    • 1. 发明专利
    • Hot caliber rolling method
    • 热校准滚压方法
    • JP2012000634A
    • 2012-01-05
    • JP2010137199
    • 2010-06-16
    • Kobe Steel Ltd株式会社神戸製鋼所
    • MUROYA YUKIKUSHIDA HITOSHISUGYO SHOJISHIRANO GOMATSUSHITA KEISUKE
    • B21B1/16B21B27/10
    • PROBLEM TO BE SOLVED: To reduce surface defects due to surface roughing of a rolling roller while securing passability of the rolling stock even when supply of lubrication oil starts before the tip of the rolling stock is engaged with the rolling roller; and to improve the yield.SOLUTION: In a hot caliber rolling method, the rolling stock 2 is hot-rolled by the rolling roller 9 including a caliber 11 on the outer periphery. The lubrication oil is supplied on an entrance side of the rolling roller 9 for rolling. A supply region E where the lubrication oil 15 is supplied toward the caliber 11 is a region outside a position apart from the center of the caliber by 0.4×(d/2) in the longitudinal direction of a body of the rolling roller 9, where d is a width of the rolling stock 2 on the entrance side.
    • 要解决的问题:为了减少轧制辊的表面粗糙化导致的表面缺陷,同时确保在轧制机械的前端与轧辊接合之前开始润滑油的供给,同时确保轧制材料的通过性; 并提高产量。 解决方案:在热口径轧制方法中,通过包括外径上的口径11的轧辊9对轧制车辆2进行热轧。 在滚动辊9的入口侧供给润滑油进行轧制。 将润滑油15向口径11供给的供给区域E是在滚动辊9的主体的长度方向上离开口径中心的位置之外的区域为0.4×(d / 2)的区域, d是入口侧的车辆2的宽度。 版权所有(C)2012,JPO&INPIT
    • 2. 发明专利
    • Method and apparatus for hot-caliber-rolling bar steel
    • 热轧板轧制钢的方法和装置
    • JP2010201487A
    • 2010-09-16
    • JP2009052150
    • 2009-03-05
    • Kobe Steel Ltd株式会社神戸製鋼所
    • MUROYA YUKIKUSHIDA HITOSHISAKAI HIDENORIDOBASHI TOMOYASHIRANO GO
    • B21B1/16B21B1/04B21B3/00B21B45/02B21C51/00
    • PROBLEM TO BE SOLVED: To prevent the occurrence of surface flaws in a method for hot-caliber-rolling bar steel. SOLUTION: This method for hot-caliber-rolling the bar steel is a method for hot-rolling by the calibers by which a rolled stock 2 is hot-rolled by rolling with square-caliber rolling rolls 9 after rolling with diamond-caliber rolling rolls 9 and a lubricant 15 is supplied to the rolled stock 2 on the upstream side of the inlet side of the square-caliber rolling rolls 9. Furthermore, preferably, it is better to measure the angle θ of twist of the rolled stock 2 on the outlet side of the diamond-caliber rolling rolls 9, to adjust the feed rate of the lubricant 15 on the basis of the measured angle θ of twist and to feed the lubricant 15 when the angle θ of twist is ≥ 3°. COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:为了防止在热轧棒钢的方法中发生表面缺陷。 解决方案:这种用于热轧棒状钢的方法是通过使用金刚石轧制的轧辊坯料2通过轧制方槽轧制辊9进行热轧后的辊径进行热轧的方法, 将口径滚轧辊9和润滑剂15供给到方筒轧制辊9的入口侧的上游侧的轧制坯料2.此外,优选地,最好测量轧制坯料的捻度的角度θ 2,根据测得的扭转角度θ来调整润滑剂15的进给速度,并且当扭转角度θ为3°时供给润滑剂15。 版权所有(C)2010,JPO&INPIT
    • 3. 发明专利
    • Method of manufacturing bar steel and wire rod
    • 制造钢铁和钢丝绳的方法
    • JP2009241133A
    • 2009-10-22
    • JP2008092037
    • 2008-03-31
    • Kobe Steel Ltd株式会社神戸製鋼所
    • KUSHIDA HITOSHIMIYAZAKI SHOJITAHIRA TOMOHIDE
    • B21B45/02B21B1/16
