热词
    • 1. 发明专利
    • Submerged arc welding method for high strength steel sheet
    • 用于高强度钢板的焊接弧焊方法
    • JP2006281303A
    • 2006-10-19
    • JP2005107989
    • 2005-04-04
    • Nippon Steel Corp新日本製鐵株式会社
    • MORIMOTO YUTAKASHINADA KOICHIYOSHIDA TATSUYATERADA YOSHIOHARA TAKUYA
    • B23K9/18B23K35/30B23K35/362B23K103/04C22C38/00C22C38/58
    • PROBLEM TO BE SOLVED: To provide a submerged arc welding method for a high strength steel sheet where, when a high strength steel sheet having a tensile strength of 700 to 1,200 MPa is subjected to submerged arc welding, a weld metal having high strength satisfying the tensile strength of 700 to 1,200 MPa which is equal to that of the steel sheet can be obtained, and also, a weld joint in which the defect of cracks generated at the toe parts of a weld bead is prevented, and which is free from defects, is sound and has excellent mechanical strength such as strength and fatigue strength can be obtained.
      SOLUTION: In the method where a high strength steel sheet having the tensile strength of 700 to 1,200 MPa is subjected to submerged arc welding using filling flux and a welding wire, using the flux having a particle distribution in which fine particles with the particle diameter of ≤210 μm are comprised by 5 to 60 mass%, a weld metal in which the ratio of the volume of a deposited metal (Vd) to the volume in a bevel per unit length of a weld bead (Vg), (Vd/Vg) is 1.05 to 3.00, and also having the tensile strength of 700 to 1,200 MPa is formed in the bevel.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:为了提供一种高强度钢板的埋弧焊接方法,其中当对具有700至1200MPa的拉伸强度的高强度钢板进行埋弧焊时,具有高的 可以获得满足与钢板相同的700〜1200MPa的拉伸强度的强度,也可以获得防止在焊缝的趾部产生的裂纹的缺陷的焊接接头, 无缺陷,声音良好,机械强度优异,可获得强度和疲劳强度。 解决方案:使用具有700〜1200MPa的拉伸强度的高强度钢板,使用填充焊剂和焊丝进行埋弧焊的方法中,使用具有粒子分布的助熔剂,其中微粒与 ≤210μm的粒径为5〜60质量%,焊接金属(其中沉积金属的体积比(Vd))与焊道单位长度的斜面(Vg)的比例(Vg),( Vd / Vg)为1.05〜3.00,在斜面上也形成了拉伸强度为700〜1200MPa。 版权所有(C)2007,JPO&INPIT
    • 2. 发明专利
    • Apparatus for manufacturing high strength welded steel pipe
    • 制造高强度焊接钢管的装置
    • JP2008260030A
    • 2008-10-30
    • JP2007103204
    • 2007-04-10
    • Nippon Steel Corp新日本製鐵株式会社
    • TERASAWA TAKASHIYOSHIDA TATSUYAHATTORI YUTAKATSURU EIJI
    • B21C37/08B21D5/12
    • PROBLEM TO BE SOLVED: To provide an apparatus for manufacturing a high strength welded steel pipe, which apparatus can manufacture a steel pipe having a sound welded portion by narrowing a seam gap and by optimizing the position of the seam while preventing the rotation and twist of the steel pipe in manufacturing the high strength welded steel pipe.
      SOLUTION: The apparatus for manufacturing the welded steel pipe by welding the butted portion of an O-can comprises a plurality of fin rolls having a circular disk shape fin portion to be partially inserted into the butted portion of the O-can to be carried and a hourglass shape drum for pressing the outer surface of the O-can in the neighborhood of the butted portion; a top roll for reforming the shape of the O-can and the shape of the butted portion; and a welding torch for welding the butted portion. The hourglass shape drum of the fin roll is formed such that the diameters of the portions separated in both directions from the fin portion outward increase with the separated distance.
      COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:为了提供一种高强度焊接钢管的制造装置,该装置可以通过缩小接缝间隙来制造具有声音焊接部分的钢管,并且通过优化接缝的位置同时防止旋转 并在制造高强度焊接钢管的钢管扭转。 解决方案:通过焊接O形罐的对接部分来制造焊接钢管的装置包括多个翅片辊,其具有圆形翅片部分,以部分地插入到O形罐的对接部分中 并且用于在对接部分附近按压O形罐的外表面的沙漏形鼓; 用于重新形成O形罐的形状的顶辊和对接部分的形状; 以及用于焊接对接部分的焊枪。 翅片辊的沙漏形状的鼓形成为使得从翅片部向外分离的部分的直径随分离距离而增加。 版权所有(C)2009,JPO&INPIT
    • 3. 发明专利
    • Method for manufacturing high-strength welded steel tube
    • 制造高强度焊接钢管的方法
    • JP2008119710A
    • 2008-05-29
    • JP2006304552
    • 2006-11-09
    • Nippon Steel Corp新日本製鐵株式会社
    • TSURU EIJIAGATA ATSUSHIYOSHIDA TATSUYASUZUKI TAKESHITERASAWA TAKASHIHATTORI YUTAKATERADA YOSHIO
    • B21C37/08B21D5/01
    • PROBLEM TO BE SOLVED: To provide a method for manufacturing a high-strength welded steel tube, which, when manufacturing a welded steel tube using a UOE process, prevents buckling, does not generate a crack from a weld part, such as a toe crack and an expanding crack, and does not cause tack-welding failure of the weld part.
