会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 81. 发明专利
    • Resin-coated metallic material, and method of producing the same
    • 树脂涂层金属材料及其制造方法
    • JP2011139986A
    • 2011-07-21
    • JP2010001632
    • 2010-01-07
    • Furukawa-Sky Aluminum Corp古河スカイ株式会社
    • KIMURA KENICHIROKATO OSAMUMAEZONO TOSHIKI
    • B05D7/14B32B15/08
    • PROBLEM TO BE SOLVED: To provide a resin-coated metallic material for use in fabricating an aluminum electrolytic capacitor case, having excellent moldability and high thermal yellowing resistance.
      SOLUTION: The resin-coated metallic material including a metallic material 2 and a resin layer 3 covering the metallic material 2, with the resin layer 3 having a thickness of 2 to 22 μm and containing an antioxidant 4, is characterized in that the concentration of the antioxidant 4 present in a segment having a thickness of 0.2 to 4 μm disposed adjacent to the interface of the resin layer 3 and the metallic material 2 is from 0.01 to 0.25 wt.% with the thickness of the segment occupying 5 to 50% of the thickness of the whole resin layer 3, and the concentration of the antioxidant 4 present in the remaining segment of the resin layer 3 is from 0.4 to 7.5 wt.%. A method of producing the same is disclosed as well.
      COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:为了提供用于制造铝电解电容器壳体的树脂涂覆的金属材料,具有优异的成型性和高的抗黄变性。 解决方案:包含金属材料2和覆盖金属材料2的树脂层3,树脂层3的厚度为2〜22μm,含有抗氧化剂4的树脂被覆金属材料的特征在于, 存在于与树脂层3和金属材料2的界面相邻设置的厚度为0.2〜4μm的部分中的抗氧化剂4的浓度为0.01〜0.25重量%,片段的厚度为5〜 整个树脂层3的厚度的50%,树脂层3的剩余部分中存在的抗氧化剂4的浓度为0.4〜7.5重量%。 也公开了其制造方法。 版权所有(C)2011,JPO&INPIT
    • 85. 发明专利
    • Method for producing aluminum alloy sheet blank for cold press forming having coating/baking hardenability, cold press forming method using the blank, and formed part
    • 生产铝合金板坯的方法,用于具有涂层/烘烤不易性的冷压成型,使用空白的冷压成型方法和成形部件
    • JP2011111657A
    • 2011-06-09
    • JP2009269980
    • 2009-11-27
    • Furukawa-Sky Aluminum Corp古河スカイ株式会社
    • ICHITANI KOJIHIBINO AKIRAKITO KOBABA RIKIZO
    • C22F1/05B21D22/20C22C21/02C22C21/06C22F1/00C22F1/04
    • PROBLEM TO BE SOLVED: To achieve the coexistence of the securance of high formability and the improvement of coating/baking hardenability as an Al alloy sheet for cold press forming mainly used for an automotive body sheet.
      SOLUTION: Using a blank made of an Al-Mg-Si based alloy sheet and having coating/baking hardenability with which a proof stress value is increased by ≥50 MPa upon artificial aging at 170°C for 20 min after plastic deformation of 2% in a state where 10 days or more are passed through after solution treatment (concretely, a blank obtained by subjecting an Al-Mg-Si based alloy rolled sheet to solution treatment at ≥480°C, rapidly cooling the sheet to a temperature range of ≤100°C and performing preliminary aging treatment of holding the sheet to a temperature in the range of 50 to 120°C for ≥5 min), the prescribed region in the blank is decided as a partial heating region, and the region is subjected to partial heating treatment under the conditions in which a temperature rising rate upon the heating is ≥20°C/sec and a heating arrival temperature is 180 to 300°C, thus the region is restored and softened.
      COPYRIGHT: (C)2011,JPO&INPIT
    • 待解决的问题:为了实现主要用于汽车车身片材的用于冷压成型的Al合金板,可实现高成形性的保证性和改善涂层/烘烤淬透性的共存性。 解决方案:使用由Al-Mg-Si基合金板制成的坯料,并且具有涂层/烘烤淬透性,当塑性变形后,在170℃下人造时效20分钟时,耐应力值增加≥50MPa 在固溶处理后通过10天以上的状态为2%(具体而言,是将Al-Mg-Si系合金轧制板在≥480℃下进行固溶处理而得到的坯料,迅速冷却至 温度范围≤100℃,进行预热时效处理,将片材保持在50〜120℃的范围内≥5分钟的温度),将坯料中的规定区域判定为局部加热区域, 区域在加热时的升温速度≥20℃/秒,加热到达温度为180〜300℃的条件下进行部分加热处理,恢复软化。 版权所有(C)2011,JPO&INPIT
    • 87. 发明专利
    • Aluminum alloy sheet for can body having satisfactory bottom wrinkle property
    • 用于具有满意度底部皱纹属性的身体的铝合金板
    • JP2011080155A
    • 2011-04-21
    • JP2010260597
    • 2010-11-22
    • Furukawa-Sky Aluminum Corp古河スカイ株式会社
    • SUZUKI SATORUTAKAO YASUYUKI
    • C22C21/06C22F1/00C22F1/04
    • PROBLEM TO BE SOLVED: To provide an aluminum alloy sheet for a can body which is improved in bottom wrinkle properties without impairing characteristics such as ironing formability, flange formability and the can body strength.
