    • Joining method of sintered hard material and metallic material
    • 烧结硬质材料和金属材料的接合方法
    • JPS61136605A
    • 1986-06-24
    • JP25978484
    • 1984-12-07
    • F S K:KkKeiichiro Shoji
    • SHOJI KEIICHIROITO KIMIYOSHI
    • B22F3/14B22F7/00B22F7/06B23P5/00B23P11/00B23P15/28B24B3/00B24D3/00C04B37/02
    • PURPOSE: To join securely a sintered hard material and metallic material at a low temp. by sandwiching a green compact composed of the specific compsn. consisting of Ti, etc. as well as Sn and Cu and heating the same in a vacuum to convert the green compact to a liquid phase then pressurizing the materials.
      CONSTITUTION: 3W30wt% powder of ≥1 kinds among Ti, Cr, Zr, Mn, Mo and W, 5W20% Sn powder and the balance Cu powder and additive metallic powder, etc. of ≥1 kinds among Ag, Zn, V, Nb, Ta and B to be added according to need are compaction-molded. Such green compact is sandwiched betweenthe sintered hard material such as diamond or cubic boron nitride and the metallic powder and is heated to about 700W750°C in about 10
      -2 W10
      -3 Torr vacuum by which the green compact is converted to the liquid phase. These materials are thereafter pressurized under about 10W100kg/cm
      2 and are cooled, by which the sintered hard material and metallic material are securely joined without cracking and performance deterioration.
      COPYRIGHT: (C)1986,JPO&Japio
    • 目的:在低温下牢固地连接烧结硬质材料和金属材料。 通过夹具由特定的compsn组成的绿色契约。 由Ti等以及Sn和Cu组成,并将其在真空中加热,以将生坯压坯转变成液相,然后对材料加压。 构成:在Ti,Cr,Zr,Mn,Mo和W中的3-30wt%粉末,Ag〜5〜20%的Sn粉末和余量的Cu粉末和添加剂金属粉末等 ,根据需要添加的Zn,V,Nb,Ta和B进行压实成型。 这种生坯被夹在诸如金刚石或立方氮化硼的烧结硬质材料和金属粉末之间,并在约10 -2 -10 -3乇真空中加热至约700-750℃,通过该真空将绿色 压块转化为液相。 然后将这些材料加压至约10-100kg / cm 2,并冷却,烧结的硬质材料和金属材料牢固地连接而不会发生龟裂和性能劣化。