    • 22. 发明专利
    • Anhydrous gypsum containing fired material and solidification material
    • 含有发泡材料和固化材料的无水胶囊
    • JP2011051876A
    • 2011-03-17
    • JP2010022442
    • 2010-02-03
    • Taiheiyo Cement Corp太平洋セメント株式会社
    • MATSUYAMA YUSUKEHAYASHI HIROSHI
    • C04B11/05C04B7/04C04B7/345C04B22/08C04B22/14C04B28/02
    • Y02P40/148
    • PROBLEM TO BE SOLVED: To provide an anhydrous gypsum containing fired material in which the containing rate is high and the strength development is excellent when used for a solidification material, and to provide a solidification material containing the same.
      SOLUTION: The invention provides the following anhydrous gypsum containing fired materials and solidification materials. (1) The anhydrous gypsum containing fired material contains 40-70 mass% of anhydrous gypsum, wherein the hydraulic modulus is 1.0-3.5, the silica modulus is 0.1-0.8, and the iron modulus is 5-25. (2) The anhydrous gypsum containing fired material contains 15-40 mass% of hauynite. (3) The anhydrous gypsum containing fired material contains 5-30 mass% of belite. (4) The solidification materials contain the anhydrous gypsum containing fired materials described in any of (1)-(3) above.
      COPYRIGHT: (C)2011,JPO&INPIT
    • 待解决的问题:提供含有率高的无机石膏的烧结材料,并且当用于固化材料时,其强度显现性优异,并且提供含有该组合物的固化材料。 解决方案:本发明提供以下含有无机石膏的烧制材料和固化材料。 (1)含无机石膏的烧成物含有40-70质量%的无水石膏,其水硬性模量为1.0-3.5,二氧化硅模量为0.1-0.8,铁模量为5-25。 (2)含无机石膏的烧成物含有15-40质量%的无水石膏。 (3)含无机石膏的烧成物含有5-30质量%的贝氏体。 (4)凝固材料含有上述(1)〜(3)中任一项所述的含有无水石膏的烧成物。 版权所有(C)2011,JPO&INPIT
    • 25. 发明专利
    • Concrete setting object and concrete composition
    • 混凝土设定对象和混凝土组合物
    • JP2007261933A
    • 2007-10-11
    • JP2007050406
    • 2007-02-28
    • Taiheiyo Cement CorpUniv Nihon太平洋セメント株式会社学校法人日本大学
    • KAJIO SATOSHIFUJITA HITOSHITSURUTA MASAHIROHASHIMOTO MASAYUKIKUBOTA HIROYASUMAKI TAKATERUIWAKI ICHIRO
    • C04B28/02C04B7/345C04B14/48C04B16/06C04B22/06C04B22/08C04B22/14C04B24/06
    • Y02P40/148
    • PROBLEM TO BE SOLVED: To provide a concrete setting object which has high strength while being accompanied by rapid development of strength, can reduce the shrinkage distortion due to self-shrinkage, drying shrinkage, etc., and can prevent the occurrence of a crack etc., due to shrinkage distortion. SOLUTION: The concrete setting object is prepared by setting a formulated material including an expandable admixture including a clinker composition containing a hydraulic composition including 0.1 to 3.0 parts by mass lithium carbonate of 1,000 to 4,000 cm 2 /g specific surface area, based on 100 parts by mass, calcium sulfoaluminate composition including 3 to 60 mass% calcium sulfoaluminate and 1 to 40 mass% anhydrous gypsum, and a composition including one or two or more kinds selected from the group consisting of a 3CaO-SiO 2 -2CaO-SiO 2 -CaO-interstitial material-based composition, 3CaO-SiO 2 -CaO-interstitial material-based composition, 2CaO-SiO 2 -CaO-interstitial material-based composition, and CaO-interstitial material-based composition, and containing 50 to 92 mass% CaO of the total mass of these compositions, and gypsum, metallic fibers or organic fibers. COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:为了提供具有高强度同时伴随着强度快速发展的混凝土设定对象,可以减少由于自收缩,干燥收缩等引起的收缩变形,并且可以防止发生 裂纹等,由于收缩变形。 解决方案:通过设定包含可膨胀混合物的配制材料来制备混凝土设定对象,所述可膨胀混合物包括含有水硬性组合物的熟料组合物,所述水硬性组合物包含0.1至3.0质量份的1,000至4,000cm 2的SP / /比表面积,基于100质量份,包含3〜60质量%的磺基铝酸钙和1〜40质量%的无水石膏的磺酸铝钙组合物,以及选自由以下组成的组中的一种或两种以上的组合物: 3CaO-SiO 2 SBA-SiO 2 SiO 2 -SaO-interstitial材料基组合物,3CaO-SiO -CaO-间质材料基 组合物,2CaO-SiO -CaO-间隙材料基组合物和CaO-间隙材料基组合物,并且含有这些组合物总质量的50-92质量%的CaO,石膏, 金属纤维或有机纤维。 版权所有(C)2008,JPO&INPIT