      SOLUTION: In manufacturing a welded steel tube, the end parts of a steel plate is bent with a pressing force w(N/mm) of an upper die, which is determined by A≤w≤B or A×C≤w≤B/D, while satisfying the following formulae 0.15≤R
      1 /D≤0.25 and 135≤u≤160, wherein, R
      1 (mm) is the radius of curvature of the working face of an upper die, u(mm) is the distance in the horizontal direction from the center of curvature of the upper die to the end part of the steel plate, s(MPa) is the tensile strength of the steel plate, D(mm) is the outer diameter of the welded tube to be manufactured, A and B are the values determined by s, and C and D are the values determined by s and u.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:提供一种制造高强度焊接钢管的方法,当使用UOE工艺制造焊接钢管防止弯曲时,不会从焊接部分产生裂纹,例如 趾裂和扩张裂纹,不会引起焊接部位的焊接失效。

      解决方案:在制造焊接钢管时,钢板的端部以上模的压力w(N / mm)弯曲,由A≤w≤B或A×C≤ w≤B/ D,同时满足下列公式:0.15≤R 1 /D≤0.25和135≤u≤160,其中,R SB =(1 / 上模的工作面的曲率,u(mm)是从上模的曲率中心到钢板的端部的水平方向的距离,s(MPa)是钢板的拉伸强度 钢板,D(mm)是要制造的焊接管的外径,A和B是由s确定的值,C和D是由s和u确定的值。 版权所有(C)2008,JPO&INPIT

    • 4. 发明专利
    • Bead shape detection technique and device thereof
    • BEAD形状检测技术及其设备
    • JP2007192721A
    • 2007-08-02
    • JP2006012416
    • 2006-01-20
    • Nippon Steel Corp新日本製鐵株式会社
    • HASHIGUCHI SHOHEIKUNINAGA MANABUTERASAWA TAKASHISUZUKI TAKESHIYOSHIDA TATSUYA
    • G01B11/24B23K9/095B23K9/127B23K31/00B23K101/06G01B11/02G01B11/26
    • PROBLEM TO BE SOLVED: To provide a bead shape detection device capable of detecting bead shape more than comparable accuracy from cross-sectional profile of steel pipe obtained by optical means, such as photo cutting technique and laser range finder and the like, even if bead is of gently uneven as well as height of bead is low.
      SOLUTION: In the bead shape detection technique where linear beam of light or scanning dotted light is irradiated to weld zones of welded steel pipes, imageries on the surface of welded zones irradiated by linear beam of light or scanning dotted light are imaged, and the cross-sectional profile of steel pipes by optical means are detected, after a coordinate of a temporary apex of the bead is computed by the peak search from the cross-sectional profile, a range of a certain width including of apex of the bead is approximated with a first function, while, by adopting a position, as a starting point, which has a certain distance far from the temporary apex of bead as a reference, a certain width at outside is approximated with a second function, and after an intersecting point of the first function and the second function is computed as a terminal point of the bead, bead shape is computed.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:为了提供一种能够从诸如光切割技术和激光测距仪等通过光学装置获得的钢管的横截面轮廓上比可比较的精度更好地检测胎圈形状的胎圈形状检测装置, 即使珠子轻轻地不均匀,珠子的高度也低。 解决方案:在将线状光束或扫描点光照射到焊接钢管的焊接区的焊道形状检测技术中,对由线性光束或扫描点亮光照射的焊接区域的表面上的成像进行成像, 并且通过光学装置对钢管的横截面轮廓进行检测,在从横截面轮廓通过峰值搜索计算出胎圈的临时顶点的坐标之后,包括珠的顶点的一定宽度的范围 以第一功能近似,而通过采用距离珠的临时顶点一定距离作为起点的位置作为参考,外部的一定宽度用第二函数近似,并且在第 计算第一功能和第二功能的相交点作为珠的终点,计算珠形。 版权所有(C)2007,JPO&INPIT
    • 7. 发明专利
    • U press machine, and method for adjusting position of locker die in u press machine
    • U压机和调压机在U型压机中的位置的方法
    • JP2009113093A
    • 2009-05-28
    • JP2007290519
    • 2007-11-08
    • Nippon Steel Corp新日本製鐵株式会社
    • YOSHIDA TATSUYA
    • B21D5/01
