    • 22. 发明专利
    • Mixed powder for powder metallurgy, and iron powder sintered compact
    • 粉末冶金粉末冶金粉末冶金粉末冶金粉末冶金粉末冶金粉末冶金粉末冶金粉末冶金
    • JP2009209410A
    • 2009-09-17
    • JP2008053725
    • 2008-03-04
    • Kobe Steel Ltd株式会社神戸製鋼所
    • TSUCHIDA TAKEHIROKUDO TAKAHIROSATO MASAAKIFURUTA TOMOYUKI
    • B22F1/00C22C33/02C22C38/00
    • PROBLEM TO BE SOLVED: To provide mixed powder for powder metallurgy which solves the conventional problems, and can obtain an iron powder sintered compact having excellent strength and toughness, and to provide the iron powder sintered compact. SOLUTION: Disclosed is mixed powder for powder metallurgy obtained by mixing mother powder composed of prealloy type steel powder and powder for alloying. The mother powder is composed of iron powder comprising W and/or V by 0.05 to 1.0 mass% in total, and the balance inevitable impurities, and, in the powder for alloying, regarding the blending mass% in the total mixed powder together with the mother powder, graphite is 0.4 to 1.5 mass%, and Cu powder and/or Ni powder is 1.0 to 8.0 mass% in total. COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:提供解决常规问题的粉末冶金用混合粉末,并且可以获得具有优异的强度和韧性的铁粉末烧结体,并提供铁粉末烧结体。 解决方案:公开了通过混合由预合金型钢粉末组成的母体粉末和用于合金化的粉末而获得的粉末冶金用混合粉末。 母粉由W和/或V的总和0.05〜1.0质量%的铁粉构成,余量为不可避免的杂质,在合金化用粉末中,关于总混合粉末的配合质量% 母粉,石墨为0.4〜1.5质量%,Cu粉末和/或Ni粉末为1.0〜8.0质量%。 版权所有(C)2009,JPO&INPIT
    • 23. 发明专利
    • Method for compacting large-sized high density green compact
    • 用于压缩大尺寸高密度绿色压缩的方法
    • JP2009013458A
    • 2009-01-22
    • JP2007175471
    • 2007-07-03
    • Kobe Steel Ltd株式会社神戸製鋼所
    • MITANI HIROYUKIHOJO TAKAFUMISATO MASAAKI
    • B22F3/035B30B11/00H01F41/02
    • PROBLEM TO BE SOLVED: To provide a method for compacting a large-sized high density green compact where, upon the compacting of a large-sized high density green compact by a die lubrication compacting process, a sound green compact free from galling and dents caused by the entanglement of a lubricant can be obtained.
      SOLUTION: Regarding the method for compacting a large-sized high density green compact having a density of ≥7.60 g/cm
      3 by a die lubrication compacting process or a warm die lubrication compacting process in a state where a die having a cavity with a depth of ≥9 cm and a volume of ≥700 cm
      3 is used, and raw material powder is packed into the cavity, the upper half part of the inner wall face of the die is coated with a lubricant in an amount satisfying the range of 3 to 6 mg/cm
      2 per unit area, and further, the lower half part is coated with a lubricant in an amount satisfying the range of 0.05 to 0.1 mg/cm
      2 per unit area.
      COPYRIGHT: (C)2009,JPO&INPIT
    • 解决问题的方案:提供一种压缩大型高密度生坯的方法,其中,通过模具润滑压实方法在大型高密度生坯压实时,不产生磨损的声音绿色压实 并且可以获得由润滑剂的缠结引起的凹痕。 解决方案:关于通过模具润滑压实工艺或温度模具润滑压实方法压实密度为≥7.60g/ cm 3以上的大型高密度生坯的方法 使用具有深度≥9cm的空腔和≥700cm3的体积的模具,将原料粉末包装到空腔中,内壁的上半部分 以每单位面积3〜6mg / cm 2·SP 2的范围内的润滑剂涂覆模具面,另外,下半部分涂布润滑剂,其量满足 每单位面积的0.05〜0.1mg / cm 2的范围。 版权所有(C)2009,JPO&INPIT