    • 65. 发明专利
    • FILM FORMING DEVICE BY LASER LIGHT
    • JPS6487767A
    • 1989-03-31
    • JP24599987
    • 1987-09-30
    • TOSHIBA CORP
    • NAKAMURA SUGURUKINOSHITA JUNICHISASAKI MITSUOMURASE AKIRAYAMADA MINORU
    • C23C14/28C01G1/00C01G3/00C30B29/22H01B12/06H01B13/00H01L21/208H01L39/24
    • PURPOSE:To optimize the respective effect of dissolving a powder material and the acceleration of the deposition of a metallic compd. on a substrate and to uniformize the energy density of laser beams by using 1st and 2nd laser projecting means so that the laser beams are projected in the routes different from the supply route of the powder material. CONSTITUTION:A DC high voltage is impressed between a substrate 22 and an electrode 34. Gaseous O2 is simultaneously supplied from a cylinder 33 and the powder material is supplied from a supplying device 31 to respective nozzles 30 so that the powder material is ejected into a vacuum chamber 20 by the gaseous O2. The gaseous O2 is activated by the glow discharge generated between the substrate 22 and an electrode 34 at this time and the substrate 22 is heated by supplying electric power from a power supply 24 to a heater 23. The laser beam is outputted from a light source 40 and is projected by the 1st projecting means 41 in the direction orthogonal with the supply directions of the gaseous O2 and the powder material and the above- mentioned discharge direction to melt the powder material. Furthermore, the laser beam is projected from the direction different from the means 41 by the 2nd projecting means 45, by which the deposition of the metallic compd. on the substrate 22 is assisted.
    • 66. 发明专利
    • CONNECTING METHOD FOR COMPOUND SUPERCONDUCTIVE CABLE
    • JPS6433871A
    • 1989-02-03
    • JP18824687
    • 1987-07-28
    • TOSHIBA CORP
    • MURASE AKIRASHIRAKI KAZUO
    • H01R43/00
    • PURPOSE:To obtain the connection of about 10 OMEGA or lower by bringing filaments at the end section into contact with each other before the heat treatment is applied, enveloping the connection section with a base metal or the same material as the base metal, and applying the temperature and pressure to connect the filaments to each other in a solid phase diffusion state. CONSTITUTION:Prior to the heat treatment, a base metal 1 is melted and removed with nitric acid over the length range of 3cm from the end section of wires 4a, 4b, for example, part of filaments 3 are exposed, the whole exposed filament portions 3a are overlapped and inserted into a sleeve 7 formed with the same composition material as the base metal 1. Part of the sleeve 7 covers the base metal 1 of the wires 4a, 4b, and the copper alloy powder with the same composition as the sleeve 7 is filled in the sleeve 7. The pressure is applied to the sleeve 7 to crush the sleeve 7, then the sleeve 7, filament portions 3a, copper alloy powder, and end sections of wires 4a, 4b are integrated, the portion fitted with the sleeve 7 is heated, then the filament portions 3a are kept in a solid phase diffusion connection state, and the connection of about 10 OMEGA or below is realized.
    • 67. 发明专利
    • MANUFACTURE OF COMPOUND SUPERCONDUCTIVE WIRE
    • JPS6410525A
    • 1989-01-13
    • JP16587987
    • 1987-07-02
    • TOSHIBA CORP
    • NAKAYAMA SHIGEOYAMADA MINORUMURASE AKIRAFUKUSHIMA EIJI
    • B28B1/00C01G1/00C04B35/00C04B35/45H01B12/04H01B13/00
    • PURPOSE:To form a wire rod with the high critical temperature and high critical current density at a low cost by storing a mixture of multiple kinds containing the elements capable of synthesizing an oxide compound superconductor in a coated tube with the double-tube structure of a copper net on the inside and silver on the outside, linearly face-reduction-machining it, and heat-treating it in the oxygen gas atmosphere. CONSTITUTION:Y2O3 powder, BaCO3 powder, and CuO powder are mixed with the mol ratio of 0.5:2.0:3.0 into a powder mixture 1, which is temporarily baked for 2hr at 900 deg.C in the air then crushed and further pulverized with a ball mill. It is stored in a coated tube 4 with the double-tube structure constituted of a silver tube 2 with the outer diameter of 14mm, inner diameter of 13mm, and length of 70mm and a copper net tube 3 with the outer diameter of 12.8mm, inner diameter of 11.0mm, and length of 70mm located on its inside, both end openings are sealed and drawing-machined to form a wire rod 5 with the diameter of about 0.5mm. The whole thickness of the coating material 6 of this wire rod 5 is 200mum, 10mum of which is a silver layer 7 and the remaining portion is a copper layer 8. The heat treatment is then applied for 24hr at 900 deg.C in the oxygen gas.
    • 70. 发明专利
    • MANUFACTURE OF SEPERCONDUCTING COIL
    • JPS63287010A
    • 1988-11-24
    • JP12185987
    • 1987-05-19
    • TOSHIBA CORP
    • YAMADA MINORUNAKAYAMA SHIGEOMURASE AKIRA
    • C04B35/00B28B3/02C01G1/00C04B35/45H01F6/06
    • PURPOSE:To manufacture a coil without cracking and distortion by containing a spiral separation filler in a compression cavity of a metal mold, filling mixture therein, applying an axial compression force to the content in the cavity to obtain a compression block, and heat treating the block. CONSTITUTION:Spirally formed separation filler 5 is contained in compression cavities of metal molds 3, 4 having a cylindrical compression cavity, and the step of filling mixture 1 of several types of powders including elements to be synthesized with oxide compound superconductor in the cavity formed by the presence of the filler 5 is provided. Then, the content in the cavity 2 is applied by axial compression force of 1000 kg/cm larger to provide the step of obtaining a cylindrical compress block. Then, the step of heat treatment for the block in an oxygen atmosphere is provided. Thus, the number of turns of the filler 5 set to simply manufacture a superconducting coil of desired num ber of turns is simply manufactured, shaped in a coil form, then heat treated at 850-950 deg.C for 2 hours. Accordingly, the superconducting layer is manufac tured without cracking and deformation.