    • 10. 发明授权
    • Heat treated high lignin content cellulosic fibers
    • 热处理高木质素含量的纤维素纤维
    • US5709774A
    • 1998-01-20
    • US638463
    • 1996-04-26
    • Shahrokh A. Naieni
    • Shahrokh A. Naieni
    • A61L15/28D21C9/00D21C9/18D21H11/00D21H11/18
    • D21H11/18A61L15/28D21C9/007D21C9/18
    • Heat-treated-in-air high lignin content cellulosic fibers which are free of moieties from crosslinking agents, for use in absorbent structures, are prepared by fluffing high lignin content fibers at a consistency of at least 40%, and heating in air at atmospheric pressure at a temperature ranging from 120.degree. C. to 280.degree. C. fluffed fiber water admixture having a consistency of at least 60% or moisture-free fluffed fibers, to remove any moisture content and heat treat the resulting moisture-free high lignin content fibers for at least 5 seconds, or by heating a sheet of dry (0-40% moisture content) high lignin content fibers utilizing these same heating conditions and then fluffing.
    • 通过以高至少40%的稠度起绒高木质素含量的纤维,并在空气中在大气中加热来制备热处理空气中高木质素含量的纤维素纤维,其不含交联剂部分用于吸收结构中 在120℃至280℃的温度下的压力,具有至少60%或不含水分的绒毛纤维的稠度的绒毛纤维水混合物,以除去任何水分含量并热处理所得无水高木质素含量 纤维至少5秒钟,或者通过使用这些相同的加热条件加热干燥(0-40%水分含量)高木质素含量的纤维,然后起毛。