    • 1. 发明申请
    • LASER ULTRASONIC FLAW DETECTION METHOD AND APPARATUS
    • 激光超声波检测方法和装置
    • WO1993010445A1
    • 1993-05-27
    • PCT/JP1991001607
    • 1991-11-22
    • DORYOKURO KAKUNENRYO KAIHATSU JIGYODANNARUO, KazuteruARAI, Keisho
    • DORYOKURO KAKUNENRYO KAIHATSU JIGYODAN
    • G01N29/04
    • G01N29/2418G01N2291/044
    • A laser beam for ultrasonic generation is emitted to a reflector/vibrator to generate an ultrasonic wave, and the ultrasonic wave is transmitted to an object to be inspected. The ultrasonic wave transmitted to the object is reflected at a flaw inside the object, returns to the reflector/vibrator and vibrates it. The vibration is detected using a laser beam for ultrasonic detection to find flaws inside the object. According to the present invention, ultrasonic flaw detection can be made for reflecting materials having corrugations on their surface or having a low reflection factor of light, and for objects made of materials which cannot easily generate the ultrasonic wave by the laser beam. For such materials, the conventional method has not been useful because it adopts the direct application of the laser beam to the surface of the object to generate the ultrasonic wave.
    • 将用于超声波产生的激光束发射到反射器/振动器以产生超声波,并且将超声波传输到待检查对象。 传递到物体的超声波在物体内部的缺陷处被反射,返回到反射器/振动器并使其振动。 使用用于超声波检测的激光束检测振动,以发现物体内的缺陷。 根据本发明,可以对其表面具有波纹或具有低的反射系数的反射材料以及由不能通过激光束容易地产生超声波的材料制成的物体进行超声波探伤。 对于这种材料,常规的方法并不有用,因为它采用将激光束直接施加到物体的表面以产生超声波。
    • 10. 发明公开
    • A method for homogeneously mixing a uranium/plutonium mixed oxide
    • 维他命Uran /钚-Mischoxid
    • EP0907186A2
    • 1999-04-07
    • EP98307678.7
    • 1998-09-22
    • DORYOKURO KAKUNENRYO KAIHATSU JIGYODAN
    • Aoki, YoshikazuJike, JunjiKayano, Masashi
    • G21C3/62
    • G21C3/623Y02E30/38
    • A method for homogeneously mixing a uranium/plutonium mixed oxide which is used for the preparation of a uranium/ plutonium mixed oxide fuel. The method comprises weighing a uranium oxide powder, a plutonium oxide powder, and a dry recovered powder prepared by grinding a uranium/plutonium mixed oxide sinter so as to give a predetermined plutonium enrichment; roughly mixing these powders together by means of a mixer; pulverizing and homogeneously mixing the roughly mixed powder by means of a jet mill (16); discharging the homogeneously mixed powder together with compressed air from the jet mill; and separating the mixed powder from the air by means of a first-stage cyclone (18) to recover at least 90% of the discharged powder.
    • 用于均匀混合用于制备铀/钚混合氧化物燃料的铀/钚混合氧化物的方法。 该方法包括称重铀氧化物粉末,钚氧化物粉末和通过研磨铀/钚混合氧化物烧结体制备的干燥回收粉末,以得到预定的钚富集; 通过混合器大致将这些粉末混合在一起; 通过喷射磨机(16)粉碎并均匀混合粗混合粉末; 将均匀混合的粉末与来自喷射磨机的压缩空气一起排出; 并通过第一级旋风分离器(18)将混合粉末与空气分离,以回收至少90%的排出的粉末。