    • 8. 发明申请
    • METHODS FOR PRODUCING CATALYST SYSTEMS
    • 生产催化剂体系的方法
    • WO2011078923A1
    • 2011-06-30
    • PCT/US2010/056794
    • 2010-11-16
    • UNIVATION TECHNOLOGIES, LLCAGAPIOU, Agapios, K.ABICHANDANI, Jeevan, S.KUO, Chi-IPATEL, Ganu, H.
    • AGAPIOU, Agapios, K.ABICHANDANI, Jeevan, S.KUO, Chi-IPATEL, Ganu, H.
    • C08F10/00C08F4/659C08F4/602
    • C08F10/00C08F4/65912C08F4/65916
    • Disclosed herein are processes to prepare polymerization catalyst compositions. The process comprises contacting an alumoxane with a support material in the presence of a solvent to form a supported alumoxane. The supported alumoxane may then be heat treated at a temperature of 85°C or greater to form a heat treated supported alumoxane which is then separated from the solvent at a temperature of 800C or less to recover a dried heat treated supported alumoxane. Alternatively, the supported alumoxane may be first separated from the solvent at a temperature of 800C or less to recover a dried supported alumoxane which is then heat treated at a temperature of 85 0C or greater to form a heat treated supported alumoxane. The dried heat treated supported alumoxane or the heat treated supported alumoxane may then be combined with a polymerization catalyst compound to form a polymerization catalyst composition.
    • 本文公开了制备聚合催化剂组合物的方法。 该方法包括在溶剂存在下使铝氧烷与载体材料接触以形成负载的铝氧烷。 然后可以在85℃或更高的温度下对负载的铝氧烷进行热处理,以形成经热处理的负载铝氧烷,然后在800℃或更低的温度下从溶剂中分离,以回收干燥的经热处理的负载铝氧烷。 或者,可以在800℃以下的温度下首先将负载的铝氧烷与溶剂分离,以回收干燥的负载型铝氧烷,然后在85℃以上的温度下进行热处理,形成经热处理的负载铝氧烷。 然后将干燥的经热处理的负载铝氧烷或经热处理的负载铝氧烷与聚合催化剂化合物组合以形成聚合催化剂组合物。