    • 57. 发明专利
    • Sintered iron alloy for valve seat
    • 用于阀座的烧结铁合金
    • JPS61139644A
    • 1986-06-26
    • JP26042084
    • 1984-12-10
    • Toyota Motor Corp
    • KADOTA YUKIOMANABE AKIRA
    • C22C38/00C22C33/02C22C38/30C22C38/60
    • PURPOSE: To obtain the titled sintered iron alloy having the well-balanced its own wear resistance and attacking action on an opposite member by dispersing the rigid particles of an alloy consisting of Co, Cr, Mo and C in an iron matrix contg. C or further contg. Ni.
      CONSTITUTION: The sintered iron alloy for a valve seat is obtd. by dispersing rigid particles of an alloy consisting of, by weight, 0.5W3.0% C, 5W20% Mo, 10W40% Cr and the balance Co in an iron matrix consisting essentially of pearlite. The iron alloy has a composition consisting of 1.9W21.1% Co, 0.5W10% Cr, 0.15W5% Mo, 0.8W2.8% C and the balance Fe or further contg. 1W10% Ni. Pb may be infiltrated into the iron alloy by 1W20wt% of the total amount. The iron alloy has the improved wear resistance and the weakened attacking action on an opposite member as compared with a conventional seat material, so an engine valve not subjected to filling or other processing for improving the wear resistance can be used stably.
      COPYRIGHT: (C)1986,JPO&Japio
    • 目的:通过将由Co,Cr,Mo和C组成的合金的刚性颗粒分散在铁基体中,获得具有良好平衡的自身耐磨性和相对构件上的攻击作用的标准烧结铁合金。 C或更进一步 倪 构成:用于阀座的烧结铁合金。 通过将由重量比为0.5-3.0%,5-20%Mo,10-40%Cr和余量Co组成的合金刚性颗粒分散在基本上由珠光体组成的铁基质中。 该铁合金具有由1.9-21.1%Co,0.5-10%Cr,0.15-5%Mo,0.8-2.8%C和余量Fe组成的组合物。 1-10%Ni。 铅可以渗入铁合金总量的1-20wt%。 与常规的座椅材料相比,铁合金具有改进的耐磨性和相对构件的削弱作用,因此可以稳定地使用不进行填充或其它加工的发动机阀来提高耐磨性。
    • 58. 发明专利
    • Low alloy iron powder for sintering
    • 低合金粉末烧结
    • JPS61117202A
    • 1986-06-04
    • JP23690684
    • 1984-11-10
    • Toyota Motor Corp
    • TAKAHASHI YOSHITAKAMANABE AKIRASUDO SHUNTARO
    • B22F1/00C22C38/00C22C38/02C22C38/42C22C38/44
    • PURPOSE: To obtain low alloy iron powder for sintering having superior hardenability and compactibility at a reduced cost of starting materials by specifying a composition consisting of Mo, C, O, Si, Cr, Cu, Ni and Fe.
      CONSTITUTION: This low alloy iron powder for sintering consists of, by weight, 0.2W2.0% Mo, ≤0.05% C, ≤0.2% O, ≤0.2% in total of Si, Cr, Cu and Ni, and the balance Fe with inevitable impurities, and it is simply obtd. by a water spraying method by which water is sprayed under high pressure on a molten alloy having said composition allowed to flow out of a tundish. The powder has superior hardenability and compactibility and is suitable for use as a material for a high density and high strength sintered material for structural machine parts.
