    • 71. 发明专利
    • METHOD FOR CONTROLLING SPEED OF TANDEM ROLLING MILL
    • JPH0446621A
    • 1992-02-17
    • JP15260790
    • 1990-06-13
    • KAWASAKI STEEL CO
    • YOSHIDA KUNIONOMURA NOBUAKITAKECHI TOSHISADA
    • B21B37/00B21B37/46B21B37/52
    • PURPOSE:To realize the stable tandem rolling by measuring the speed change of the stand which speed is reduced with electric-controlling caused on the over load, and reducing the speed of the other all stands only by the rate of this speed change. CONSTITUTION:For example, if the over load is generated on the 2nd stand and the speed control device 8 controls the electric current of the motor 7, the speed command being powered finally from the speed control device 8 to the motor 7, the signal of the contact point A to close with the current control to the motor 7, and the present rolling speed outputting from the pulse generator 18 are transmitted to the MRH correcting circuit 17. So, the MRH correcting circuit 17 searches the rate of the speed change generated based on the above electric wave control with the speed control 8 at each stand, controls for reducing the speed of the other all stands with the above rate of speed change till that the value of electric current of the motor 7 of this electric current controlled stand is stabilized within the regular max. electric current (concretely 90% of the max. electric current). Therefore, the stable tandem rolling can be executed if the speed change is generated on the electric current control stand.
    • 75. 发明专利
    • ROLLING METHOD FOR CONTROLLING WIDTH OF HOT STRIP
    • JPS61232012A
    • 1986-10-16
    • JP7403085
    • 1985-04-08
    • KAWASAKI STEEL CO
    • NOMURA NOBUAKIITO YASUMICHI
    • B21B37/00B21B37/22
    • PURPOSE:To eliminate width variations for even cooled products and to increase a yield by setting the width target value within a specified length from the front end of a strip at a smaller value than the target value for the residual length of the strip. CONSTITUTION:A computer 1 containing a numerical table used to correct deviations of a plate width of products after cooling based on types of steel and a size of cooled materials 2 determines a target value, a target value changing point, and succeeding target values of the front end of the rolled material 2 at the outlet side of a rougher 3 with consideration for width variations of the rolled material 2 in a finisher 6 following the rougher 8 and a rolling schedule, and outputs those values to a width control computer 4. The width of the material 2 in a specified length from the front end of the material 2 at the outlet side of the finisher 6 is controlled to be smaller than that of the residual length of the material 2, so that the material 2 would by a winder 8 at the rear of the outlet sie of the finisher 6 and cooled has little width variation in the longitudinal direction.