      SOLUTION: The aluminum alloy sheet has a composition containing 0.8 to 1.5% Mg, 0.7 to 1.5% Mn, 0.05 to 0.25% Cu, 0.1 to 0.4% Si and 0.2 to 0.6% Fe, and further comprising 0.005 to 0.05% Ti, 0.0001 to 0.001% B and the balance Al with inevitable impurities, and in which the average of the r value in the final sheet stock is ≥0.75, and also, the in-plane anisotropy Δr of the r value lies in the range from -0.15 to +0.05, and elongation is ≥5%.
      COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:提供一种罐身的铝合金板,其能够改善底部褶皱性能,而不会削弱诸如熨烫成型性,凸缘成形性和罐体强度等特性。 解决方案:铝合金板具有含有0.8〜1.5%的Mg,0.7〜1.5%的Mn,0.05〜0.25%的Cu,0.1〜0.4%的Si和0.2〜0.6%的Fe,进一步含有0.005〜0.05% Ti,0.0001〜0.001%B,剩余部分Al含有不可避免的杂质,其中最终片材的r值的平均值为≥0.75,r值的面内各向异性Δr为 从-0.15到+0.05,伸长率为≥5%。 版权所有(C)2011,JPO&INPIT
    • 88. 发明专利
    • Aluminum alloy plate for lithographic printing plate and method for producing the same
    • 用于平版印刷板的铝合金板及其制造方法
    • JP2011058049A
    • 2011-03-24
    • JP2009208942
    • 2009-09-10
    • Fujifilm CorpFurukawa-Sky Aluminum Corp古河スカイ株式会社富士フイルム株式会社
    • OSUGA HIROTAKEKOYAMA KATSUMIMURAMATSU TOSHIKISAWADA HIROKAZUKUROKAWA MASAYAUESUGI AKIO
    • C22C21/00B41N1/08B41N3/00C22F1/00C22F1/04
    • PROBLEM TO BE SOLVED: To provide an Al alloy plate for a lithographic printing plate which has excellent stain resistance in an image part and uniformity in appearance after roughening treatment, and particularly, to provide an Al alloy plate which is particularly suitable for a desk developing type printing plate. SOLUTION: The Al alloy sheet has a composition comprising 0.05 to 0.20% Fe, 0.05 to 0.20% Si, 0.005 to 0.07% Cu and 0.005 to 0.05% Ti, and in which the Fe content/the Si content lies in the range of 0.5 to 2.5, and the balance substantially Al, wherein a ratio in diffraction strength between Al 3 Fe an Al lies in the range of 0.0001 to 0.005. In its production method, without performing homogenizing treatment or after the performance of homogenizing treatment at 350 to 480°C for 1 to 10 hr, hot rough rolling is performed at a rolling starting temperature of 350 to 480°C and at the final draft of 50 to 80%, successively, hot finish rolling is performed at the final draft of 50 to 80% and at the rolling finishing temperature of 300 to 350°C, and cold rolling is performed. Alternatively, the hot rolling finishing temperature is controlled to 200 to 300°C, and thereafter, annealing is performed before the finishing of the cold rolling. COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:提供一种用于平版印刷版的铝合金板,其在图像部分中具有优异的耐污性和粗糙化处理后的外观均匀性,特别是提供一种特别适用于 台式显影型印版。 解决方案:Al合金板具有包含0.05至0.20%的Fe,0.05至0.20%的Si,0.005至0.07%的Cu和0.005至0.05%的Ti的组成,并且其中Fe含量/ Si含量位于 范围为0.5〜2.5,余量基本为Al,其中Al 3 SB 3 Fe与Al之间的衍射强度比在0.0001〜0.005的范围内。 在其制造方法中,在不进行均化处理的情况下,或者在350〜480℃下均匀化处理1〜10小时后,在350〜480℃的轧制开始温度下进行热粗轧, 50〜80%的条件下,在最终通气量为50〜80%,轧制终轧温度为300〜350℃下进行热精轧,进行冷轧。 或者,将热轧终轧温度控制在200〜300℃,然后在冷轧精加工前进行退火。 版权所有(C)2011,JPO&INPIT
    • 89. 发明专利
    • Heat exchanger using comb-type radiation unit
    • 热交换器使用组合式辐射单元
    • JP2011054778A
    • 2011-03-17
    • JP2009202618
    • 2009-09-02
    • Furukawa-Sky Aluminum Corp古河スカイ株式会社
    • EDA YOSHIYAHOSOKAWA TOSHIYUKI
    • H01L23/467H01L23/473H05K7/20
    • PROBLEM TO BE SOLVED: To form a heat exchanger that demonstrates a superior heat dissipation effect by controlling the flow of a cooling fluid with a smaller number of parts in a heat exchanger wherein a radiation fin for heat transfer to a cooling fluid is provided on a base plate connected thermally with heat generation parts, and to reduce the cost.