    • 28. 发明专利
    • Woody cement board and method for producing the same
    • 木质水泥板及其制造方法
    • JP2006306671A
    • 2006-11-09
    • JP2005132598
    • 2005-04-28
    • Sumitomo Osaka Cement Co Ltd住友大阪セメント株式会社
    • AKIYAMA TATSUSHISHIRAI MAKOTOKAMEI SEIYA
    • C04B28/02C04B7/345C04B16/02C04B18/26
    • Y02P40/148Y02W30/97
    • PROBLEM TO BE SOLVED: To provide a woody cement board and a method for producing the same using a cement composition which has high adsorption ability of organic matter, does not inhibit the setting reaction of cement without adding a setting accelerator, is inexpensive and can be easily produced, has good flowability, and can assure development of strength. SOLUTION: The woody cement board uses a cement composition in which the clinker mineral composition contains C 3 S, C 2 S, and a gap phase and does not contain C 3 A and gypsum; particularly, the gap phase is a continuous solid solution which does not contain C 3 A and has an average composition in the range of C 4 AF to C 6 AF 2 ; and the clinker mineral has a Fe 2 O 3 content of 4.0 mass% or more and a molar ratio of Fe 2 O 3 /Al 2 O 3 of 1 or more. The woody cement board can be obtained by mixing the cement composition with woody fibers and water, shaping the mixture into a predetermined shape followed by curing and setting. COPYRIGHT: (C)2007,JPO&INPIT
    • 待解决的问题:为了提供木质水泥板及其制造方法,使用具有高有机物吸附能力的水泥组合物,不会抑制水泥的凝固反应而不添加凝固促进剂,价格便宜 并且可以容易地生产,具有良好的流动性,并且可以确保强度的发展。 解决方案:木质水泥板使用水泥组合物,其中熟料矿物组合物含有C 3 SB 3,S 2,S 2,S 3,以及间隙相,不含 C&lt; 3&gt; A和石膏; 特别地,间隙相是不含C 3 S 3 S的连续固溶体,其平均组成在C 4 AF至C <6> / SB> AF 2 ; 熟料矿物含有4.0质量%以上的Fe 2 3 ,Fe 2 O 3 / A1 2 3 为1以上。 木质水泥板可以通过将水泥组合物与木质纤维和水混合而获得,将混合物成形为预定形状,然后固化和固化。 版权所有(C)2007,JPO&INPIT
    • 29. 发明专利
    • Hydraulic cement composition, cement concrete composition, cement concrete hardened body and method of producing the same
    • 液压水泥组合物,水泥混凝土组合物,水泥混凝土硬化体及其生产方法
    • JP2006076856A
    • 2006-03-23
    • JP2004264797
    • 2004-09-13
    • Denki Kagaku Kogyo Kk電気化学工業株式会社
    • HIGUCHI TAKAYUKIMORIOKA MINORUYOSHINO RYOETSUISHIDA TSUMORU
    • C04B7/32C04B28/06
    • Y02P40/148
    • PROBLEM TO BE SOLVED: To provide a cement concrete hardened body or a cement concrete structure having excellent acid resistance, sulfate resistance and neutralization resistance by using a specific hydraulic cement composition or a cement concrete composition. SOLUTION: The hydraulic cement composition contains CaO and Al 2 O 3 -SiO 2 . The hydraulic cement composition contains 5-300 pts. of γ-2CaO-SiO 2 and 100 pts. of glass-based hydraulic compound containing 40-55 pts. of CaO, 30-40 pts. of Al 2 O 3 and 10-25 pts. of SiO 2 . The hardened body of the cement concrete composition is steam-cured or autoclave-cured, or steam cured or autoclave-cured in water and contains the hydraulic cement composition. The method of producing the same is provided. The cement concrete structure is obtained by lining the existing cement concrete surface with the hydraulic cement composition. COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:通过使用特定的水硬性水泥组合物或水泥混凝土组合物来提供具有优异的耐酸性,耐硫酸盐性和耐中和性的水泥混凝土硬化体或水泥混凝土结构体。

      解决方案:水硬性水泥组合物含有CaO和Al 2 3 -SiO 2 。 水硬性水泥组合物含有5-300磅。 的γ-2CaO-SiO 2 和100个。 含40-55分的玻璃基液压复合材料。 的CaO,30-40磅。 的Al 2 SB 3 O 3和10-25 pts。 的SiO 2 。 将水泥混凝土组合物的硬化体蒸汽固化或高压釜固化,或在水中蒸汽固化或高压釜固化,并含有水硬性水泥组合物。 提供其制造方法。 水泥混凝土结构采用水泥水泥组合物对现有水泥混凝土表面进行衬砌。 版权所有(C)2006,JPO&NCIPI