    • 59. 发明授权
    • Reduction casting method
    • 还原铸造法
    • US06932142B2
    • 2005-08-23
    • US10384717
    • 2003-03-11
    • Keisuke Ban
    • Keisuke Ban
    • B22D18/02B22D15/00B22D17/00B22D21/00B22D21/04B22D23/00B22D27/00B22D27/04B22D27/09B22D27/18
    • B22D21/00B22D15/00B22D17/00B22D21/007B22D27/00B22D27/09
    • A reduction casting method includes the steps of: pouring a molten metal into a cavity of a molding die; and performing casting while reducing an oxide film formed on a surface of the molten metal by allowing the molten metal and a reducing substance to come into contact with each other in the cavity. On this occasion, the molten metal is poured into the cavity in a state in which the molding die is forcibly cooled by a cooling device, thereby being rapidly cooled. Further, on this occasion, a solidification speed at which the molten metal is rapidly cooled is allowed to be 600° C./min or more. Still further, on this occasion, the molten metal is filled into the cavity in a filling time of from 1.0 second to 9.0 seconds.
    • 还原铸造方法包括以下步骤:将熔融金属浇注到成型模具的空腔中; 并且通过使熔融金属和还原性物质在空腔中相互接触来还原形成在熔融金属表面上的氧化膜的同时进行铸造。 在这种情况下,在模具被冷却装置强制冷却的状态下将熔融金属倒入空腔中,从而迅速冷却。 此外,在这种情况下,将熔融金属快速冷却的凝固速度设定为600℃/分钟以上。 此外,在这种情况下,熔融金属以1.0秒至9.0秒的填充时间填充到空腔中。