    • PROBLEM TO BE SOLVED: To provide a line for rolling/manufacturing a bar steel and wire rod and a method of manufacturing the bar steel and wire rod by which the desired product of the bar steel and wire rod is obtained. SOLUTION: In a method of manufacturing the bar steel and wire rod by which the bar steel and wire rod 2 having the final wire diameter of 5.0-21.0 mm in the final wire diameter is rolled under a rolling condition that the rolling speed is 15-110 m/s, the bar steel and wire rod 2 is manufactured so that the difference ΔT1 between the surface temperature after winding of the bar steel and wire rod 2 and the minimum value of the bar steel and wire rod 2 during cooling is ≤150°C. When controlling the surface temperature of the bar steel and wire rod 2, by installing cooling means 9a, 9b, 9c for water-cooling the bar steel and wire rod 2 between the final rolling mill 11 for performing the final rolling of the bar steel and wire rod 2 and a winding reel 8 for winding the bar steel and wire rod 2 which is finally rolled, the flow rate distribution in the cooling means is adjusted. COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:提供一种用于轧制/制造棒钢和线材的生产线,以及制造棒钢和线材的方法,通过该方法获得棒钢和线材的所需产品。 解决方案:在制造棒钢和线材的方法中,使最终线直径的最终丝直径为5.0-21.0mm的钢丝和线材2在轧制速度 为15-110m / s,制造棒钢和线材2,使得钢筋和线材2卷绕后的表面温度与制冷时钢筋和线材2的最小值之差ΔT1 ≤150°C。 在控制钢筋和线材2的表面温度时,通过安装冷却装置9a,9b,9c,用于将棒钢和线材2水平冷却到终轧机11之间,以进行钢坯的最终轧制和 线材2和用于卷绕最终轧制的钢筋和线材2的卷取卷轴8,调节冷却装置中的流量分布。 版权所有(C)2010,JPO&INPIT
    • 4. 发明专利
    • Method for hot rolling wire rod and steel bar
    • JP2004001041A
    • 2004-01-08
    • JP2002159576
    • 2002-05-31
    • Kobe Steel Ltd株式会社神戸製鋼所
    • KUSHIDA HITOSHIOZAKI KATSUHIKOTOYAMA MASAOKOIZUMI FUJIO
    • B21B1/16B21B45/04B21B45/08
    • PROBLEM TO BE SOLVED: To provide a method for reducing surface flaws which makes the surface flaws generated by a rolling mill on the upstream side such as a roughing mill row to be easily eliminated by pressure fitting in the following rolling processes and hardly residual on the surface of products in the hot caliber rolling of wire rods and steel bars.
      SOLUTION: A scale at a place where the surface flaws in a wrinkle shape are usually generated in the vicinity on both sides at a corner part in which a rolled material is reduced is eliminated by jetting out high pressure water from a nozzle on the exit side of at least one caliber of a rhombic caliber or an angular caliber in the method for hot rolling the wire rods and the steel bars in which the rolled material is finished to be at required dimensions by gradually reducing a cross-sectional area with a caliber schedule including the rhombic caliber and the angular caliber from a raw material billet. By this constitution, the surface flaws are made shallow and uneven with wider flaw width. The scale is prevented from intruding inside the surface flaws. As a result, the surface flaws are easily eliminated by the deformation with the following calibers and the depth of product flaws is surely reduced.
