    • 11. 发明专利
    • Thermoplastic elastomer
    • 热塑性弹性体
    • JP2013256639A
    • 2013-12-26
    • JP2013056106
    • 2013-03-19
    • Nof Corp日油株式会社
    • SATO KAZUHIROMOCHIDATE KAZUOMITASAKA TOMOHISA
    • C08L33/06C08K3/00C08K5/00C08L51/06C08L67/00
    • PROBLEM TO BE SOLVED: To provide a thermoplastic elastomer having good molding processability, flexibility, thermal conductivity and heat resistance.SOLUTION: A thermoplastic elastomer includes (A) 50-85 pts.mass of acrylic rubber, (B) 15-50 pts.mass of a thermoplastic polyester resin, (C) 20-900 pts.mass of heat conductive filler, (D) 1-20 pts.mass of a compatibilizer and (E) 0.01-1 pt.mass of a crosslinking agent. The (A) is obtained by copolymerizing 100 pts.mass of at least one of general formulae (1) or (2), and 0.1-10 pts.mass of an epoxy group-containing (meth)acrylic monomer, and has a glass transition temperature of -60 to -15°C. The (D) is a graft copolymer, in which the main chain is an ethylene-ethyl acrylate copolymer, an ethylene-methyl acrylate copolymer, or an ethylene-vinyl acetate copolymer, or a polyolefin containing a functional group (anyone among a carboxy group, hydroxy group and an epoxy group), and the side chain is a polymer including at least one kind among general formulae (1) or (2).
    • 要解决的问题:提供具有良好模塑加工性,柔韧性,导热性和耐热性的热塑性弹性体。解决方案:热塑性弹性体包括(A)50-85重量份丙烯酸橡胶,(B)15-50重量份。 热塑性聚酯树脂的质量,(C)20-900质量度的导热填料,(D)1-20质量份的增容剂和(E)0.01-1重量%的交联剂。 (A)通过将100质量份的通式(1)或(2)中的至少一种和0.1-10质朴的含环氧基的(甲基)丙烯酸单体共聚而得到,并具有玻璃 转变温度为-60〜-15℃。 (D)是主链是乙烯 - 丙烯酸乙酯共聚物,乙烯 - 丙烯酸甲酯共​​聚物或乙烯 - 乙酸乙烯酯共聚物或含有官能团的聚烯烃(羧基中的任一个)的接枝共聚物 ,羟基和环氧基),侧链是包括通式(1)或(2)中的至少一种的聚合物。
    • 12. 发明专利
    • 熱可塑性エラストマー
    • 热塑性弹性体
    • JP2014210874A
    • 2014-11-13
    • JP2013088421
    • 2013-04-19
    • 日油株式会社Nof Corp
    • MOCHIDATE KAZUOMITASAKA TOMOHISA
    • C08L33/04C08F220/10C08K5/00C08L67/00
    • C08K5/00C08L33/04C08L67/00
    • 【課題】機械的強度等のほか、シール性にも優れる熱可塑性エラストマーを提供する。【解決手段】(A)アクリルゴム100質量部と、(B)熱可塑性ポリエステル15〜70質量部とを含む混合物を、成分(A)100質量部に対して(C)架橋剤が0.1〜5質量部存在する条件下で、動的架橋させてなる熱可塑性エラストマーであって、(A)アクリルゴムは、(a−1)アクリル酸アルキルエステル及び/又はアクリル酸アルコキシアルキルエステル由来の構成単位100質量部と、(a−2)側鎖に架橋性基である塩素基を有する単官能単量体由来の構成単位0.5〜5質量部とを含み、多官能単量体を含まない。【選択図】なし
