热词
    • 71. 发明授权
    • Process for producing powdery linear polymer having improved powder properties
    • 具有改善的粉末性质的粉末状线性聚合物的制备方法
    • US07157520B2
    • 2007-01-02
    • US10493935
    • 2002-08-28
    • Atsuhiro HiguchiYasuhiro Suzuki
    • Atsuhiro HiguchiYasuhiro Suzuki
    • B32B5/16C08L31/02
    • C08F291/00C08F6/22C08F257/02C08F265/04C08F285/00C08L51/003Y10S525/902Y10T428/2998C08L2666/02
    • A powdery linear polymer having a narrow particle size distribution with little dusting and excellent in anti-blocking property is recovered from a latex of a linear polymer containing a large proportion (35–75 wt. %) of soft polymer (S) component through a two-step coagulation process including a first (moderate coagulation) step causing 70–98 wt. % of the coagulation. The linear polymer in the latex has a multilayer structure comprising a linear polymer (S) having a glass transition temperature below 40° C. and a linear polymer (H) having a higher glass transition temperature disposed in totally at least two layers and containing 35–75 wt. %, as a whole, of the linear polymer (S) with the proviso that the linear polymer (S) cannot be contained in excess of 30 wt. % in an outermost layer of the multilayer structure.
    • 从具有较大比例(35-75重量%)软质聚合物(S)组分的线性聚合物的胶乳通过一种或多种的软质聚合物(S)组分回收具有窄粉粒度分布小且抗粘连性优异的粉末状线性聚合物 两步凝结过程包括第一(中等凝结)步骤,产生70-98wt。 %的凝血。 胶乳中的线性聚合物具有包含玻璃化转变温度低于40℃的线性聚合物(S)和具有较高玻璃化转变温度的直链聚合物(H)的多层结构,其总体上至少设置在两层中并含有35 -75重量% 线性聚合物(S)的整体上的%,条件是线性聚合物(S)不能超过30重量%。 %的多层结构的最外层。
    • 76. 发明申请
    • Process for producing molded article of reclaimed thermoplastic resin
    • 回收热塑性树脂成型体的制造方法
    • US20050127579A1
    • 2005-06-16
    • US10502116
    • 2003-01-23
    • Yasuhiro Suzuki
    • Yasuhiro Suzuki
    • B29B17/00B29C44/34B29C45/17B29D22/00B29C45/00
    • B29C44/3411B29B17/0042B29C45/1704Y02W30/62
    • The object of the present invention is to provide a recycled molded article, not having defects such as sink, warping, bending, and the like, and whose molding contraction does not change substantially depending on its recycle turn number so that said molded article having a good dimensional stability can be manufactured without changing design of the injection molding machine or molding conditions in every turn. To attain this object, the gas assist injection molding method or the expansion injection molding method wherein gas pressure or expansion pressure is effected on the melted molding material mixture in the mold, are applied in the present invention. By applying these methods, the melted molding material mixture may fill the mold uniformly and contraction strain by cooling may be absorbed in the inner hollow or the foamed structure in the resulting molded article, and further change of mold contraction depending on recycle turn number is reduced to obtain a molded article having a good dimension stability.
    • 本发明的目的是提供一种不具有凹陷,翘曲,弯曲等缺陷的再循环成型品,其成型收缩根据其循环回转数不发生显着变化, 可以在不改变注塑机的设计或每一轮的成型条件的情况下制造良好的尺寸稳定性。 为了达到上述目的,在本发明中应用气体辅助注射成型法或膨胀注射成型法,其中在模具中熔融的成型材料混合物上进行气体压力或膨胀压力。 通过应用这些方法,熔融的成型材料混合物可以均匀地填充模具,通过冷却的收缩应变可以被吸收到所得模制品中的内部中空或发泡结构中,并且根据再循环转数而进一步改变模具收缩 以获得具有良好尺寸稳定性的模塑制品。
    • 79. 发明授权
    • Molding thermoplastic resin material and a method for equal quality recycle of thermoplastic resin mold
    • 热塑性树脂模塑成型和热塑性树脂模具等质量循环的方法
    • US06703445B2
    • 2004-03-09
    • US09969975
    • 2001-10-03
    • Yasuhiro Suzuki
    • Yasuhiro Suzuki
    • C08K554
    • C08J11/06B29B17/00Y02W30/62Y02W30/701
    • The object of the present invention is to provide a molding thermoplastic resin material giving resin mold whose quality and value are substantially equal to original resin mold even in a case where said resin mold is recycled. To attain said object, olefin group rubber and/or acrylic rubber to which monomer(s) being the same or similar monomer as (to) monomer(s) composing said molding thermoplastic resin material is(are) graft-copolymerized to give said rubbers compatibility with said molding thermoplastic resin material is(are) added in said molding thermoplastic resin material to improve said equal quality recycling property (property that quality and value are substantially equal to original thermoplastic resin mold even in a case where said thermoplastic resin mold is recycled). Said olefin group rubber and/or said acrylic rubber has(have) excellent thermal stability, heat-resistance, ozone resistance, oxidation resistance, and durability and has(have) effect on improvement of impact resistance for said thermoplastic resin material which is substantially immutable against heat history affected by repeated recycles and said molding thermoplastic resin material of the present invention can be used as a resin material of equal quality resin mold whose quality and value are substantially equal to resin mold using virgin resin material even in a case where said resin mold is recycled.
    • 本发明的目的是提供一种成型热塑性树脂材料,其树脂模具的质量和价值基本上等于原始树脂模具,即使在所述树脂模具被再循环的情况下,为了达到上述目的,烯烃基橡胶和/或 丙烯酸橡胶与构成所述成型热塑性树脂材料的(单体)单体相同或相似的单体被接枝共聚以使所述橡胶与所述成型热塑性树脂材料相容, 添加在所述成型热塑性树脂材料中以改善所述相同质量的再循环性能(即使在所述热塑性树脂模具被再循环的情况下,其质量和数值基本上等于原始热塑性树脂模具的性质)。烯烃基橡胶和/或所述丙烯酸酯 橡胶具有优异的热稳定性,耐热性,耐臭氧性,抗氧化性和耐久性,并具有对改进的影响 所述热塑性树脂材料的电阻基本上不能反映受重复再循环影响的热历史,并且本发明的所述模塑热塑性树脂材料可用作等品质树脂模具的树脂材料,其质量和值基本上等于树脂模具 即使在所述树脂模具被再循环的情况下也使用原始树脂材料。