    • 1. 发明公开
    • METHOD FOR PRODUCING POWDER COMPOUND CORES MADE FROM NANO-CRYSTALLINE MAGNETIC MATERIAL
    • 从纳米晶体材料制造粉末复合体的方法
    • KR20070085168A
    • 2007-08-27
    • KR20070017945
    • 2007-02-22
    • VACUUMSCHMELZE GMBH & CO KG
    • BRUNNER MARKUS
    • H01F41/02B22F3/00H01F1/00
    • H01F1/15375H01F1/14783H01F1/15333H01F41/0246
    • A method for producing powder compound cores made from a nano-crystalline magnetic material is provided to generate a flexible material with a range without an additional grinding at a pressure ranging from 1 to 20t/cm^2. A method for producing powder compound cores made from a nano-crystalline magnetic material includes the steps of: compressing an alloy powder used to generate a magnetic core in an amorphous state; and performing a heat treatment before grinding and compression under protective gas at a temperature ranging from 200 to 400 degrees in order to obtain brittleness of a material for grinding. A grinding of a reinforced tape is performed at a temperature between a temperature of a liquid nitrogen and a maximum room temperature according to a brittleness process temperature. A heat treatment of the magnetic core is performed at a temperature ranging from 540 to 580 degrees after molding.
    • 提供一种由纳米晶体磁性材料制成的粉末化合物芯的方法,以在1至20t / cm 2的压力范围内产生具有一定范围的柔性材料,而不需要另外研磨。 一种由纳米晶体磁性材料制成的粉末化合物芯的方法包括以下步骤:压制用于产生非晶状态的磁芯的合金粉末; 在200〜400度的保护气体中进行研磨压缩之前的热处理,以获得研磨材料的脆性。 根据脆性工艺温度,在液氮温度和最高室温之间的温度下进行加强带的研磨。 在成型后,在540〜580度的温度下进行磁芯的热处理。
    • 9. 发明专利
    • Magneto-acoustic marker for electronic article surveillance
    • 用于电子文章监视器的磁铁标记(MAGNETO-ACOUSTIC MARKER FOR ELECTRONIC ARTICLE SURVEILLANCE)
    • JP2011026703A
    • 2011-02-10
    • JP2010155302
    • 2010-07-07
    • Vacuumschmelze Gmbh & Co Kgヴァキュームシュメルツェ ゲーエムベーハー ウント コンパニー カーゲー
    • HERZER GISELHER
    • C22C45/02C22F1/10C21D6/00C22C19/03C22C45/04C22F1/00G08B13/24H01F1/153H01L41/12
    • G08B13/2408G08B13/2437G08B13/244G08B13/2442
    • PROBLEM TO BE SOLVED: To provide a magneto-acoustic marker having reduced size without degrading its performance. SOLUTION: A resonator for use in a marker containing a bias element which produces a bias magnetic field in a magnetomechanical electronic article surveillance system is produced from an annealed ferromagnetic ribbon having a basic composition FeaCobNicSixByMz (wherein a, b, c, x, y and z are in at%, wherein M is one or more glass formation promoting elements and/or one or more transition metals, and further, 46≤a≤53, 0≤b≤2, 30≤c≤35, 1≤x≤2, 15.5≤y≤16.5, 0≤z≤0.5 and a+b+c+x+y+z=100 are satisfied). The ferromagnetic ribbon is annealed in a magnetic field oriented perpendicularly to the ribbon axis and/or while applying a tensile stress to the ribbon along the ribbon axis. Single resonator or multiple resonator assemblies can be formed by cutting elements from the annealed ribbon. COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:提供具有减小的尺寸而不降低其性能的磁声标志。 解决方案:用于包含偏磁元件的标记的谐振器,该偏振元件在磁机电电子物品监视系统中产生偏置磁场,由具有基本组成FeaCobNicSixByMz(其中a,b,c,x)的退火铁磁带产生 ,y和z为%,其中M为一种或多种玻璃形成促进元素和/或一种或多种过渡金属,此外,46≤a≤53,0≤b≤2,30≤c≤35,1 ≤x≤2,15.5≤y≤16.5,0≤z≤0.5,a + b + c + x + y + z = 100)。 铁磁带在垂直于带状轴线定向的磁场中退火,和/或沿着带状轴向带状物施加拉伸应力。 可以通过从退火的带切割元件来形成单个谐振器或多个谐振器组件。 版权所有(C)2011,JPO&INPIT