抛光容易地制造预成型体材料和光学元件,并提供光学元件。 解决方案:光学玻璃以相对于玻璃的总质量的以氧化物计的质量%含有5.0〜40.0%的P 2 5 组分和10.0至60.0%的Nb 2 0 5 组分。 在光学玻璃中,光谱透射率为70%的波长(λ 70 )为500nm,光学玻璃的液相温度为500〜1200℃。 此外,光学元件由作为基体的光学玻璃构成。 版权所有(C)2011,JPO&INPIT
    • 5. 发明专利
    • Optical glass
    • 光学玻璃
    • JP2007269584A
    • 2007-10-18
    • JP2006098088
    • 2006-03-31
    • Ohara Inc株式会社オハラ
    • ISHIOKA JUNKOOGINO MICHIKOONOZAWA MASAHIRO
    • C03C3/068C03B11/00G02B1/00
    • C03C3/068
    • PROBLEM TO BE SOLVED: To provide optical glass with a high refractive index and low dispersion having ≥1.75 refractive index (nd) and ≥35 Abbe number (νd), and hardly suffering from influence of imaging characteristic due to temperature variation of use environment.
      SOLUTION: The optical glass realizing product α×β of an average linear expansion coefficient α for -30°C to +70°C and an opto-elastic constant β at 546.1 nm wavelength of ≤130×10
      -12 °C×nm×cm
      -1 ×Pa
      -1 is obtained by containing SiO
      2 , B
      2 O
      3 and La
      2 O
      3 as essential components and adjusting the ratio between the structural components.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:为了提供具有≥1.75的折射率(nd)和≥35阿贝数(νd)的高折射率和低色散的光学玻璃,并且几乎不受由于温度变化引起的成像特性的影响 使用环境。

      解决方案:实现-30℃至+ 70℃平均线性膨胀系数α的产品α×β的光学玻璃和546.1nm波长的光弹性常数β≤130×10 - 12 ℃×nm×cm -1 ×Pa -1 通过含有SiO 2 ,B 2 作为必需组分,并调节结构组分之间的比例。 版权所有(C)2008,JPO&INPIT

    • 6. 发明专利
    • Optical glass
    • 光学玻璃
    • JP2003048746A
    • 2003-02-21
    • JP2002140080
    • 2002-05-15
    • Ohara Inc株式会社オハラ
    • OGINO MICHIKOMORI KATSUOONOZAWA MASAHIROISHIOKA JUNKO
    • G02B5/30C03C3/072C03C3/074C03C4/00G02B1/00
    • PROBLEM TO BE SOLVED: To provide an optical glass having a high refractive index suitable to be used for an optical element of a lens, prism or the like or for a substrate, in particular, suitable to be used for an optical element in a polarizing optical system or for a polarization controlling element of a PBS(polarizing beam splitter), SLM(spatial light modulator) or the like. SOLUTION: The optical glass contains SiO2 , PbO and B2 O3 and further contains >=0.1 mass% TeO2 and >=0.4 mass% Li2 O. Preferably, when the glass is 10±0.1 mm thick, the glass has 80% transmittance for light at radiation illuminance for 10 minutes.
    • 要解决的问题:提供一种适合用于透镜,棱镜等的光学元件或基板的具有高折射率的光学玻璃,特别适合用于偏光的光学元件 光学系统或PBS(偏振分束器)的偏振控制元件,SLM(空间光调制器)等。 解决方案:光学玻璃含有SiO 2,PbO和B 2 O 3,还含有> = 0.1质量%的TeO 2和> = 0.4质量%的Li 2 O.当玻璃的厚度为10±0.1mm时,玻璃的透光率为80% 在<= 420nm的波长处,并且通过在2.2W·cm -2辐射照度的UV区域和/或可见光区域中的射线照射10分钟,玻璃的透射率降低= 3.0%。
    • 7. 发明专利
    • Optical glass, preform and optical element
    • 光学玻璃,预制和光学元件
    • JP2013063888A
    • 2013-04-11
    • JP2011249168
    • 2011-11-14
    • Ohara Inc株式会社オハラ
    • OGINO MICHIKO
    • C03C3/068C03C3/15C03C3/155C03C3/23G02B1/00
    • PROBLEM TO BE SOLVED: To provide optical glass having a refractive index (n) and an Abbe number (ν) within expected range, applicable preferably to correcting chromatic aberration, and having reduced material cost, and to provide a preform and an optical element using the same.SOLUTION: This optical glass includes a BOcomponent and an F component, and the total mass of LnOcomponents (in the formula, Ln represents one kind or more selected from a group comprising La, Gd, Y, Tb and Lu) is
    • 要解决的问题:提供折射率(n d )和阿贝数(ν d )的光学玻璃 >)在预期范围内,优选地适用于校正色像差并且具有降低的材料成本,并且提供使用其的预成型件和光学元件。

      解决方案:该光学玻璃包括B 2 O 3 分量和F分量,以及Ln的总质量 组分(在该式中,Ln表示从包含La,Gd,Y,Y的组中选出的一种或多种) Tb和Lu)以质量%计<50.0%,相对于组合物的整个玻璃质量为氧化物。 预成型件和光学元件包括光学玻璃。 版权所有(C)2013,JPO&INPIT

    • 9. 发明专利
    • Optical glass, optical element, and preform for precision press molding
    • 光学玻璃,光学元件和精密压模成型
    • JP2010260745A
    • 2010-11-18
    • JP2009111386
    • 2009-04-30
    • Ohara Inc株式会社オハラ
    • TSUCHIBUCHI NANAOGINO MICHIKO
    • C03C3/16C03C3/064C03C3/066C03C3/068C03C3/17C03C3/19C03C3/21C03C3/253G02B1/00
    • PROBLEM TO BE SOLVED: To provide optical glass which has a low Abbe number (ν
      d ) even though the refractive index (n
      d ) thereof is within a desired range, is highly transparent to visible light, and is easily softened at a low temperature, and to provide an optical element and a preform for precision press molding.
      SOLUTION: The optical glass contains, in mass% relative to the total mass of the glass in terms of oxides, 5.0 to 40.0% of a P
      2 0
      5 component and 10.0 to 60.0% of an Nb
      2 O
      5 component, contains at least any one selected from an Li
      2 O component, an Na
      2 O component and a K
      2 O component, and has a glass transition point (Tg) of ≤700°C. The optical element and preform for precision press molding are composed of the optical glass as a matrix.
      COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:为了提供具有低阿贝数(ν d )的光学玻璃,即使其折射率(n d )在期望的 范围对可见光高度透明,并且在低温下容易软化,并且提供用于精密冲压成型的光学元件和预成型件。 光学玻璃以氧化物计相对于玻璃的总质量的质量%含有5.0〜40.0%的P 2 5 成分和10.0〜60.0%的Nb 2 SB 3 O组成中的至少一种,含有选自Li SB 2 O 3成分,Na (SB)2 O组分和K 2 O组分,玻璃化转变点(Tg)≤700℃。 用于精密加压成型的光学元件和预成型件由作为基体的光学玻璃构成。 版权所有(C)2011,JPO&INPIT