    • 要解决的问题:提供除了机械强度以外的密封性能优异的热塑性弹性体。解决方案:提供一种热塑性弹性体,其通过动态交联含有(A)100质量份丙烯酸橡胶和(B)15 至(C)0.1〜5质量份的交联剂的情况下,以100重量份的(A)成分为基准,将丙烯酸系橡胶(A)含有(C) a-1)来源于丙烯酸烷基酯和/或丙烯酸烷氧基烷基酯的结构单元的100磅/吋(a-2)来自具有氯基团的单官能单体的结构单元的0.5-5重量份 ,其是侧链上的可交联基团,并且不含多官能单体。
    • 13. 发明专利
    • 熱可塑性エラストマー
    • 热塑性弹性体
    • JP2014210873A
    • 2014-11-13
    • JP2013088419
    • 2013-04-19
    • 日油株式会社Nof Corp
    • MOCHIDATE KAZUOMITASAKA TOMOHISA
    • C08L33/14C08J3/24C08L67/00
    • C08J3/24C08L33/14C08L67/00
    • 【課題】機械的強度等のほか、シール性にも優れる熱可塑性エラストマーを提供する。【解決手段】(A)アクリルゴム100質量部と、(B)熱可塑性ポリエステル15〜70質量部とを含む混合物を、成分(A)100質量部に対して(C)架橋剤が0.1〜5質量部存在する条件下で、動的架橋させてなる熱可塑性エラストマーであって、(A)アクリルゴムは、(a−1)アクリル酸アルキルエステル及び/又はアクリル酸アルコキシアルキルエステル由来の構成単位100質量部と、(a−2)側鎖に架橋性基であるエポキシ基を有する単官能単量体由来の構成単位0.5〜5質量部とを含み、多官能単量体を含まない。【選択図】なし
    • 要解决的问题:提供除了机械强度以外的密封性能优异的热塑性弹性体。解决方案:提供一种热塑性弹性体,其通过动态交联含有(A)100质量份丙烯酸橡胶和(B)15 至(C)0.1〜5质量份的交联剂的情况下,以100重量份的(A)成分为基准,将丙烯酸系橡胶(A)含有(C) a-1)来源于丙烯酸烷基酯和/或丙烯酸烷氧基烷基酯的结构单元的100盎司,和(a-2)衍生自具有环氧基的单官能单体的结构单元的0.5至5重量份 ,其是侧链上的可交联基团,并且不含多官能单体。
    • 14. 发明专利
    • Resin composition for putty, and putty obtained by curing the same
    • 酚醛树脂组合物和通过固化获得的酯
    • JP2014019836A
    • 2014-02-03
    • JP2012162095
    • 2012-07-20
    • Nof Corp日油株式会社
    • NISHIMA KEISUKEUCHIDA ATSUSHITASAKA TOMOHISA
    • C09K3/10C08F283/01
    • PROBLEM TO BE SOLVED: To provide a resin composition for a putty, having appropriate hardness and satisfying aspects of dimensional accuracy, adhesion and abradability.SOLUTION: A resin composition for a putty contains (A) an unsaturated polyester resin, (B) an ethylenically unsaturated monomer, (C) a low constrictive agent and (D) a filler, and (C) the low constrictive agent is an A-B type block copolymer containing an A segment which is a polymer based on a monomer containing vinyl acetate and a B segment which is a polymer based on styrene, and a percentage of the A segment in the A-B type block copolymer is 30 to 50 mass% and a percentage of B segment is 70 to 50 mass%, and a number average molecular weight of the A-B type block copolymer is 10,000 to 100,000.
