    • 9. 发明公开
    • INTERLAYER FOR LAMINATED GLASS AND LAMINATED GLASS
    • 夹层玻璃和夹层玻璃夹层
    • EP3219685A1
    • 2017-09-20
    • EP15858800.4
    • 2015-11-10
    • KURARAY CO., LTD.
    • KOBAYASHI, TakuyaKUSUDOU, TakeshiYUI, TaigaISOUE, Koichiro
    • C03C27/12B32B25/08E06B3/66
    • B32B17/1055B32B17/10036B32B17/10577B32B17/10587B32B17/10724B32B17/10743B32B17/10761B32B17/1077B32B17/10788B32B25/042B32B25/08B32B2307/30B32B2309/105E06B3/66E06B3/6707E06B3/6715
    • An object of the present invention is to provide an interlayer film for laminated glass which has excellent sound insulating properties and which even when used for a long period of time in a high-temperature and high-humidity environment, is able to keep a haze good and is also able to suppress whitening from an edge side thereof.
      The present invention is concerned with an interlayer film for laminated glass including a sound insulating layer (layer A) and thermoplastic resin layers containing a thermoplastic resin (layers B), the sound insulating layer (layer A) being located between at least two of the thermoplastic resin layers (layers B), wherein with respect to a laminated glass obtained by interposing the interlayer film for laminated glass by two sheets of float glass and a laminated glass obtained by holding the laminated glass under conditions at 80°C and at a relative humidity of 95% for 1,000 hours, when a haze of a central portion of the laminated glass in accordance with JIS K 7105 is measured, an increase of the haze of the laminated glass after holding relative to the haze of the laminated glass before holding is 2% or less, and a distance of whitening from an edge side of the laminated glass after holding is 4 mm or less.
    • 本发明的目的在于提供一种隔音性优异,并且即使在高温高湿环境下长时间使用也能够保持良好的雾度的夹层玻璃用中间膜 并且还能够抑制从其边缘发白。 本发明涉及一种夹层玻璃用中间膜,其包含隔音层(A层)和含有热塑性树脂(B层)的热塑性树脂层,所述隔音层(A层)位于所述隔音层 对于夹层玻璃用夹层玻璃用夹层玻璃用夹层玻璃,夹持2片浮法玻璃而得到的夹层玻璃和将该夹层玻璃在80℃,相对温度80℃的条件下保持的夹层玻璃进行热塑性树脂层(B层) 湿度95%的条件下测定1000小时,相对于保持前的夹层玻璃的雾度,测定保持后的夹层玻璃的雾度的增加量,根据JIS K 7105测定夹层玻璃的中央部的雾度时 2%以下,保持后的夹层玻璃的边缘侧的白化距离为4mm以下。