热词
    • 8. 发明公开
    • 무방향성 전기강판용 강의 제조 방법
    • 用于制造非导电电工钢板的方法
    • KR1020130053177A
    • 2013-05-23
    • KR1020110118790
    • 2011-11-15
    • 주식회사 포스코
    • 채진우김대옥
    • C21D8/12
    • C21C3/00C21C7/064C21C7/0645
    • PURPOSE: A method for manufacturing steel for a non-oriented electric steel sheet is provided to control less than 0.004 weight% of a content of [S] and to minimize a content of [Al] by injecting a making material during a converter steel tapping in order to improve desulphurization efficiency in a second refining process by increasing a supplementary material content. CONSTITUTION: A method for manufacturing steel for a non-oriented electric steel sheet comprises the following steps: A supplementary material including a quicklime more than 7 kg/molten steel-ton and a fabrication agent are injected during a converter steel tapping; The steel for non-oriented electric steel sheet has less than 0.004 weight% of a content of [S] and less than 0.03 weight% of a content of [Al]; The supplementary material additionally includes a fluorite more than 1 kg/molten steel-ton as the steel for the non-oriented electric steel sheet. [Reference numerals] (AA) Quicklime input(kg/molten steel-ton); (BB) Mild steel[S], (%); (CC) Steel-making material input; (DD) Line type(steel-making material input)
    • 目的:提供一种用于制造用于非取向电工钢板的钢的方法,以控制小于0.004重量%的[S]含量,并且通过在转炉钢丝攻期间注入制造材料来使[Al]的含量最小化 为了通过增加补充材料含量来提高第二精炼过程中的脱硫效率。 构成:用于制造无方向性电工钢板用钢的方法,其特征在于,包括以下步骤:在转炉钢丝攻过程中,注入含有7kg以上的生石灰和钢水的补充材料和制造剂。 无取向电工钢板钢的含量小于0.004重量%,[Al]含量小于0.03重量%。 补充材料另外包括作为非取向电工钢板的钢的超过1kg /钢水的萤石。 (附图标记)(AA)生石灰输入(kg /钢水吨); (BB)轻钢[S],(%); (CC)炼钢材料投入; (DD)线型(炼钢材料输入)