      COPYRIGHT: (C)1986,JPO&Japio
    • 目的:通过指定由Mo,C,O,Si,Cr,Cu,Ni和Fe组成的组成,以降低成本的原料获得具有优异的淬透性和可压实性的低合金铁粉。 构成:用于烧结的低合金铁粉由Si,Cr,Cu和Ni的总计重量计为0.2-2.0%Mo,<= 0.05%C,<= 0.2%O,<= 0.2% 平衡Fe与不可避免的杂质,简直就是说。 通过喷水法将水在高压下喷洒在具有允许从中间包流出的组成的熔融合金上。 该粉末具有优异的淬透性和可压实性,并且适用于用于结构机械部件的高密度和高强度烧结材料的材料。
    • 59. 发明专利
    • Silicon carbide fiber reinforced copper compound material for electrode
    • 用于电极的碳化硅纤维增强铜复合材料
    • JPS6195786A
    • 1986-05-14
    • JP21909384
    • 1984-10-18
    • Toyota Motor Corp
    • SUDO SHUNTAROMANABE AKIRATAKAHASHI YOSHITAKADONOMOTO TADASHI
    • B23K11/30B23K35/00B23K35/02B23K35/22
    • B23K35/222
    • PURPOSE:To provide the titled compound material having both excellent mechanical property of wear resistance, strength, etc. and electrical and thermal properties of conductivity, thermal conductivity, etc. by consisting of the silicon carbide fiber in the range of the specified volume factor specified respectively a mean fiber diameter and aspect ratio as a reinforced material and a pure copper as a matrix. CONSTITUTION:The silicon carbide fiber reinforced copper compound material for electrode is composed of the silicon carbide fiber of
    • 目的:提供具有优异的耐磨性,强度等的机械性能以及导电性,导热性等的电气和热性能的特殊复合材料,其特征在于规定体积因子范围内的碳化硅纤维 分别作为增强材料的平均纤维直径和纵横比,以及作为基质的纯铜。 构成:用于电极的碳化硅纤维增强铜复合材料由<=50μm的碳化硅纤维,特别是0.1-10μm的平均纤维直径和5-500wt%,特别是10-300纵横比组成,作为增强材料,纯的 大于99.5%的铜,特别是99.7%的纯度作为基质。 该复合材料中的碳化硅纤维的体积系数也是2.0-25%,特别是5.0-20%也是必须的。 此外,该复合材料的密度比大于0.90,特别是大于0.92。 该复合材料适用于搭接电阻焊接用电极的形成。
    • 60. 发明专利
    • Manufacture of iron-base sintered material
    • 铁基烧结材料的制造
    • JPS6191346A
    • 1986-05-09
    • JP21337784
    • 1984-10-12
    • Toyota Motor Corp
    • TAKAHASHI YOSHITAKAMANABE AKIRASUDO SHUNTARO
    • C22C33/02
    • PURPOSE: To obtain a high density iron-base sintered material having improved strength by mixing iron powder or iron-base powder as a matrix material with powder of an Fe-Mo-C mother alloy having a low m.p. and graphite powder and by molding and sintering the mixture.
      CONSTITUTION: Iron powder or iron-base powder as a matrix material is mixed with 0.5W10% powder of an Fe-Mo-C mother alloy having a low m.p. and ≤2.0% graphite powder. The mother alloy forms a liq. phase or a solid-liq. coexisting phase at ≤1,150°C and consists of, by weight, 5W30% Mo, 1.5W6.0% C, ≤5% one or more among Cr, Mn, B, Co, Ni, P, Si, Ti, V, W, Nb, Zr and Cu, and the balance Fe with ≤1.0% impurities. The mixture is molded and sintered. By this method, a high density iron-base sintered material having improved strength is easily obtd. without carrying out heat treatment.
      COPYRIGHT: (C)1986,JPO&Japio
    • 目的:通过将铁粉或铁基粉末作为基质材料与低熔点的Fe-Mo-C母合金粉末混合,获得具有改进强度的高密度铁基烧结材料。 和石墨粉末,并通过模制和烧结混合物。 构成:将铁粉或铁基粉末作为基质材料与0.5-10%的低熔点Fe-Mo-C母合金粉末混合。 和<= 2.0%的石墨粉末。 母合金形成液晶。 阶段或固体。 在<= 1,150℃下共存相,并且由Cr,Mn,B,Co,Ni,P,Si中的5-30%Mo,1.5-6.0%C,≤5%中的一种或多种组成, Ti,V,W,Nb,Zr和Cu,余量为<= 1.0%杂质的Fe。 混合物被模制和烧结。 通过这种方法,容易获得具有改善强度的高密度铁基烧结材料。 不进行热处理。