    • Reactive stock solution for reaction injection moulding, reaction injection molding method and reaction injection molded article
    • 反应注射成型反应注射成型方法及反应注射成型的反应性解决方案
    • JP2009263469A
    • 2009-11-12
    • JP2008113504
    • 2008-04-24
    • Rimtec KkRimtec株式会社
    • KAMEI NOBUTO
    • C08G61/08B29C45/00C08K3/04C08K3/22C08K3/28C08K3/36C08K3/38C08L65/00
    • PROBLEM TO BE SOLVED: To provide a reaction injection molded article having no air bubbles in the inside of the molded article without imposing an undue burden on equipment and with a simple formulation.
      SOLUTION: A reactive stock solution (A) for reaction injection molding is used for reaction injection molding by subjecting a norbornene-based monomer to bulk polymerization within a mold and comprises at least a norbornene-based monomer, a non-basic filler and a Shiff base coordinated metathesis polymerization catalyst represented by formula (1). A reaction injection molding method comprises injecting a blending solution comprising as an essential component the reactive stock solution for reaction injection molding (A) into a mold and carrying out bulk polymerization within the mold. A reaction injection molded article is produced by the reactive injection molding method.
      COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:提供在模制品内部没有气泡的反应注射成型制品,而不会对设备造成不必要的负担,并且具有简单的配方。 解决方案:用于反应注射成型的反应性储备溶液(A)用于反应注射成型,其通过使降冰片烯类单体在模具内进行本体聚合,并且至少包含降冰片烯系单体,非碱性填料 和由式(1)表示的希夫碱协同易位聚合催化剂。 反应注射成型方法包括将包含反应注射成型(A)的反应性储备溶液作为必要成分的共混溶液注入模具中并在模具内进行本体聚合。 通过反应性注射成型法制造反应注塑制品。 版权所有(C)2010,JPO&INPIT
    • 64. 发明专利
    • In-mold coating method and coated molding
    • 模内涂层方法和涂层成型
    • JP2007313395A
    • 2007-12-06
    • JP2006143576
    • 2006-05-24
    • Rimtec KkRimtec株式会社
    • TAKEUCHI MASAKI
    • B05D7/14B29C45/16
    • PROBLEM TO BE SOLVED: To provide an in-mold coating method capable of forming an even cover coating film without causing a non-coated defective portion even if a coated object is a big molding and a coated molding obtained thereby.
      SOLUTION: In-mold coating method that injects a cover into a cover coating space formed by a resin molding and a mold from cover injection ports provided at the mold to form a cover layer on a surface of the resin molding, after forming a resin where a resin material is injected into a cavity formed by the mold of a pair of male mold and female mold, wherein a surface area of the cover coating on the resin molding is 2 m
      2 or more, a settling starting time at 90°C thereof is 60 seconds or more and 200 seconds or less, a cover with a viscosity of 3,500 Pa/s or less is used, and the cover injection ports are provided so as to allow the shortest flowing distance to be 1.3 m or less out of distances between all points in the cover coating space and each of the cover injection ports.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:即使涂覆物体是大型模制品,并且由此得到的涂覆模塑件,提供能够形成均匀的覆盖涂膜而不引起未涂覆的缺陷部分的模内涂覆方法。 解决方案:在模具涂布方法中,将成型后的盖注入口的树脂成型体和模具形成的覆盖层空间注入模内,在树脂成形体的表面形成覆盖层,成形后 将树脂材料注入由一对阳模和阴模的模具形成的空腔中的树脂,其中,树脂模制品上的覆盖涂层的表面积为2μm×SP 2以上 在90℃下的沉降开始时间为60秒以上且200秒以下,使用粘度为3,500Pa / s以下的盖,并且盖喷射口设置成允许最短流动 在覆盖空间和每个盖注入口中的所有点之间的距离距离为1.3μm以下。 版权所有(C)2008,JPO&INPIT