    • PROBLEM TO BE SOLVED: To easily adjust the position of a locker die in a U press machine U-shaping a steel sheet. SOLUTION: The side confronted with a punch 21 with a bracket 23 sandwiched in the width direction of a steel sheet 2 includes a first movable body 26 movable along the length direction of the steel sheet 2. Further, the space between the bracket 23 and the first movable body 26 includes a second movable body 27 movable along the width direction of the steel sheet 2. The first movable body 26 includes a first movable body contact face being in contact with the second movable body 7, so as to be tilted with respect to the width direction and length direction of the steel sheet 2. The second movable body 27 includes a second movable body contact face being in contact with the first movable body contact face toward a direction along the first movable body contact face. COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:在U型机U型成型钢板中容易地调整更换模具的位置。 解决方案:在具有夹在钢板2的宽度方向上的支架23的冲头21的侧面上包括沿着钢板2的长度方向可移动的第一移动体26.此外,支架之间的空间 23和第一可移动体26包括沿着钢板2的宽度方向可移动的第二移动体27.第一可移动体26包括与第二可移动体7接触的第一可移动体接触面,以便于 相对于钢板2的宽度方向和长度方向倾斜。第二可移动体27包括与第一可移动体接触面朝向第一可移动体接触面的方向接触的第二可移动体接触面。 版权所有(C)2009,JPO&INPIT
    • 9. 发明专利
    • Method for producing high strength welded steel tube
    • 生产高强度焊接钢管的方法
    • JP2007275953A
    • 2007-10-25
    • JP2006107229
    • 2006-04-10
    • Nippon Steel Corp新日本製鐵株式会社
    • TSURU EIJIAGATA ATSUSHIYOSHIDA TATSUYATERASAWA TAKASHISUZUKI TAKESHI
    • B21D3/14B21C37/08B23K35/30C22C38/00C22C38/58
    • PROBLEM TO BE SOLVED: To provide a method for producing a high strength welded steel tube where the cracks of an expanded tube and thickness deviation in a seam weld zone produced upon tube expansion after seam welding can be prevented.
      SOLUTION: In the method for producing a high strength welded steel tube, a steel plate having a tensile strength of ≥850 MPa is formed into a tubular shape, the edge parts of the steel plate are butted each other and are seam-welded, and thereafter, tube expansion is performed in such a manner that a region with a high friction coefficient applied in which the friction coefficient between the inside face of the steel tube 1 and each tube expansion segment 3 is ≥0.15 is controlled so as to be a range where the central angle of the steel tube is 25° to 180° with the seam weld zone 2 as the center in the circumferential direction, and the friction coefficient between the inside face of the steel tube and each segment in the part other than the region with a high friction coefficient applied is controlled to
    • 要解决的问题:提供一种高强度焊接钢管的制造方法,其中可以防止在焊缝之后在管膨胀时产生的发泡管的裂纹和在焊缝区域中的厚度偏差。 解决方案:在高强度焊接钢管的制造方法中,将拉伸强度≥850MPa的钢板形成为筒状,钢板的边缘部彼此对接, 焊接后,进行管膨胀,使得控制钢管1的内面与各管膨胀段3之间的摩擦系数≥0.15的高摩擦系数的区域,以便 是以焊缝区域2为圆周方向为中心的钢管的中心角为25°〜180°的范围,钢管的内侧面与其他部分的各段之间的摩擦系数 比施加摩擦系数高的区域控制在<0.15。 版权所有(C)2008,JPO&INPIT
    • 10. 发明专利
    • U press machine, and method for adjusting locker die position in u press machine
    • U压机,以及在U压机中调节锁定位置的方法
    • JP2009113092A
    • 2009-05-28
    • JP2007290517
    • 2007-11-08
    • Nippon Steel Corp新日本製鐵株式会社
    • YOSHIDA TATSUYA
    • B21D5/01
    • PROBLEM TO BE SOLVED: To provide a U press machine for U-shaping a steel sheet in which the operation of inserting a spacer between a bracket and a bed and the operation of taking out the spacer from the space between the bracket and the bed can be smoothly performed, and also the position of the locker die can easily be adjusted.
      SOLUTION: The U press machine includes: a spacer supporting body 51 capable of supporting a plurality of spacers 30 at a position elevated from a bed 25; and an elevating/lowering body 52 capable of elevating/lowering relative to the spacer supporting body 51. The elevating/lowering body 52 lowers relative to the spacer supporting body 51, thus one or more spacers 30 among a plurality of the spacers 30 are collectively lowered relative to the spacer supporting body 51, and it elevates relative to the spacer supporting body 51, the lowered one or more spacers 51 are collectively elevated relative to the spacer supporting body 51.
      COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:提供一种U型成型机,用于U型成型钢板,其中在支架和床之间插入间隔件的操作以及从支架和托架之间的空间中取出间隔件的操作 床可以顺利地进行,并且也可以容易地调整储物柜的位置。 解决方案:U压机包括:间隔件支撑体51,其能够在从床25升高的位置处支撑多个间隔件30; 以及能够相对于间隔件支撑体51升降的升降体52.升降体52相对于间隔件支撑体51下降,因此多个间隔件30中的一个或多个间隔件30被集体 相对于间隔件支撑体51降低,并且相对于间隔件支撑体51升高,降低的一个或多个间隔件51相对于间隔件支撑体51共同升高。版权所有(C)2009,JPO&INPIT