    • Powder far-infrared radiator and its manufacturing method
    • 粉末红外辐射器及其制造方法
    • JP2003062093A
    • 2003-03-04
    • JP2001252830
    • 2001-08-23
    • Koichi Imai孝一 今井
    • IMAI KOICHI
    • A63B71/08A23L1/304A61F7/02A61F7/08A61K8/06A61K8/19A61K8/25A61K9/08A61K9/10A61K9/70A61K35/02A61L2/08A61L2/23A61L15/58A61N5/06A61P17/00A61Q19/00B02C19/00A61K7/00B02C19/12
    • A61K8/25A43B1/0045A61K2800/81A61L2/23A61N2005/0659A61Q19/00
    • PROBLEM TO BE SOLVED: To provide an extended use of a powder far-infrared radiator which emits far-infrared rays at ordinary temperatures, enabling it to be used in various fields.
      SOLUTION: In trituration process P1, the quartz schist B having ordinary temperature far-infrared radioactivity is wet ground until it becomes fines-like using a wet grinding mill. Next, in the sieve process P2, only the particle of the shape of fines 1.6 micrometers or less is extracted using the vibrating-screen machine equipped with a 1.6-micrometer mesh. In the dehydration process P3, the fines of the quartz schist B which became cake-like after a certain level of dehydration is obtained and in the following dryness/heating process P4, the fines of the quartz schist B which became cake-like is dried for 50 to 70 hours with warm air of 60°C to 90°C as well as the heat-treatment of 300°C to 400°C is performed for 30 minutes to 40 minutes. In the last unfolding process P5, solidified fines is unfolded to obtain the powder far-infrared radiator A.
      COPYRIGHT: (C)2003,JPO
    • 要解决的问题:提供在普通温度下发射远红外线的粉末远红外线辐射体的扩展使用,使其能够用于各种领域。 解决方案:在研磨过程P1中,具有常温远红外放射性的石英片岩B被湿磨,直到使用湿磨机变细。 接下来,在筛过程P2中,仅使用配备有1.6微米网的振动筛机提取1.6微米或更小的微细形状的颗粒。 在脱水处理P3中,获得在一定水平的脱水后变成饼状的石英片岩B的细粉,并且在随后的干燥/加热过程P4中,将成为饼状的石英片岩B的细粉干燥 在60〜90℃的温暖​​空气中进行50〜70小时,300℃〜400℃的热处理30分钟〜40分钟。 在最后一个展开过程P5中,展开固化的细粒以获得粉末远红外辐射体A.