    • 要解决的问题:提供一种用于油灰的具有适当硬度和满足尺寸精度,粘合性和耐磨性方面的油灰的树脂组合物。解决方案:用于油灰的树脂组合物含有(A)不饱和聚酯树脂,(B)烯属 不饱和单体,(C)低收缩剂和(D)填料,(C)低收缩剂是AB型嵌段共聚物,其含有作为基于含有乙酸乙烯酯的单体和B部分的聚合物的A链段 其为基于苯乙烯的聚合物,AB型嵌段共聚物中的A链段的百分比为30〜50质量%,B链段的百分比为70〜50质量%,AB型的数均分子量 嵌段共聚物为10,000〜100,000。
    • 16. 发明专利
    • 熱可塑性エラストマー
    • 热塑性弹性体
    • JP2015017226A
    • 2015-01-29
    • JP2013146660
    • 2013-07-12
    • 日油株式会社Nof Corp
    • MOCHIDATE KAZUOMITASAKA TOMOHISA
    • C08L51/00C08F265/06C08J3/24C08K5/00C08L67/00
    • 【課題】製造性及び機械的強度に優れる熱可塑性エラストマーを提供する。【解決手段】(A)アクリルゴム100質量部と(B)熱可塑性ポリエステル15〜70質量部とを含む混合物を、0.1〜5質量部の(C)架橋剤の存在下、動的に架橋させて得られる。成分(A)は、ゲル分を含まないコア層と、ゲル分を含むシェル層とからなるコア−シェル構造となっている。コア層は、側鎖に炭素−炭素二重結合を有する多官能単量体由来の構成単位を含まず、シェル層は、側鎖に炭素−炭素二重結合を有する多官能単量体由来の構成単位を含む。【選択図】なし
    • 要解决的问题:提供可生产性和机械强度优异的热塑性弹性体。解决方案:通过动态交联包含100盎司(A)丙烯酸弹性体和15至70盎司((A) B)热塑性聚酯,在(C)交联剂的0.1〜5重量%的存在下进行。 组分(A)具有由不含凝胶含量的核心层组成的核 - 壳结构和含有凝胶含量的壳层。 核心层不包含衍生自侧链中具有碳 - 碳双键的多官能单体的结构单元和源自侧链中具有交联性基团的单体的结构单元,壳层包含衍生自 来自侧链中具有碳 - 碳双键的多官能单体。
    • 17. 发明专利
    • Thermoplastic elastomer
    • 热塑性弹性体
    • JP2013224382A
    • 2013-10-31
    • JP2012097847
    • 2012-04-23
    • Nof Corp日油株式会社
    • MOCHIDATE KAZUOMISUGIHARA YASUSHITASAKA TOMOHISA
    • C08L33/08C08J3/24C08K5/00C08L101/00
    • PROBLEM TO BE SOLVED: To provide a thermoplastic elastomer that is excellent in mechanical strength, sealability and the like by using a modified acrylic rubber having no gel content and having a crosslinking point.SOLUTION: A thermoplastic elastomer is produced by dynamically crosslinking a mixture including 100 pts.mass of (Y) a modified acrylic rubber and 15-70 pts.mass of (C) a thermoplastic resin under the condition that (D) a crosslinking agent is present in an amount of 0.1-2 pts.mass. The modified acrylic rubber (Y) is produced by the grafting reaction of 100 pts.mass of (A) an acrylic rubber including (a-1) a structural unit derived from EA in an amount of 30-70 pts.mass, (a-2) a structural unit derived from BA represented by formula (1) and/or MEA in an amount of 30-70 pts.mass and (a-3) a structural unit derived from GMA in an amount of 1-5 pts.mass based on (a-1)+(a-2)=100 pts.mass, with 0.5-10 pts.mass of (B) a polyfunctional compound having both one functional group that can react with an epoxy group and at least one carbon-carbon double bond. (In the formula, X is a methylene group or oxygen).
    • 要解决的问题:通过使用不具有凝胶含量并具有交联点的改性丙烯酸橡胶,提供机械强度,密封性等优异的热塑性弹性体。溶解性:热塑性弹性体是通过动态交联包括 (Y)改性丙烯酸橡胶的100重量份,(C)热塑性树脂的15-70重量份,(D)交联剂的量为0.1-2重量份。 改性丙烯酸橡胶(Y)通过100重量份的(A)丙烯酸类橡胶(包括(a-1)来自EA的结构单元)(30〜70重量份)的(a-1)的接枝反应 -2)衍生自由式(1)表示的BA和/或MEA的结构单元,其量为30-70pts.mass,(a-3)来自GMA的结构单元的量为1-5个。 基于(a-1)+(a-2)= 100pts.mass的质量,具有0.5-10质量份的(B)具有可与环氧基反应的一个官能团的多官能化合物和至少一种 碳 - 碳双键。 (式中,X为亚甲基或氧)。
    • 18. 发明专利
    • Material for forming film
    • 成膜材料
    • JP2005094270A
    • 2005-04-07
    • JP2003323761
    • 2003-09-16
    • Nof Corp日本油脂株式会社
    • TASAKA TOMOHISA
    • H04R7/02H04R1/00
    • PROBLEM TO BE SOLVED: To provide a material for forming a film used for a diaphragm for a speaker which can display an excellent waterproofing performance for a long period of time, and which can suppress a decrease in tone quality.