      COPYRIGHT: (C)2004,JPO
    • 5. 发明专利
    • Method for manufacturing precision rolled stock
    • 制造精密滚筒的方法
    • JP2003053406A
    • 2003-02-26
    • JP2001243817
    • 2001-08-10
    • Kobe Steel Ltd株式会社神戸製鋼所
    • KUSHIDA HITOSHIHATTORI SHIGEOSUGYO SHOJISHIMONO SHIGEJIUTSUNO HIDEOSUGANO NAOKI
    • B21B37/16B21B37/00
    • PROBLEM TO BE SOLVED: To roll a wire less in dimensional variation in the radial direction over the entire length and is excellent in dimensional accuracy by a rolling line provided with a finishing mill and a final finishing mill. SOLUTION: When rolling the wire by the rolling line, by using the relationship among the dimensional difference ΔD in the radial direction over the entire length from the tip part to the rear end part of the wire after the final rolling, the roll gap d between the rolls in the 1st stage of the final finishing mill, the revolving speed ratio Nr (N1/N2) of the revolving speed N1 of the final finishing mill to the revolving speed N2 of the finishing mill and the speed ratio Vr of the speed of the rear end part of the wire after the rear end part of the wire is passed through the finishing mill to the speed of the intermediate part of the wire when the wire is rolled with the finishing mill and the final finishing mill and the relationship between the speed ratio Vr and the dimensional difference ΔD, the roll gap d and the revolving speed ratio Nr are adjusted so that the speed ratio Vr is constant.
    • 要解决的问题:在整个长度上滚动径向尺寸变化较小的线材,并且通过设有精轧机和最终精轧机的轧制线具有优异的尺寸精度。 解决方案:通过轧制线轧制钢丝时,通过使用最终轧制后的钢丝的前端部分与后端部分之间的整个长度上的径向尺寸差ΔD之间的关系,轧辊间隙d在 最终精轧机的第一阶段的轧辊,最终精轧机的转速N1与精轧机的转速N2的转速比Nr(N1 / N2)和速度的速度Vr 当电线用精轧机和最终精轧机轧制后,钢丝的后端部分之后的钢丝的后端部分通过精轧机进入钢丝的中间部分的速度, 速度比Vr和尺寸差ΔD,辊隙d和转速比Nr被调节,使得速度比Vr恒定。
    • 7. 发明专利
    • Control method for cooling bar steel and wire rod
    • 冷却钢筋和钢丝绳的控制方法
    • JP2009050893A
    • 2009-03-12
    • JP2007220004
    • 2007-08-27
    • Kobe Steel Ltd株式会社神戸製鋼所
    • MIYAZAKI SHOJITAHIRA TOMOHIDEKUSHIDA HITOSHI
    • B21B45/02B21C51/00
    • PROBLEM TO BE SOLVED: To provide a control method for cooling a bar steel and a wire rod, capable of accurately estimating the internal temperature of the bar steel and the wire rod and obtaining a desired metal texture based on the estimated internal temperature. SOLUTION: The control method for cooling the bar steel and the wire rod 6 is executed as follows: the distance between rolling mills 3, 4 and cooling means 8, 10 arranged in the upstream side of the rolling mills 3, 4 is previously set to be long enough to enable sufficient advance of recuperation of the bar steel and the wire rod 6; in rolling, a deformation resistance K of the bar steel and the wire rod 6 in the rolling mills 3, 4 is determined, and an internal temperature T of the bar steel and the wire rod 6 is estimated from the deformation resistance K; and the cooling performances of cooling means 8, 10, 11 are controlled based on the estimated internal temperature T. COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:提供一种用于冷却棒钢和线材的控制方法,能够精确地估计钢筋和线材的内部温度,并根据估计的内部温度获得所需的金属质地 。 解决方案:用于冷却钢筋和线材6的控制方法如下执行:轧机3,4之间的距离和布置在轧机3,4的上游侧的冷却装置8,10是 预先设定为足够长以能够充分推进钢筋和线材6的回收; 在轧制中,确定轧钢机3,4中的钢筋和线材6的变形抗力K,并根据变形抗力K推定棒钢和线材6的内部温度T. 并根据估计的内部温度T控制冷却装置8,10,11的冷却性能。版权所有(C)2009,JPO&INPIT
    • 9. 发明专利
    • Method of rolling bar steel
    • 轧钢棒的方法
    • JP2007313527A
    • 2007-12-06
    • JP2006144379
    • 2006-05-24
    • Kobe Steel Ltd株式会社神戸製鋼所
    • KUSHIDA HITOSHIMIYAZAKI SHOJIISHIDA TAKESHI
    • B21B31/18B21B31/20
    • PROBLEM TO BE SOLVED: To provide a rolling method capable of suppressing the twist of a rolled stock and improving a dimensional accuracy in a rolling process by a sizing mill for bar steel such as a wire rod and a steel bar.