      SOLUTION: In a radiation fin, a plurality of long plates are erected parallel to each other as a comb from a base side and gaps among the long plates are used for fluid paths for cooling, and the base side of a radiation unit is thermally connected with the surface of a base plate. A fluid guiding means is provided on the base plate to guide the flow of a cooling fluid entering from an inlet by the inplane parallel to the plate surfaces of the base plate, thereby guiding the cooling fluid to the comb-type radiation unit from the inlet. Thus, the heat exchanger is configured to guide the flow of the cooling fluid so that the cooling fluid almost uniformly passes through many gaps (fluid paths for cooling) of the long plate in the comb-type radiation unit and then goes to the outlet.
      COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:为了形成热交换器,其通过在热交换器中控制具有较少数量的部件的冷却流体的流动来显示出优异的散热效果,其中用于传递到冷却流体的散热片为 设置在与发热部件热连接的基板上,并降低成本。 解决方案:在辐射翅片中,多个长板作为梳子从基座侧彼此平行地竖立,并且长板之间的间隙用于用于冷却的流体路径,并且辐射单元的基部侧 与基板的表面热连接。 流体引导装置设置在基板上,以引导从入口进入的冷却流体的流动通过平行于基板的板表面的平面,从而将冷却流体从入口引导到梳状辐射单元 。 因此,热交换器被构造成引导冷却流体的流动,使得冷却流体几乎均匀地通过梳状辐射单元中的长板的许多间隙(用于冷却的流体路径),然后进入出口。 版权所有(C)2011,JPO&INPIT
    • 90. 发明专利
    • Age hardening aluminum alloy brazing sheet, method for producing the same, and heat exchanger using the same
    • 老化铝合金烧结片,其制造方法和使用其的热交换器
    • JP2011042823A
    • 2011-03-03
    • JP2009190829
    • 2009-08-20
    • Furukawa-Sky Aluminum Corp古河スカイ株式会社
    • ANDO MAKOTOSUZUKI YOSHIKAZUHIBINO AKIRA
    • C22C21/00B23K1/00B23K1/19B23K35/22B23K35/28B23K101/14B23K103/10C22F1/00C22F1/04C22F1/043C22F1/047C22F1/053C22F1/057F28F21/08
    • PROBLEM TO BE SOLVED: To provide an aluminum alloy brazing sheet using a 6XXX series alloy as a core material, in which diffusion of a brazing material upon brazing is suppressed so as to achieve satisfactory brazing, and which has excellent strength by performing a suitable aging treatment after the brazing, and to provide a method for producing the same.
      SOLUTION: The aluminum alloy brazing sheet is obtained by cladding one side or both sides of a core material with an Al-Si based brazing filler metal. The core material has a composition which comprises, by mass, 0.2 to 1.0% Si, 0.03 to 0.4% Fe, 0.1 to 0.5% Mg and 0.05 to 1.0% C, and in which an X value decided by the Si content Sic and the Cu content Cuc: X=6×Sic+2.5×Cuc satisfies the relation of 2.0≤X≤6.0, and further comprises one or more kinds selected from 0.05 to 0.3% Mn, 0.05 to 0.3% Zr and 0.05 to 0.3% Cr, and the balance Al with inevitable impurities. Its metallic structure after final cold rolling includes intermetallic compounds of 0.05 to 1 μm by 5 to 50 pieces per μm
      2 in the observation of the cross-sectional structure.
      COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:提供一种使用6XXX系列合金作为芯材的铝合金钎焊片,其中钎焊材料在钎焊时的扩散被抑制以获得令人满意的钎焊,并且通过执行优异的强度 在钎焊之后进行合适的时效处理,并提供其制造方法。 解决方案:通过用Al-Si基钎料包覆芯材的一侧或两侧来获得铝合金钎焊片。 芯材的组成为:质量分数为0.2〜1.0%的Si,0.03〜0.4%的Fe,0.1〜0.5%的Mg和0.05〜1.0%的C,由Si含量Sic和 Cu含量Cuc:X = 6×Sic + 2.5×Cuc满足2.0≤X≤6.0的关系,进一步包含选自0.05〜0.3%的Mn,0.05〜0.3%的Zr和0.05〜0.3%的Cr, 余量为Al与不可避免的杂质。 其最终冷轧后的金属结构在横截面结构的观察中包括0.05〜1μm微米×5〜50个/μm·SP 2的金属间化合物。 版权所有(C)2011,JPO&INPIT