      SOLUTION: The material for forming the film used to form the film coating the surface of the diaphragm for the speaker includes a fluorine-containing polymer segment formed of a monomer containing a fluorine, and a fluorine-containing block copolymer made of a non-fluorine polymer segment formed of the monomer containing no fluorine. The fluorine-containing polymer segment is preferably formed of a mixture of the monomer containing a single monomer including the fluorine or a fluorine and an alkyl methacrylate having 12-22 of number of carbons of an alkyl group. The fluorine-containing block copolymer is preferably manufactured by a manufacturing method by a two-stage polymerizing method using a polymeric peroxide as a polymerization initiator.
      COPYRIGHT: (C)2005,JPO&NCIPI
    • 要解决的问题:提供一种用于形成用于扬声器的膜的材料,其可以长时间显示优异的防水性能,并且可以抑制音质的降低。 < P>解决方案:用于形成用于形成扬声器用隔膜的表面的膜的成膜用材料包括由含有氟的单体形成的含氟聚合物链段和含有氟的嵌段共聚物 由不含氟的单体形成的非氟聚合物链段。 含氟聚合物链段优选由含有包含氟或氟的单一单体的单体和具有烷基数的碳数为12-22的甲基丙烯酸烷基酯的混合物形成。 含氟嵌段共聚物优选通过使用聚合过氧化物作为聚合引发剂的两阶段聚合法的制造方法制造。 版权所有(C)2005,JPO&NCIPI
    • 20. 发明专利
    • Surface material for pen input device and pen input device
    • 用于笔输入装置和笔输入装置的表面材料
    • JP2003296008A
    • 2003-10-17
    • JP2003022653
    • 2003-01-30
    • Nof Corp日本油脂株式会社
    • HARADA EIJITASAKA TOMOHISAKUNISAWA SATORUTAKIZUKA NORIKAZU
    • G06F3/041G06F3/03
    • PROBLEM TO BE SOLVED: To provide a surface material for a pen input device and a pen input device excellent in the writing feel in particular based on the smoothness in writing. SOLUTION: The surface material for the pen input device consists of a base material and a surface layer. The coefficient of dynamic friction of the surface material is 0.02-0.5 when the surface of the surface layer is moved at the speed of 10 cm/sec by using an input pen whose load is 200 g under the atmosphere in a temperature of 20°C and with the relative humidity of 50% and the coefficient of static friction is 0.4-1.5. The surface material is restored with the load of at least 10 g on a super hard scratcher when the surface of the surface layer is scratched at the speed of 10 cm/sec by using the super hard scratcher whose diameter at the tip is 0.75 mm under the atmosphere in a temperature of 20°C and with the relative humidity of 50%. COPYRIGHT: (C)2004,JPO
    • 要解决的问题:提供一种用于笔输入装置的表面材料和特别是基于书写平滑度的书写感觉优异的笔输入装置。

      解决方案:笔输入装置的表面材料由基材和表面层组成。 当表面层的表面以10cm /秒的速度移动时,表面材料的动摩擦系数为0.02-0.5,使用在大气中在20℃的温度下负荷为200g的输入笔 相对湿度为50%,静摩擦系数为0.4-1.5。 当表面层的表面以10厘米/秒的速度被刮伤时,使用超硬的刮刀将其表面材料以至少10克的载荷恢复到超硬的刮刀上,该超硬刮刀的尖端直径为0.75毫米 气氛温度为20℃,相对湿度为50%。 版权所有(C)2004,JPO