      SOLUTION: In the rolling process with a two-way roll type sizing mill having at least two stands, by deciding the positions of the axial centers of upper and lower roll calibers by determining the contact positions T1, T2 between the upper and lower roll calibers G1, G2 and the rolled stock 4 by respectively fitting the shapes of the upper and lower roll calibers G1, G2 of the final roll stand of the sizing mill to the cross-sectional shape 4a of the rolled stock 4 which is measured on the outlet side of this sizing mill, the deviation (δ1) in the axial direction of the upper and lower roll calibers is determined. In this way, by determining the deviation in the axial direction of the roll of the upper and lower roll calibers accurately and easily, the thrusts of the rolls of the final roll stand can be adjusted, the inclination and the twist on the outlet side of the caliber of the rolled stock can be suppressed and the improvement of the dimensional accuracy are made possible.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:提供一种能够抑制轧制坯料的扭曲并通过用于诸如线材和钢棒的棒钢的上浆机来提高轧制过程中的尺寸精度的轧制方法。 解决方案:在具有至少两个支架的双向辊式定型磨机的轧制过程中,通过确定上下辊筒的轴向中心的位置,通过确定上和下辊口径之间的接触位置T1,T2, 通过将定径轧机的最终辊架的上下辊口径G1,G2的形状分别配合到被测量的轧制坯料4的横截面形状4a,分别配置下辊口径G1,G2和轧制坯料4 在该精整机的出口侧,确定上下辊筒径轴向的偏差(δ1)。 以这种方式,通过精确而容易地确定上下辊口径辊的轴向偏差,可以调节最终辊架的辊的推力,出口侧的倾斜和扭转 可以抑制轧制坯料的口径,并且可以提高尺寸精度。 版权所有(C)2008,JPO&INPIT
    • 10. 发明专利
    • Method for hot-rolling bar material
    • 热轧棒材的方法
    • JP2007061908A
    • 2007-03-15
    • JP2006228217
    • 2006-08-24
    • Kobe Steel Ltd株式会社神戸製鋼所
    • KUSHIDA HITOSHIKAKIMOTO HIDEKIKIRIHARA KAZUHIKOSAKAI HIDENORI
    • B21B1/16B21B27/02
    • PROBLEM TO BE SOLVED: To provide a method of hot-rolling a bar material for manufacturing bar-material products which satisfies severe warranty of surface defect in the late years by suppressing the generation of fine surface defects caused by rolling deformation in a hot-rolling stage of the bar material such as a wire rod, bar steel and a square material.
      SOLUTION: Provided is the method of hot-rolling the bar material by which a billet of a base stock is made into a required size by successively reducing the cross-sectional area by respective rolling systems by calibers provided on the rolls of a plurality of arranged rolling mills so that the compressive strain is ≤0.5 in the peripheral direction of the rolled stock by the calibers of the respective rolling systems. In this way, the surface defect which becomes problems so that defects are caused by working in the succeeding working stage by the rolling deformation can not be generated and the products made of the bar material which is excellent in the surface quality which deals with the severe warranty of the surface defect in the late years can be provided.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:提供一种热轧用于制造棒材产品的棒材的方法,其通过抑制由于轧制变形引起的细小表面缺陷的产生而在后期得到严格的表面缺陷保修 杆材,棒材,方钢等棒材的热轧阶段。 解决方案:提供一种将棒料坯料热轧制成所需尺寸的方法,通过相应的轧制系统连续减小设置在辊筒上的口径的横截面积 多个布置的轧机,使得轧制坯料的圆周方向上的压缩应变通过各个轧制系统的机芯而≤0.5。 以这种方式,不能产生由于轧制变形而在后续工作阶段中工作而引起缺陷的问题的表面缺陷,由表面质量优异的棒材制成的产品 可以提供近年来表面缺陷的保修。 版权所有(C)2007,JPO&INPIT