    • 13. 发明专利
    • Lightweight japanese lacquer resin molding with heat insulation property imparted thereto
    • 轻质日本LACQUER树脂模具与热绝缘性能
    • JP2011074329A
    • 2011-04-14
    • JP2009230011
    • 2009-10-01
    • Tomohiro Maruyama智裕 丸山
    • MARUYAMA TOMOHIRO
    • C08L93/00C08J9/35C08K7/28C09D7/12C09D193/00
    • PROBLEM TO BE SOLVED: To provide a lightweight Japanese lacquer resin composition which has preferable heat insulation property and can be provided for substrate process of Japanese lacquer coating in place of substrate material of the traditional Japanese lacquer coating, and to provide a Japanese lacquer resin molding serving as a base material by using a Japanese lacquer resin itself with respect to commodity such as flatware made by subjecting a resin base material prepared by mixing a synthetic resin, wooden powder, etc. to the Japanese lacquer coating.
      SOLUTION: The substrate material of the Japanese lacquer coating which has light weight and has preferable heat insulation property is made by using the Japanese lacquer resin composition prepared by compounding hollow glass beads having an average particle size of 10 to 80 μm to a Japanese lacquer resin. Further, a foamed resin molding using Japanese lacquer can be provided by foaming and curing the Japanese lacquer resin composition at a temperature of 80 to 200°C.
      COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:为了提供一种具有优选的隔热性能的轻质日本漆树脂组合物,可以提供日本漆涂料的基底处理代替日本传统漆器的基材,并提供日本 通过使用日本漆树脂本身对于通过将通过混合合成树脂,木粉等制备的树脂基材进行日本漆涂料制成的扁平餐具的商品来作为基材的漆树脂模制品。 解决方案:通过使用通过将平均粒径为10至80μm的中空玻璃珠与通过将平均粒径为10至80μm的中空玻璃珠复合而制备的日本漆树脂组合物来制造具有轻质量并且具有优选的隔热性的日本漆层的基材 日本漆树脂。 此外,使用日本漆的发泡树脂成型体可以通过在80〜200℃的温度下发泡和固化日本漆树脂组合物来提供。 版权所有(C)2011,JPO&INPIT
    • 14. 发明专利
    • Coating composition for tableware or chopsticks, tableware, chopsticks and method of manufacturing the same
    • 用于餐具或筷子,餐具,筷子及其制造方法的涂料组合物
    • JP2011016979A
    • 2011-01-27
    • JP2010118936
    • 2010-05-25
    • Hyozaemon:Kk株式会社兵左衛門
    • URATANI HYOGONAKAMURA TERUO
    • C09D193/00C09D5/00C09D181/00
    • PROBLEM TO BE SOLVED: To provide a coating material which is safe as a coating material for tableware and chopsticks and has substantially colorless gloss, to provide tableware and chopsticks having a coating layer excellent in water-resistance, durability, alkali resistance and also excellent in practicality, and to provide a method of manufacturing a coating composition using a mastic resin, and tableware or chopsticks using the coating composition in a simple manner at low cost.SOLUTION: There are provided a coating composition for tableware or chopsticks, at least having a natural resin, a vegetable oil, and an organic solvent. In particular, the natural resin is preferably a mastic resin. Preferably, the natural resin is esterified to the vegetable oil. In addition, it is preferable that the vegetable oil is a fatty acid triglyceride, and the organic solvent is any one of a pine oil, turpentine, and an orange oil.
    • 要解决的问题:为了提供作为餐具和筷子用涂料的安全性的涂料,具有基本无色的光泽,提供具有耐水性,耐久性,耐碱性优异的涂层的餐具和筷子, 并提供使用该乳胶树脂制造涂料组合物的方法,以及以简单的方式使用该涂料组合物的餐具或筷子,成本低廉。解决方案:提供一种用于餐具或筷子的涂料组合物,至少具有 天然树脂,植物油和有机溶剂。 特别地,天然树脂优选为乳香树脂。 优选地,将天然树脂酯化成植物油。 此外,优选植物油为脂肪酸甘油三酯,有机溶剂为松油,松节油和橙油中的任一种。
    • 15. 发明专利
    • Japanese lacquer and method for manufacturing japanese lacquer
    • 日本薰衣草和制造日本薰衣草的方法
    • JP2010222453A
    • 2010-10-07
    • JP2009070392
    • 2009-03-23
    • Ishikawa Prefecture石川県
    • ETO TOSHIROOYA YUKIYOKAJII NORITAKA
    • C09D193/00C09D7/12
    • PROBLEM TO BE SOLVED: To provide a japanese lacquer liquid to form a japanese lacquer coated film which has little deterioration by ultraviolet rays and little fading by hot water, a detergent or the like, namely has the excellent weatherability and cleaning resistance, and besides which has the same blackishness as a black Japanese lacquer.
