    • 80. 发明专利
    • Steel for cold forging having superior suitability to carbonitriding
    • 用于冷锻的钢用于碳化的优先适用性
    • JPS6144159A
    • 1986-03-03
    • JP16700084
    • 1984-08-08
    • Kobe Steel Ltd
    • NAKAMURA MORIFUMIMATSUSHIMA YOSHITAKEKAWAKAMI HEIJIRO
    • C22C38/00C22C38/18C22C38/44C22C38/60
    • PURPOSE: To obtain a steel for cold forging having superior suitability to carbonitriding by adding prescribed percentages of C, Si, Mn, Cr, Al and O while satisfying specified equations.
      CONSTITUTION: This steel for cold forging having superior suitability to carbonitriding consists of, by weight, 0.10W0.30% C, 0.05W0.35% Si, 0.30W1.50% Mn, ≤2.5% Cr, 0.02W0.5% Al, ≤0.0030% O and the balance Fe with inevitable impurities and satisfies equations I, II. The steel has low deformation resistance during working by cold forging, and when the steel is carbonitrided after the working, an effective hardened layer having ≥800 hardness Hv is obtd. up to a large depth.
      COPYRIGHT: (C)1986,JPO&Japio
    • 目的:通过在满足规定的方程式的同时加入规定百分比的C,Si,Mn,Cr,Al和O,获得具有优越适用于碳氮共渗的冷锻钢。 构成:对于碳氮共渗具有优异适用性的这种用于冷锻的钢用重量比为0.10-0.30%的C,0.05-0.35%的Si,0.30-1.50%的Mn,<= 2.5%的Cr,0.02-0.5%的Al, 0.0030%O,余量为Fe与不可避免的杂质,满足式I,II。 该钢在通过冷锻加工时具有低的变形阻力,并且当加工后钢被碳氮共混时,可获得具有> = 800硬度Hv的有效硬化层。 达到很大的深度。