    • 86. 发明专利
    • Electrolytic cell using ion exchange membrane
    • 使用离子交换膜的电解槽
    • JPS61124591A
    • 1986-06-12
    • JP24314984
    • 1984-11-20
    • Asahi Glass Co Ltd
    • MORIMOTO TAKESHIMATSUBARA TOSHIYA
    • C25B9/00C25B1/46C25B9/08
    • PURPOSE:To sustain a small cell voltage by disposing an anode and cathode stuck with non-conductive hydrophilic particles on the surfaces facing an ion exchange membrane so as to contact with the ion exchange membrane. CONSTITUTION:The anode or cathode stuck with the non-conductive hydrophilic particles having no electrode activity on the surface facing the ion exchange membrane is disposed to contact with the ion exchange membrane in an electrolytic cell for electrolyzing an aq. alkali choride soln. The hydrophilic particles are preferably stuck in the form of a porous layer having about
    • 目的:通过在面向离​​子交换膜的表面上设置粘附有非导电亲水性颗粒的阳极和阴极以与离子交换膜接触来维持小电池电压。 构成:与面向离子交换膜的表面不具有电极活性的非导电性亲水性粒子粘合的阳极或阴极配置成与电解池中的电解池中的离子交换膜接触。 碱氯化钠 亲水性颗粒优选以多孔层的形式粘附,其具有约10%厚度和约10-90%的孔隙率,对于其而言。 使用诸如IVA,IVB,VB,铁族金属,Cr或Mn组的氧化物,氢氧化物,氮化物或碳化物的材料。 小电池电压由这样的电解池维持。
    • 87. 发明专利
    • Manufacture of gas diffusing electrode
    • 气体扩散电极的制造
    • JPS59133386A
    • 1984-07-31
    • JP15459482
    • 1982-09-07
    • Asahi Glass Co Ltd
    • MORIMOTO TAKESHIMATSUBARA TOSHIYA
    • C25B11/03C25B9/00C25B9/06C25B9/08C25B11/00C25B11/12C25B13/00H01M4/88
    • Y02E60/50
    • PURPOSE:To manufacture a gas diffusing electrode having a dual structure, showing high electrode activity and impermeable to a liq. by sticking a layer of a mixture consisting of carbon powder having a deposited catalyst and a resin contg. fluorine to a microporous sheet contg. dispersed carbon powder. CONSTITUTION:Polytetrafluoroethylene (PTFE) powder is mixed with carbon powder, preferably carbon black powder of
    • 目的:制造具有双重结构的气体扩散电极,显示出高电极活性和不渗透的气体扩散电极。 通过粘附由具有沉积催化剂的碳粉末和树脂粘合剂组成的混合物层。 氟到微孔板 分散碳粉。 构成:将聚四氟乙烯(PTFE)粉末与碳粉末混合,优选炭黑粉末为≤1μm的粒度和液体。 润滑剂。 将混合物成型为片材,通过加热或其它方法从成型体除去润滑剂,形成微孔片材。 分散碳粉。 该片具有PTFE的细纤维结构。 碳颗粒。 在结构中,PTFE的许多细结PTFE的细纤维以三维状态结合在一起。 由具有沉积催化剂如铂族金属的碳粉末和树脂粘合剂组成的混合物层。 通过丝网印刷或其它方法将氟如四氟乙烯 - 六氟丙烯共聚物粘合到片材上以获得气体扩散电极。
    • 88. 发明专利
    • Manufacture of gas diffusing electrode
    • 气体扩散电极的制造
    • JPS5950188A
    • 1984-03-23
    • JP15954582
    • 1982-09-16
    • Asahi Glass Co Ltd
    • MORIMOTO TAKESHIMATSUBARA TOSHIYA
    • C25B11/03C25B11/04C25B11/12H01M4/86
    • Y02E60/50
    • PURPOSE: To obtain the titled electrode without causing the problem of a liq. leak in the electrode and deteriorating the formability which may be caused when much carbon is blended, by providing a two-layered structure consisting of layers contacting with gas and liq., respectively to a gas diffusing electrode contg. carbon powder dispersed in a porous body of fluororesin.
      CONSTITUTION: A thin film of a polymer contg. fluorine is superposed on a thin fiom contg. fluororesin and carbon having catalyst supported thereon, and they are stretched. Satisfactory joining is carried out between the two layers, and the resulting stretched sheet has a fine porous structure in which fine fibers are three-dimensionally oriented and crossed. Polytetrafluoroethylene is preferably used as said polymer contg. fluorine.
      COPYRIGHT: (C)1984,JPO&Japio
    • 目的:获得标题电极而不引起液晶显示器的问题。 通过提供由分别与气体和液体接触的层组成的两层结构分别提供给气体扩散电极接头,从而使电极中的漏电和恶化了可能在混合多量碳时引起的成形性。 碳粉分散在氟树脂的多孔体中。 构成:聚合物薄膜 氟重叠在薄膜上 含有催化剂的氟树脂和碳,并进行拉伸。 在两层之间进行良好的接合,所得到的拉伸片材具有微细的三维取向和交叉的微细结构。 聚四氟乙烯优选用作所述聚合物。 氟。
    • 89. 发明专利
    • Material for gas diffusion electrode
    • 气体扩散电极材料
    • JPS5943889A
    • 1984-03-12
    • JP15277082
    • 1982-09-03
    • Asahi Glass Co Ltd
    • MORIMOTO TAKESHIMATSUBARA TOSHIYAYOSHIDA NAOKI
    • C25B11/03C25B11/04C25B11/12H01M4/86
    • Y02E60/50
    • PURPOSE: To manufacture a material for gas diffusion electrode having excellent characteristics and good durability, by dispersing carbon depositing a catalyst and a fluorine-containing hydrophobic polymer to an electric insulating material having open-cell type fine pores and mixing them.
      CONSTITUTION: 7W90pts. carbon powder depositing a catalyst such as platinum, etc. and having ≤1μ particle diameter and 10W500m
      2 /g specific surface area, and 0.5W90pts.wt. hydrophobic fluoropolymer such as a copolymer of tetrafluoroethylene with hexafluoropropylene (FEP), etc. are added to an electric insulating material having open cell type fine pores such as polytetrafluoroethylene (PTFE), or furthermore, a 20W300pts.wt. liquid lubricant such as petroleum, solvent naphtha, etc., is added to 100pts.wt. the total amt. of PTFE, carbon, and polymer to bring the mixture into a paste state. The paste is fabricated into a sheet shape and stretched to one direction after the liquid lubricant is removed heating. A material for gas diffusion electrode having excellent characteristics in void, and air permeability, and good durability is obtd.
      COPYRIGHT: (C)1984,JPO&Japio
    • 目的:为了制造具有优异特性和良好耐久性的气体扩散电极材料,通过将碳沉积催化剂和含氟疏水性聚合物分散在具有开孔型细孔的电绝缘材料中并将其混合。 组成:7-90pts。 碳粉末沉积催化剂如铂等,并且具有<= 1mu粒径和10-500m 2 / g比表面积,和0.5-90pss.wt。 将疏水性含氟聚合物如四氟乙烯与六氟丙烯(FEP)的共聚物等添加到具有开孔型细孔的电绝缘材料如聚四氟乙烯(PTFE),或者还有20-300pts.wt。 液体润滑剂如石油,溶剂石脑油等加入到100pts.wt。 总计。 的PTFE,碳和聚合物,以使混合物成为糊状态。 在除去加热液体润滑剂后,将该糊料制成片状并拉伸至一个方向。 具有优异的空隙特性,透气性,耐久性良好的气体扩散电极用材料。