      SOLUTION: This japanese lacquer liquid is manufactured by adding inorganic microparticles (zinc oxide, silica and titanium oxide) to a natural japanese lacquer liquid or a purified japanese lacquer using a crude japanese lacquer as a raw material, and by dispersing it homogeneously using a kneading apparatus such as a three-roll mill or a mixer and by inhibiting the elution of the rubbery matter to cause the deterioration of japanese lacquer coated film. The inorganic microparticles dispersed have a particle diameter of 20-100 nm, and have the loadings of 1-20 wt.%. The added inorganic microparticles includes preferably zinc oxide microparticles, particularly the zinc oxide microparticles with a silica-alumina coating or a polysiloxane coating.
      COPYRIGHT: (C)2011,JPO&INPIT
    • 待解决的问题:提供日本漆液以形成几乎没有紫外线劣化的日本漆涂膜,并且由热水,洗涤剂等几乎没有褪色,即具有优异的耐候性和耐清洁性, 除了与黑色日本漆相同的黑色。 解决方案:这种日本漆液是通过将日本纯天然漆作为原料,将天然日本漆液或日本纯净的日本漆添加到无机微粒(氧化锌,二氧化硅和氧化钛)中并通过均匀分散而制成的。 使用三辊研磨机,混合机等捏合装置,抑制橡胶状物质的溶出,使日本漆涂膜发生变质。 分散的无机微粒的粒径为20〜100nm,负载量为1-20重量%。 添加的无机微粒优选包括氧化锌微粒,特别是具有二氧化硅 - 氧化铝涂层或聚硅氧烷涂层的氧化锌微粒。 版权所有(C)2011,JPO&INPIT
    • 17. 发明专利
    • Repairing agent for japanese lacquer coated material
    • JAPANESE LACQUER涂层材料修理剂
    • JP2009051912A
    • 2009-03-12
    • JP2007218857
    • 2007-08-24
    • Sumitomo Forestry Co Ltd住友林業株式会社
    • KAKIYA TOMO
    • C09D193/00B05D7/24E04F15/12E04F19/00
    • PROBLEM TO BE SOLVED: To provide a repairing agent and a repairing method by which the damaged coating film of a japanese lacquer coated article is safely and simply repaired, and the repaired japanese lacquer coated article wherein a repaired part colored to be matched with a non-repaired part is inconspicuous.
      SOLUTION: The repairing agent for a japanese lacquer coated article comprises an astringent persimmon and a basic water-soluble compound or the aqueous solution. The repairing method of the japanese lacquer coated article is carried out by applying a mixture of the astringent persimmon and the basic water-soluble compound or the aqueous solution on a coating film damaged part of the japanese lacquer coated article. The repaired japanese lacquer coated article is obtained by repairing the coating film damaged part of the japanese lacquer coated article using the repairing agent for the japanese lacquer coated article.
      COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:提供修复剂和修复方法,通过该修复方法和日本漆涂层制品的损伤涂膜被安全且简单地修复,并且修复的日本漆涂层制品,其中修复的部分被着色为匹配的 没有修理的部分是不明显的。 解决方案:日本漆涂层制品的修复剂包括收敛柿子和碱性水溶性化合物或水溶液。 日本漆涂层制品的修复方法是通过将涩味柿子和碱性水溶性化合物或水溶液的混合物施加在日本漆涂层制品的涂膜损坏部分上进行的。 修理日本涂漆制品是通过使用日本漆涂层制品的修复剂修复日本漆涂层制品的涂膜损坏部分而获得的。 版权所有(C)2009,JPO&INPIT
    • 20. 发明专利
    • Aerosol lacquer
    • AEROSOL LACQUER
    • JP2006169307A
    • 2006-06-29
    • JP2004360813
    • 2004-12-14
    • Kyoto IchiYasushi OyabuSato Kiyomatsu Shoten:Kk京都市泰 大薮株式会社佐藤喜代松商店
    • SATO TAKAHIKOOYABU YASUSHI
    • C09D193/00B65D83/34B65D83/36C09D189/00
    • PROBLEM TO BE SOLVED: To solve a problem that lacquer coating has not been easily performed by ordinary people because it has various problems such as: one may get easily poisoned with lacquer; control of drying conditions is difficult; and various tools are required. SOLUTION: Lacquer has been filled in an aerosol container so that lacquer coating can be easily performed. Although filling of lacquer in an aerosol container has been considered difficult because lacquer is a W/O-type emulsion, the filling of lacquer in an aerosol container has become possible by appropriately selecting an injection agent and a diluent and by appropriately adjusting the ratio of the lacquer, the injection agent and the diluent. LPG, DME and the like are particularly suitable for the injection agent. Control of the gloss of the dried coating film is also possible by adjusting the mixing ratio of these components. COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:为了解决普通人不容易进行漆涂层的问题,因为它有各种问题,例如:可能容易被漆中毒; 干燥条件控制困难; 并需要各种工具。

      解决方案:漆已经填充在气溶胶容器中,使得漆涂层可以容易地进行。 虽然由于漆是W / O型乳液,但是在气溶胶容器中填充漆已经被认为是困难的,通过适当选择注射剂和稀释剂,通过适当地调节喷雾剂和稀释剂的比例,可以使气雾剂容器中的漆的填充成为可能, 漆,注射剂和稀释剂。 LPG,DME等特别适用于注射剂。 干燥涂膜的光泽度的控制也可以通过调节这些组分的混合比来实现。 版权所有(C)2006,JPO&NCIPI