会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 7. 发明公开
    • SURFACE-COATED CUTTING TOOL WITH RIGID COATING LAYERS EXHIBITING EXCELLENT CHIPPING RESISTANCE
    • 表面涂层切削刀具具有刚性涂层,表现出优异的耐磨性
    • EP3269478A1
    • 2018-01-17
    • EP16764886.4
    • 2016-03-11
    • Mitsubishi Materials Corporation
    • SATO KenichiTATSUOKA ShoYAMAGUCHI Kenji
    • B23B27/14B23C5/16C23C16/34C23C16/36
    • B23B27/14B23B2228/105C23C16/34C23C16/347C23C16/36C23C16/403C23C28/042C23C28/044C23C28/42C23C30/005
    • Provided is a coated tool in which a hard coating layer has excellent hardness and toughness and exhibits excellent chipping resistance during high-speed intermittent cutting work. In a surface-coated cutting tool including at least a (Ti,Al) (C,N) layer as a hard coating layer on a surface of the coated tool, the layer includes an upper layer in which a periodic compositional variation in Ti and Al is present in crystal grains having an NaCl type face-centered cubic structure, and a lower layer in which a periodic compositional variation in Ti and Al is not present in crystal grains having an NaCl type face-centered cubic structure, the upper layer has a relatively high Al amount, the lower layer has a relatively low Al amount, a value of I (200)/I(111) of the upper layer is preferably greater than 10, a value of I(200)/I(111) of the lower layer is preferably less than 3, the lower layer is configured to have a composition inclined structure in which the Al amount gradually and continuously increases from a tool body side towards an upper layer side, the lower layer is formed of a layered structure including a plurality of layers, and the Al amount of each layer can gradually and stepwisely increase from the tool body side towards the upper layer side.
    • 本发明提供一种涂层工具,其中硬涂层具有优异的硬度和韧性,并且在高速断续切割加工期间表现出优异的耐崩裂性。 在至少包括(Ti,Al)(C,N)层作为涂覆工具表面上的硬涂层的表面涂覆切削工具中,该层包括上层,其中Ti和 Al存在于具有NaCl型面心立方结构的晶粒中,并且其中Ti和Al的周期性组成变化不存在于具有NaCl型面心立方结构的晶粒中的下层,上层具有 Al含量相对较高,下层的Al含量相对较低,上层的I(200)/ I(111)的值优选大于10,I(200)/ I(111) 优选小于3,下层被构成为具有Al量从工具主体侧朝向上层侧逐渐连续增加的组成倾斜构造,下层由层状结构形成 包括多个层,以及每层的Al量 能够从工具主体侧朝向上层侧逐渐地逐步增大。
    • 8. 发明公开
    • SURFACE-COATED CUTTING TOOL IN WHICH HARD COATING LAYER EXHIBITS EXCELLENT CHIPPING RESISTANCE
    • 麻醉药师SCHNEIDWERKZEUG MIT HARTERÜBERZUGSSCHICHTMIT HERVORRAGENDERSCHLAGBESTÄNDIGKEIT
    • EP3103572A1
    • 2016-12-14
    • EP15843784.8
    • 2015-09-18
    • Mitsubishi Materials Corporation
    • TATSUOKA ShoSATO KenichiYAMAGUCHI Kenji
    • B23B27/14C23C16/34C23C16/36
    • B23B27/148B23B2222/16B23B2222/28B23B2224/04B23B2226/125B23B2228/04B23B2228/105C23C16/0272C23C16/34C23C16/36C23C28/042C23C28/044C23C28/42
    • Provided is a coated tool in which a hard coating layer has excellent hardness and toughness and exhibits chipping resistance and defect resistance during long-term use. A surface-coated cutting tool is formed by coating the surface of a tool body with a (Ti 1-x Al x ) (C y N 1-y ) layer (the average amount Xavg of Al and the average amount Yavg of C satisfy 0.60 ≤ Xavg ≤ 0.95 and 0 ≤ Yavg ≤ 0.005). Crystal grains having an NaCl type face-centered cubic structure in the layer have {111} orientation, a columnar structure in which the average grain width W of the individual crystal grains having an NaCl type face-centered cubic structure is 0.1 µm to 2.0 µm and the average aspect ratio A thereof is 2 to 10 is included, and in the individual crystal grains having an NaCl type face-centered cubic structure, a periodic compositional variation in Ti and Al in the composition formula: (Ti 1-x Al x ) (C y N 1-y ) is present and the difference Δx between the average of maximum values of x which varies periodically and the average of minimum values thereof is 0.03 to 0.25.
    • 提供一种硬涂层具有优异的硬度和韧性并且在长期使用中具有耐崩裂性和耐缺陷性的涂覆工具。 通过用(Ti 1-x Al x)(C y N 1-y)层(Al的平均量Xavg和C的平均量Yavg满足C 1 N y y y)层涂覆工具主体的表面来形成表面涂覆的切削工具 0.60‰Xavg‰¤0.95和0‰¤Yavg‰0.005)。 层中具有NaCl型面心立方结构的晶粒具有{111}取向,其中具有NaCl型面心立方结构的单个晶粒的平均晶粒宽度W为0.1μm至2.0μm的柱状结构 并且其平均纵横比A为2至10,并且在具有NaCl型面心立方结构的单个晶粒中,组成式中的Ti和Al的周期性组成变化:(Ti 1-x Al x )(C y N 1-y),并且周期性变化的x的最大值的平均值和最小值的平均值之间的差“x”为0.03〜0.25。