    • 1. 发明专利
    • Apparatus for carrying material to be treated, and electrostatic coating method
    • 用于承载待处理材料的装置和静电涂层方法
    • JP2013136023A
    • 2013-07-11
    • JP2011288238
    • 2011-12-28
    • Koa Glass Kk興亜硝子株式会社
    • FUSHIMI KUNIHIRO
    • B05B5/08B05B13/02B05D1/04
    • PROBLEM TO BE SOLVED: To provide an apparatus for carrying materials to be treated and an electrostatic coating method using the apparatus, wherein the sideways or slanted striped pattern, gradation pattern or the like can easily be applied to the material to be treated by carrying the material while rotating in such a state as held at a gradient angle to the rotary shaft of a spindle and by applying a coating to the material in the above state.SOLUTION: The apparatus for carrying the material to be treated is provided with a spindle having a rotary shaft in a vertical direction. The spindle has a curved arm tool for holding the material at a slanted angle to the rotary shaft of the spindle, and the material is rotated in such a state as held at a prescribed gradient angle to the rotary shaft of the spindle.
    • 要解决的问题:提供一种用于承载待处理材料的设备和使用该设备的静电涂布方法,其中侧面或倾斜的条纹图案,渐变图案等可以容易地通过承载待处理的材料施加到被处理材料 材料,同时以与主轴的旋转轴成倾斜角度保持的状态旋转,并且在上述状态下对材料施加涂层。解决方案:用于承载待处理材料的装置设置有具有 旋转轴在垂直方向上。 主轴具有弯曲的臂工具,用于将材料以与主轴的旋转轴成倾斜的角度保持,并且材料以与主轴的旋转轴成规定的倾斜角度保持的状态旋转。
    • 2. 发明专利
    • Tubular flame burner and method for processing glass
    • 管状火焰燃烧器和玻璃加工方法
    • JP2013019557A
    • 2013-01-31
    • JP2011150955
    • 2011-07-07
    • Koa Glass Kk興亜硝子株式会社
    • MANABE CHIAKIISHIZUKA SATORU
    • F23D14/02C03B3/02C03B29/06C03C17/02C03C17/22F23D14/24F23D14/32F23D14/56
    • Y02P40/58
    • PROBLEM TO BE SOLVED: To provide a tabular flame burner that carries out flame polish processing and the like in a very short time by using tabular flame without contaminating the surface of a glass, and to provide a method of processing the glass.SOLUTION: This relates to the tabular flame burner, including: a block body; a cylindrical combustion chamber; a rectification path for fuel; an oxygen-containing gas rectification path formed along the cylindrical combustion chamber in the direction of another tangent; a fuel supply path formed along the rectification path for fuel in the direction of a normal; and an oxygen-containing gas formed along the oxygen-containing gas supply path in the direction of the normal; and relates to the method for processing the glass using the same. In the cylindrical combustion chamber, the fuel introduced through the fuel supply path and fuel rectification path and the oxygen-containing gas introduced through the oxygen-containing gas supply path and oxygen-containing gas rectification path are mixed to be burned.
    • 要解决的问题:提供一种通过使用片状火焰在非常短的时间内进行火焰抛光加工等而不污染玻璃表面的片状火焰燃烧器,并提供加工玻璃的方法。

      解决方案:这涉及片状火焰燃烧器,包括:块体; 圆柱形燃烧室; 燃油整流路; 沿圆筒形燃烧室沿另一切线方向形成的含氧气体整流路径; 燃料供给路径沿着正常方向沿燃料的整流路径形成; 以及沿着含氧气体供给路径沿法线方向形成的含氧气体; 涉及使用该玻璃的玻璃的加工方法。 在圆筒形燃烧室中,通过燃料供给路径和燃料精馏路径导入的燃料和通过含氧气体供给路径和含氧气体整流路径导入的含氧气体混合燃烧。 版权所有(C)2013,JPO&INPIT

