    • GLASS-CERAMICS AND METHOD FOR MANUFACTURING THE SAME
    • 玻璃 - 陶瓷及其制造方法
    • WO2006080557A1
    • 2006-08-03
    • PCT/JP2006/301713
    • 2006-01-26
    • KABUSHIKI KAISHA OHARAMINAMIKAWA, Hiroyuki
    • MINAMIKAWA, Hiroyuki
    • C03C10/00
    • C03C10/0027
    • There are provided glass-ceramics comprising, in mass %, 50 - 60% SiO 2 , 22 - 26% Al 2 O 3 and 3 - 5% Li 2 O, having an average crystal grain diameter exceeding 100nm, and having an average linear thermal expansion coefficient of 30 x10 -7 /°C or below within a temperature range of 0°C to 50°C. These glass-ceramics are manufactured by a step of melting glass raw materials, a step of forming the molten glass, a step of annealing the formed glass, a first heat treating step for heat treating the annealed glass at a temperature of 650 - 750°C for 0.1 hour to 200 hours, and a second heat treating step for heat treating the glass at a temperature of 800 - 1000°C for 0.1 hour to 50 hours.
    • 提供了玻璃陶瓷,以质量%计含有50-60%的SiO 2,22-26%的Al 2 O 3 3和3 - 平均晶粒直径超过100nm的平均线性热膨胀系数为30×10 -7 /℃以下的5%Li 2 O 3 温度范围为0°C至50°C。 这些玻璃陶瓷通过熔融玻璃原料,形成熔融玻璃的步骤,退火所形成的玻璃的步骤,在650-750℃的温度下对退火玻璃进行热处理的第一热处理步骤来制造 0.1小时〜200小时,第二热处理工序,在800〜1000℃的温度下将玻璃热处理0.1小时〜50小时。