    • 자동차 폐 시트의 폴리우레탄 폼을 이용한 흡차음재 제조 방법 및 그에 의해 제조된 흡차음재 조성물
    • 使用来自汽车座垫泡沫的聚氨酯泡沫制造防腐材料的方法及其组合物
    • KR1020130005593A
    • 2013-01-16
    • KR1020110067079
    • 2011-07-06
    • 현대자동차주식회사기아자동차주식회사(주)경북
    • 구홍모김경남양준호김용태
    • D04H1/48D04H1/42
    • B29B17/0042B29K2075/00B29K2105/04D04H1/413D04H1/4266D04H1/485D04H1/544Y02W30/62
    • PURPOSE: A method for fabricating a soundproofing material is provided to recycle polyurethane foam and to prevent and to prevent static electricity generation. CONSTITUTION: A method for fabricating a soundproofing material comprises: a step of finely pulverizing a waste sheet; a step of mixing a polyester-based fiber, polyester-based fiber of low melting point, polypropylene fiber, thermoplastic fiber, and hemp in a polyurethane foam-crushed material; a step of carding the mixture; a step of needle-punching; a step of thermoforming and cooling; and a step of forming the mixture in a felt and cutting. The polyurethane foam is waste sheet foam or thermosetting polyurethane foam. [Reference numerals] (AA) Item; (BB) Operation; (CC) Picture; (DD) Condition; (EE) Pulverization; (F1) Pulverizing PU Foam + fibers; (F2) Mixing and Pulverizing PU Foam and fibers 2 times; (GG) Mixing; (H1,H4) Mixing PU, LM Fiber, PET Fiber Cloth; (H2) Using a hopper: uniformizing particles before carding; (H3) Primarily secondarily mixing; (II) Carding; (J1) Constantly material pulverizing and mixing -> forming web; (J2) Repeatedly carding -> increasing rolling and mixing rate; (J3) Carding 2 times: keeping predetermined supplying amount; (J4) Feed at 160-170rpm; (J5) Doper at 30-32M/min; (KK) Needle punching; (L1) Needle punching for firmly fixing PU with textile and fiber and constantly mixing materials; (L2) Bonding non-woven fabric; (L3) Rpm: 500-800; (L4) Depth; (MM) Thermoforming and cooling; (N1) Increasing bonding force by melting each material and LMFiber; (N2) Lowering the temperature of a board due to thermoforming; (N3) Using an oven, top: 190°C, bottom: 200°C; (N4) Using an air cooler, cooling temperature: 20-24°C; (OO) Heating roller and cutting; (P1) Adjusting thickness by a roller; (P2) Cutting a board into predetermined sizes; (P3) Using a heating roller (temperature: 201°C)
    • 目的:提供一种制造隔音材料的方法来回收聚氨酯泡沫,并防止和防止产生静电。 构成:隔音材料的制造方法,其特征在于,包括以下步骤:将废片细粉碎; 在聚氨酯泡沫破碎材料中混合聚酯类纤维,低熔点聚酯类纤维,聚丙烯纤维,热塑性纤维和大麻的工序; 梳理混合物的一步; 针刺一步; 热成型和冷却的一个步骤; 以及在毛毡和切割中形成混合物的步骤。 聚氨酯泡沫是废片泡沫或热固性聚氨酯泡沫。 (附图标记)(AA)项目; (BB)操作; (CC)图片; (DD)条件; (EE)粉碎; (F1)粉碎PU泡沫+纤维; (F2)混合和粉碎PU泡沫和纤维2次; (GG)混合; (H1,H4)混合PU,LM纤维,PET纤维布; (H2)使用料斗:梳理前使颗粒均匀; (H3)主要二次混合; (二)梳理; (J1)不断的材料粉碎和混合 - >成网; (J2)重复梳理 - >提高轧制速度; (J3)梳理2次:保持预定供应量; (J4)以160-170rpm进给; (J5)Doper以30-32M / min; (KK)针刺; (L1)针刺用于固定PU与纺织和纤维,并不断混合材料; (L2)粘合无纺布; (L3)Rpm:500-800; (L4)深度; (MM)热成型和冷却; (N1)通过熔化每种材料和LMFiber增加粘结力; (N2)通过热成型降低板的温度; (N3)使用烤箱,顶部:190℃,底部:200℃; (N4)使用空气冷却器,冷却温度:20-24℃; (OO)加热辊和切割; (P1)通过滚筒调节厚度; (P2)将板切割成预定尺寸; (P3)使用加热辊(温度:201℃)