    • 3. 发明专利
    • Antibacterial glass and method for manufacturing the same
    • 防霉玻璃及其制造方法
    • JP2012214381A
    • 2012-11-08
    • JP2012160278
    • 2012-07-19
    • Koa Glass Kk興亜硝子株式会社
    • KOBAYASHI YOSHINAOKITAMURA MAMORUKANAMARU SHINOBUTANAKA KENICHI
    • C03C12/00
    • PROBLEM TO BE SOLVED: To provide antibacterial glass capable of discharging a predetermined amount of silver ions quickly and for a long period of time and at the same time, excellent in discoloration preventing effect and discrimination ability, and a method for manufacturing the same.SOLUTION: In the granular antibacterial glass that exhibits the antibacterial effect by discharging silver ions and the method for manufacturing the same, the average granule diameter of the antibacterial glass is set to a value within a range of from 0.1 to 100 μm (100 μm is not included) and as a compounding ingredient, cobalt oxide as an inorganic colorant is contained and at the same time, the amount of addition of cobalt oxide is set to a value within a range of from 0.001 to 0.5 wt.% to the total amount.
    • 要解决的问题:为了提供能够快速且长时间地排出预定量的银离子并且同时具有优异的防变色效果和辨别能力的抗菌玻璃,以及制造方法 相同。 解决方案:在通过放出银离子而具有抗菌作用的颗粒状抗菌玻璃及其制造方法中,抗菌玻璃的平均颗粒直径设定在0.1〜100μm的范围内 不包括100μm),并且作为配混成分,含有作为无机着色剂的氧化钴,同时,氧化钴的添加量设定在0.001〜0.5重量%的范围内,相对于 总金额。 版权所有(C)2013,JPO&INPIT
    • 4. 发明专利
    • Decorative glass container and method for manufacturing the same
    • 装饰玻璃容器及其制造方法
    • JP2012179874A
    • 2012-09-20
    • JP2011045827
    • 2011-03-03
    • Koa Glass Kk興亜硝子株式会社
    • FUSHIMI KUNIHIRO
    • B41M5/00B05D1/26B41M1/34B41M5/50B41M5/52
    • PROBLEM TO BE SOLVED: To provide a decorative glass container configured to visually recognize an ink-jet decorative layer comprising an ultraviolet curable resin formed by an ink-jet method, and a method for efficiently manufacturing the decorative glass container.SOLUTION: In the decorative glass container etc., the ink-jet decorative layer 12 is formed at the back face side of the glass container 10 having a front face glass wall 10a and a rear face glass wall 10b arranged in parallel at a predetermined interval, and the ink-jet decorative layer is visually recognized via the front face glass wall and the rear face glass wall. The ink-jet decorative layer is formed by using the ultraviolet curable resin by the ink-jet method.
    • 要解决的问题:提供一种装配玻璃容器,其构造为在视觉上识别包括通过喷墨法形成的紫外线固化树脂的喷墨装饰层,以及用于有效地制造装饰玻璃容器的方法。 解决方案:在装饰玻璃容器等中,喷墨装饰层12形成在玻璃容器10的背面侧,玻璃容器10具有平行布置的前面玻璃壁10a和后面玻璃壁10b 预定间隔,并且经由前面玻璃壁和后面玻璃壁视觉识别喷墨装饰层。 通过喷墨法使用紫外线固化树脂形成喷墨装饰层。 版权所有(C)2012,JPO&INPIT
    • 5. 发明专利
    • Decorative container and method for manufacturing decorative container
    • 装饰容器及制造装饰容器的方法
    • JP2009001283A
    • 2009-01-08
    • JP2007160917
    • 2007-06-19
    • Koa Glass KkShiseido Co Ltd株式会社資生堂興亜硝子株式会社
    • MITSUMORI MITSUCHIKASAITO NAOMASAINOUE TAKASHI
    • B65D25/56A45D34/00B05D7/24B65D51/24
    • PROBLEM TO BE SOLVED: To provide a decorative container provided with a specified optical transmitting part so as to recognize the remaining amount or the like of a content in the decorative container which is opaque as a whole, and to provide a method for manufacturing such the decorative container. SOLUTION: The decorative container prepared by forming a resin coating film on the surface of a decorative container body equipped with a cap and the method for manufacturing it are provided. The optical transmitting part which is exposed under a condition that the decorative container is rotated in the vertical direction and employed for visualizing the content is provided on a part of the decorative container main body. For example, under a condition that the cap is perfectly mounted, the cap covers the optical transmitting part, and under a condition that the cap is imperfectly mounted, the optical transmitting part is exposed. COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:提供一种设置有特定的光学透射部件的装饰容器,以便识别整个不透明的装饰容器中的内容物的剩余量等,并且提供一种方法 制造这样的装饰容器。 解决方案:提供通过在装有盖的装饰容器主体的表面上形成树脂涂膜而制备的装饰容器及其制造方法。 在装饰容器主体的一部分上设置在装饰容器沿垂直方向旋转并用于使内容物可视化的条件下露出的光学传送部。 例如,在帽完全安装的情况下,盖覆盖光透射部,并且在帽不完全地安装的情况下,光透射部露出。 版权所有(C)2009,JPO&INPIT
    • 7. 发明专利
    • Fluorescent glass container and its manufacturing method
    • 荧光玻璃容器及其制造方法
    • JP2005047544A
    • 2005-02-24
    • JP2003281026
    • 2003-07-28
    • Fujikura Kasei Co LtdKoa Glass Kk興亜硝子株式会社藤倉化成株式会社
    • FUSHIMI KUNIHIROYAMAMOTO HARUICHIKOBAYASHI TATSU
    • B65D23/08B65D25/34C09K11/06
    • Y02W30/805Y02W30/807
    • PROBLEM TO BE SOLVED: To provide a fluorescent glass container with a uniform dispersibility of a condensing fluorescent pigment in a cured film coating, and also, which is excellent in the strength or the adhesion of the cured film coating, and its manufacturing method. SOLUTION: This fluorescent glass container is equipped with the cured film coating having a thickness of 3 to 60 μm which comprises a hardening fluorescent composition containing 0.1 to 100 pts.wt. of a polyol compound and in a range of 0.01 to 1 pts.wt. of the condensing fluorescent pigment based on 100 pts.wt. of a formaldehyde based resin or an acrylate based compound. The outer peripheral section of the glass container is selectively fluorescence-colored, and at the same time, at non-outer peripheral sections of the glass container, the visibility of a content is made excellent. COPYRIGHT: (C)2005,JPO&NCIPI
    • 要解决的问题:为了提供在凝固膜涂层中具有均匀分散性的聚光荧光颜料的荧光玻璃容器,以及固化膜涂层的强度或粘合性优异的荧光玻璃容器及其制造 方法。

      解决方案:该荧光玻璃容器配备有厚度为3〜60μm的固化膜涂层,其包含含有0.1〜100重量份的硬化荧光组合物。 的多元醇化合物,并且在0.01至1重量份的范围内 的聚光荧光颜料基于100重量份 的甲醛基树脂或丙烯酸酯类化合物。 玻璃容器的外周部分选择性地是荧光色的,同时在玻璃容器的非外周部分,内容物的可见度变得优异。 版权所有(C)2005,JPO&NCIPI