    • 68. 发明专利
    • Repair method of concrete structure and the concrete structure
    • 混凝土结构修复方法及混凝土结构
    • JP2012007290A
    • 2012-01-12
    • JP2010141144
    • 2010-06-22
    • Denki Kagaku Kogyo Kk電気化学工業株式会社
    • FUJIMA SEIJIANDO TOSHIHIRO
    • E04G23/02
    • PROBLEM TO BE SOLVED: To provide a repair method of a concrete structure capable of visually observing the progress of degradation such as a crack present on a surface of the concrete structure even after attaching a fiber sheet to the concrete structure, improving workability during construction, more stably holding the fiber sheet on the surface of the concrete structure and performing highly reliable repair in a long term.SOLUTION: In a repair method of a concrete structure, a fiber sheet is attached to a surface of the concrete structure with a 2-liquid main agent type acrylic resin adhesive comprising a primer and a fiber adhesive. The viscosity of the primer at 20°C and 20 rpm measured according to JIS K 7117-1 is 200-2,000 mPa s, the viscosity of the fiber adhesive at 20°C and 20 rpm measured immediately after mixing 2 liquids thereof is 2,500-5,000 mPa s, and the viscosity of the mixed liquid at 20°C and 20 rpm measured after leaving it still for five minutes is 15,000-30,000 mPa s.
    • 要解决的问题:即使在将纤维片材粘合到混凝土结构体上之后,提供能够目视观察劣化进展的混凝土结构的修复方法,例如在混凝土结构的表面上存在的裂纹,提高加工性 在施工期间,将纤维片更稳定地保持在混凝土结构的表面上,并且长期进行高度可靠的修复。 解决方案:在混凝土结构的修复方法中,纤维片用包含底漆和纤维粘合剂的2-液体主剂型丙烯酸树脂粘合剂附着在混凝土结构的表面上。 在根据JIS K 7117-1测量的20℃和20rpm下底漆的粘度为200-2,000mPa·s,在混合2个液体后立即测量的20℃和20rpm下的纤维粘合剂的粘度为2500- 5,000mPa·s,并且在静置5分钟后测量的20℃和20rpm下的混合液的粘度为15,000-30,000mPa·s。 版权所有(C)2012,JPO&INPIT
    • 69. 发明专利
    • Composition and composition for impregnation
    • 组合物和组合物进行印刷
    • JP2010202467A
    • 2010-09-16
    • JP2009051389
    • 2009-03-04
    • Denki Kagaku Kogyo Kk電気化学工業株式会社
    • ANDO TOSHIHIROFUJIMA SEIJIITO SHUNJI
    • C04B41/63C08F299/00C08L47/00C09D4/02C09D7/12
    • C04B41/483C04B41/009C04B2111/2038C04B2111/26C04B41/50C04B2103/10C04B28/06
    • PROBLEM TO BE SOLVED: To provide a composition for impregnation capable of improving the corrosion resistance of a hydraulic material precursor by being applied and impregnated on the surface of the hydraulic material precursor such as concrete.
      SOLUTION: The composition comprises (a) a polyfunctional (meth)acrylate having two or more ethylenically unsaturated double bonds which are not adjacent to carbonyl group in one molecule and two or more (meth)acryloyl groups in one molecule, (b) a monofunctional acrylate and/or a polyfunctional acrylate having no two or more ethylenically unsaturated double bonds, which are not adjacent the carbonyl group in one molecule, (c) a polymerization initiator, (d) a decomposition accelerating agent and (e) an inorganic layered compound.
      COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:提供一种浸渍组合物,其能够通过施加和浸渍在诸如混凝土的水硬性材料前体的表面上来提高水硬性材料前体的耐腐蚀性。 组合物包含(a)具有两个以上烯键式不饱和双键的多官能(甲基)丙烯酸酯,其在一个分子中不与羰基相邻,在一个分子中具有两个或更多个(甲基)丙烯酰基,(b )单分子中不邻近羰基的单官能丙烯酸酯和/或不具有两个或更多个烯属不饱和双键的多官能丙烯酸酯,(c)聚合引发剂,(d)分解促进剂和(e) 无机层状化合物。 版权所有(C)2010,JPO&INPIT
    • 70. 发明专利
    • Resin composition
    • 树脂组合物
    • JP2009275116A
    • 2009-11-26
    • JP2008127735
    • 2008-05-14
    • Denki Kagaku Kogyo Kk電気化学工業株式会社
    • ANDO TOSHIHIROTOMOSAWA AKIHISAFUJIMA SEIJI
    • C08F2/44C08F220/10C09J4/02C09J11/04C09J11/06C09J11/08
    • PROBLEM TO BE SOLVED: To provide a resin composition ensuring necessary water cut-off performance even when a bonded part is brought into contact with water for a long term. SOLUTION: The resin composition comprises 100 pts.mass of a (meth)acrylic acid ester monomer (A) having one or more phenyl groups in the molecule and giving a cured product having a glass transition temperature of ≤0°C, 5-100 pts.mass of a hydroxyalkyl (meth)acrylate (B), a petroleum resin (C), a filler (D), a polymerization initiator (E), a metallic soap (F), and semi-drying oil and/or drying oil (G). Based on 100 pts.mass of the total of the components (A) and (B), the content of the component (C) is 1-40 pts.mass, the content of the component (D) is 20-300 pts.mass, the content of the component (E) is 0.5-8 pts.mass, and in terms of metal, the content of the component (F) is 0.01-1.0 pts.mass. A concrete structure and a metallic structure, wherein adhesive bonding by the resin composition is carried out, are also provided. COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:即使当长期接合部分与水接触时,也提供确保必要的截水性能的树脂组合物。 解决方案:树脂组合物包括100分钟的分子中具有一个或多个苯基的(甲基)丙烯酸酯单体(A),并得到玻璃化转变温度≤0℃的固化产物, 5-100份(甲基)丙烯酸羟烷基酯(B),石油树脂(C),填料(D),聚合引发剂(E),金属皂(F)和半干性油 /或干油(G)。 基于组分(A)和(B)的总计100份,组分(C)的含量为1-40个氨基甲酸,组分(D)的含量为20-300个。 质量,组分(E)的含量为0.5-8质量%,以金属计,组分(F)的含量为0.01-1.0质量份。 还提供了通过树脂组合物进行粘合的具体结构和金属结构。 版权所有(C)2010,JPO&INPIT