    • 4. 发明授权
    • Method of injection molding an optical article out of thermoplastic synthetic material
    • 从热塑性合成材料注射成型光学制品的方法
    • US06790388B2
    • 2004-09-14
    • US10015663
    • 2001-12-17
    • Hao-Wen ChiuHsinjin Yang
    • Hao-Wen ChiuHsinjin Yang
    • B29D1100
    • B29D11/00413B29C45/561B29C45/73B29C45/7337B29C2045/7393B29L2011/0016Y10S425/808
    • For each lens molding cycle, the method comprises the following steps: raising the wall of the mold cavity to a heating temperature higher than or equal to the molding temperature of said material; filling the molding cavity with said material; at the end of filling, increasing the pressure of said material introduced in this way into the molding cavity up to a compacting pressure; and bringing the wall of the molding cavity to a cooling temperature to cool said molded material down to an unmolding temperature below its molding temperature, said cooling temperature being lower than said unmolding temperature. The molding cavity begins to be filled with said material before the heating temperature has been reached. Once both the compacting pressure of said material and the heating temperature of the molding cavity wall have been reached, they are both maintained for a given length of time.
    • 对于每个透镜成型周期,该方法包括以下步骤:将模腔的壁升高至高于或等于所述材料的成型温度的加热温度;用所述材料填充模腔;在填充结束时, 将以这种方式引入的所述材料的压力增加到模制腔中直到压实压力; 将模腔的壁磨成冷却温度以将所述模制材料冷却至低于其成型温度的未模制温度,所述冷却温度低于所述脱模温度。在加热温度之前,模制腔开始填充所述材料 已经到达 一旦达到了所述材料的压实压力和模腔壁的加热温度,则它们都保持一段给定的时间长度。